engineering fundamentals
Wide Flange Steel I Beam: W12 × 136
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Four Equal Spans » Wide Flange Steel I Beam » W12 × 136
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in four equal spans, we compute the displacement at the middle of the first and fourth spans, and the maximum normal stress stress_max occuring at the second and fourth supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1240 in4) for the W12 × 136 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 3.18 × 10-6 8.51
200 4.67 × 10-6 12.5
300 7.00 × 10-6 18.8
400 9.34 × 10-6 25.0
500 1.17 × 10-5 31.3
600 1.40 × 10-5 37.5
700 1.63 × 10-5 43.8
800 1.87 × 10-5 50.0
900 2.10 × 10-5 56.3
1000 2.33 × 10-5 62.5
2000 4.67 × 10-5 125
3000 7.00 × 10-5 188
4000 9.34 × 10-5 250
5000 1.17 × 10-4 313
6000 1.40 × 10-4 375
7000 1.63 × 10-4 438
8000 1.87 × 10-4 500
9000 2.10 × 10-4 563
1.00 × 104 2.33 × 10-4 625
2.00 × 104 4.67 × 10-4 1250
3.00 × 104 7.00 × 10-4 1880
4.00 × 104 9.34 × 10-4 2500
5.00 × 104 0.00117 3130
6.00 × 104 0.00140 3750
7.00 × 104 0.00163 4380
8.00 × 104 0.00187 5000
9.00 × 104 0.00210 5630
1.00 × 105 0.00233 6250
2.00 × 105 0.00467 1.25 × 104
3.00 × 105 0.00700 1.88 × 104
4.00 × 105 0.00934 2.50 × 104
5.00 × 105 0.0117 3.13 × 104
6.00 × 105 0.0140 3.75 × 104
7.00 × 105 0.0163 4.38 × 104
8.00 × 105 0.0187 5.00 × 104
9.00 × 105 0.0210 5.63 × 104
1.00 × 106 0.0233 6.25 × 104
2.00 × 106 0.0467 1.25 × 105
3.00 × 106 0.0700 1.88 × 105
4.00 × 106 0.0934 2.50 × 105
4.75 × 106 0.111 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 2.45 × 10-5 23.6
200 3.60 × 10-5 34.7
300 5.40 × 10-5 52.1
400 7.21 × 10-5 69.5
500 9.01 × 10-5 86.9
600 1.08 × 10-4 104
700 1.26 × 10-4 122
800 1.44 × 10-4 139
900 1.62 × 10-4 156
1000 1.80 × 10-4 174
2000 3.60 × 10-4 347
3000 5.40 × 10-4 521
4000 7.21 × 10-4 695
5000 9.01 × 10-4 869
6000 0.00108 1040
7000 0.00126 1220
8000 0.00144 1390
9000 0.00162 1560
1.00 × 104 0.00180 1740
2.00 × 104 0.00360 3470
3.00 × 104 0.00540 5210
4.00 × 104 0.00721 6950
5.00 × 104 0.00901 8690
6.00 × 104 0.0108 1.04 × 104
7.00 × 104 0.0126 1.22 × 104
8.00 × 104 0.0144 1.39 × 104
9.00 × 104 0.0162 1.56 × 104
1.00 × 105 0.0180 1.74 × 104
2.00 × 105 0.0360 3.47 × 104
3.00 × 105 0.0540 5.21 × 104
4.00 × 105 0.0721 6.95 × 104
5.00 × 105 0.0901 8.69 × 104
6.00 × 105 0.108 1.04 × 105
7.00 × 105 0.126 1.22 × 105
8.00 × 105 0.144 1.39 × 105
9.00 × 105 0.162 1.56 × 105
1.00 × 106 0.180 1.74 × 105
1.71 × 106 0.308 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 3.92 × 10-4 94.5
200 5.76 × 10-4 139
300 8.65 × 10-4 208
400 0.00115 278
500 0.00144 347
600 0.00173 417
700 0.00202 486
800 0.00231 556
900 0.00259 625
1000 0.00288 695
2000 0.00576 1390
3000 0.00865 2080
4000 0.0115 2780
5000 0.0144 3470
6000 0.0173 4170
7000 0.0202 4860
8000 0.0231 5560
9000 0.0259 6250
1.00 × 104 0.0288 6950
2.00 × 104 0.0576 1.39 × 104
3.00 × 104 0.0865 2.08 × 104
4.00 × 104 0.115 2.78 × 104
5.00 × 104 0.144 3.47 × 104
6.00 × 104 0.173 4.17 × 104
7.00 × 104 0.202 4.86 × 104
8.00 × 104 0.231 5.56 × 104
9.00 × 104 0.259 6.25 × 104
1.00 × 105 0.288 6.95 × 104
2.00 × 105 0.576 1.39 × 105
3.00 × 105 0.865 2.08 × 105
4.00 × 105 1.15 2.78 × 105
4.27 × 105 1.23 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.00198 213
200 0.00292 313
300 0.00438 469
400 0.00584 625
500 0.00730 782
600 0.00876 938
700 0.0102 1090
800 0.0117 1250
900 0.0131 1410
1000 0.0146 1560
2000 0.0292 3130
3000 0.0438 4690
4000 0.0584 6250
5000 0.0730 7820
6000 0.0876 9380
7000 0.102 1.09 × 104
8000 0.117 1.25 × 104
9000 0.131 1.41 × 104
1.00 × 104 0.146 1.56 × 104
2.00 × 104 0.292 3.13 × 104
3.00 × 104 0.438 4.69 × 104
4.00 × 104 0.584 6.25 × 104
5.00 × 104 0.730 7.82 × 104
6.00 × 104 0.876 9.38 × 104
7.00 × 104 1.02 1.09 × 105
8.00 × 104 1.17 1.25 × 105
9.00 × 104 1.31 1.41 × 105
1.00 × 105 1.46 1.56 × 105
