Author: rorschach
Time: 04/02/03 15:01 PST
This is a reply to message no. 10937 by gearloose
Reply | Original Message | New Topic | List Topics | List Messages on This Topic
Current Topic:
METAL HEAT TREATMENT, carbon stopoff paste for carburizing
hey, no problem, I'm used to the taste of shoe leather myself....

Haven't heard of Electrolytic Nickel being used (perhaps it is still in development), but the question(s) is (are), can you:
A) prevent any holidays in the plating so that you don't have an anodic site.

B) how do you strip the nickel without damaging the Nitrided surface?
[ List Replies to This Message Only ]