1.90 × 105 2.77 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.00627 378
200 0.00922 556
300 0.0138 834
400 0.0184 1110
500 0.0231 1390
600 0.0277 1670
700 0.0323 1950
800 0.0369 2220
900 0.0415 2500
1000 0.0461 2780
2000 0.0922 5560
3000 0.138 8340
4000 0.184 1.11 × 104
5000 0.231 1.39 × 104
6000 0.277 1.67 × 104
7000 0.323 1.95 × 104
8000 0.369 2.22 × 104
9000 0.415 2.50 × 104
1.00 × 104 0.461 2.78 × 104
2.00 × 104 0.922 5.56 × 104
3.00 × 104 1.38 8.34 × 104
4.00 × 104 1.84 1.11 × 105
5.00 × 104 2.31 1.39 × 105
6.00 × 104 2.77 1.67 × 105
7.00 × 104 3.23 1.95 × 105
8.00 × 104 3.69 2.22 × 105
9.00 × 104 4.15 2.50 × 105
1.00 × 105 4.61 2.78 × 105
1.07 × 105 4.93 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.0153 591
200 0.0225 869
300 0.0338 1300
400 0.0450 1740
500 0.0563 2170
600 0.0676 2610
700 0.0788 3040
800 0.0901 3470
900 0.101 3910
1000 0.113 4340
2000 0.225 8690
3000 0.338 1.30 × 104
4000 0.450 1.74 × 104
5000 0.563 2.17 × 104
6000 0.676 2.61 × 104
7000 0.788 3.04 × 104
8000 0.901 3.47 × 104
9000 1.01 3.91 × 104
1.00 × 104 1.13 4.34 × 104
2.00 × 104 2.25 8.69 × 104
3.00 × 104 3.38 1.30 × 105
4.00 × 104 4.50 1.74 × 105
5.00 × 104 5.63 2.17 × 105
6.00 × 104 6.76 2.61 × 105
6.84 × 104 7.70 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.0318 851
200 0.0467 1250
300 0.0700 1880
400 0.0934 2500
500 0.117 3130
600 0.140 3750
700 0.163 4380
800 0.187 5000
900 0.210 5630
1000 0.233 6250
2000 0.467 1.25 × 104
3000 0.700 1.88 × 104
4000 0.934 2.50 × 104
5000 1.17 3.13 × 104
6000 1.40 3.75 × 104
7000 1.63 4.38 × 104
8000 1.87 5.00 × 104
9000 2.10 5.63 × 104
1.00 × 104 2.33 6.25 × 104
2.00 × 104 4.67 1.25 × 105
3.00 × 104 7.00 1.88 × 105
4.00 × 104 9.34 2.50 × 105
4.75 × 104 11.1 2.97 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.100 1510
200 0.148 2220
300 0.221 3340
400 0.295 4450
500 0.369 5560
600 0.443 6670
700 0.517 7780
800 0.590 8900
900 0.664 1.00 × 104
1000 0.738 1.11 × 104
2000 1.48 2.22 × 104
3000 2.21 3.34 × 104
4000 2.95 4.45 × 104
5000 3.69 5.56 × 104
6000 4.43 6.67 × 104
7000 5.17 7.78 × 104
8000 5.90 8.90 × 104
9000 6.64 1.00 × 105
1.00 × 104 7.38 1.11 × 105
1.82 × 104 13.4 2.02 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.245 2360
200 0.360 3470
300 0.540 5210
400 0.721 6950
500 0.901 8690
600 1.08 1.04 × 104
700 1.26 1.22 × 104
800 1.44 1.39 × 104
900 1.62 1.56 × 104
1000 1.80 1.74 × 104
2000 3.60 3.47 × 104
3000 5.40 5.21 × 104
4000 7.21 6.95 × 104
5000 9.01 8.69 × 104
6000 10.8 1.04 × 105
7000 12.6 1.22 × 105
7440 13.4 1.29 × 105
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.508 3400
200 0.747 5000
300 1.12 7510
400 1.49 1.00 × 104
500 1.87 1.25 × 104
600 2.24 1.50 × 104
700 2.61 1.75 × 104
800 2.99 2.00 × 104
900 3.36 2.25 × 104
1000 3.74 2.50 × 104
2000 7.47 5.00 × 104
3000 11.2 7.51 × 104
3590 13.4 8.98 × 104
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 0.941 4630
200 1.38 6810
300 2.08 1.02 × 104
400 2.77 1.36 × 104
500 3.46 1.70 × 104
600 4.15 2.04 × 104
700 4.84 2.38 × 104
800 5.54 2.72 × 104
900 6.23 3.06 × 104
1000 6.92 3.41 × 104
1940 13.4 6.60 × 104
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 1.61 6050
200 2.36 8900
300 3.54 1.33 × 104
400 4.72 1.78 × 104
500 5.90 2.22 × 104
600 7.08 2.67 × 104
700 8.26 3.11 × 104
800 9.45 3.56 × 104
900 10.6 4.00 × 104
1000 11.8 4.45 × 104
1140 13.4 5.05 × 104
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 2.57 7660
200 3.78 1.13 × 104
300 5.67 1.69 × 104
400 7.56 2.25 × 104
500 9.46 2.81 × 104
600 11.3 3.38 × 104
700 13.2 3.94 × 104
709 13.4 3.99 × 104
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 3.92 9450
200 5.76 1.39 × 104
300 8.65 2.08 × 104
400 11.5 2.78 × 104
465 13.4 3.23 × 104
Steel I Beam: W12 × 136 (Wide Flange 12 inch tall × 136 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
136 9.57 1.48 × 104
191 13.4 2.07 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.