engineering fundamentals
Wide Flange Steel I Beam: W12 × 79
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Four Equal Spans » Wide Flange Steel I Beam » W12 × 79
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in four equal spans, we compute the displacement at the middle of the first and fourth spans, and the maximum normal stress stress_max occuring at the second and fourth supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 662 in4) for the W12 × 79 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 3.45 × 10-6 8.54
80.0 3.50 × 10-6 8.65
90.0 3.94 × 10-6 9.73
100 4.37 × 10-6 10.8
200 8.75 × 10-6 21.6
300 1.31 × 10-5 32.4
400 1.75 × 10-5 43.3
500 2.19 × 10-5 54.1
600 2.62 × 10-5 64.9
700 3.06 × 10-5 75.7
800 3.50 × 10-5 86.5
900 3.94 × 10-5 97.3
1000 4.37 × 10-5 108
2000 8.75 × 10-5 216
3000 1.31 × 10-4 324
4000 1.75 × 10-4 433
5000 2.19 × 10-4 541
6000 2.62 × 10-4 649
7000 3.06 × 10-4 757
8000 3.50 × 10-4 865
9000 3.94 × 10-4 973
1.00 × 104 4.37 × 10-4 1080
2.00 × 104 8.75 × 10-4 2160
3.00 × 104 0.00131 3240
4.00 × 104 0.00175 4330
5.00 × 104 0.00219 5410
6.00 × 104 0.00262 6490
7.00 × 104 0.00306 7570
8.00 × 104 0.00350 8650
9.00 × 104 0.00394 9730
1.00 × 105 0.00437 1.08 × 104
2.00 × 105 0.00875 2.16 × 104
3.00 × 105 0.0131 3.24 × 104
4.00 × 105 0.0175 4.33 × 104
5.00 × 105 0.0219 5.41 × 104
6.00 × 105 0.0262 6.49 × 104
7.00 × 105 0.0306 7.57 × 104
8.00 × 105 0.0350 8.65 × 104
9.00 × 105 0.0394 9.73 × 104
1.00 × 106 0.0437 1.08 × 105
2.00 × 106 0.0875 2.16 × 105
2.75 × 106 0.120 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 2.67 × 10-5 23.7
80.0 2.70 × 10-5 24.0
90.0 3.04 × 10-5 27.0
100 3.37 × 10-5 30.0
200 6.75 × 10-5 60.1
300 1.01 × 10-4 90.1
400 1.35 × 10-4 120
500 1.69 × 10-4 150
600 2.02 × 10-4 180
700 2.36 × 10-4 210
800 2.70 × 10-4 240
900 3.04 × 10-4 270
1000 3.37 × 10-4 300
2000 6.75 × 10-4 601
3000 0.00101 901
4000 0.00135 1200
5000 0.00169 1500
6000 0.00202 1800
7000 0.00236 2100
8000 0.00270 2400
9000 0.00304 2700
1.00 × 104 0.00337 3000
2.00 × 104 0.00675 6010
3.00 × 104 0.0101 9010
4.00 × 104 0.0135 1.20 × 104
5.00 × 104 0.0169 1.50 × 104
6.00 × 104 0.0202 1.80 × 104
7.00 × 104 0.0236 2.10 × 104
8.00 × 104 0.0270 2.40 × 104
9.00 × 104 0.0304 2.70 × 104
1.00 × 105 0.0337 3.00 × 104
2.00 × 105 0.0675 6.01 × 104
3.00 × 105 0.101 9.01 × 104
4.00 × 105 0.135 1.20 × 105
5.00 × 105 0.169 1.50 × 105
6.00 × 105 0.202 1.80 × 105
7.00 × 105 0.236 2.10 × 105
8.00 × 105 0.270 2.40 × 105
9.00 × 105 0.304 2.70 × 105
9.89 × 105 0.334 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 4.27 × 10-4 94.9
80.0 4.32 × 10-4 96.1
90.0 4.86 × 10-4 108
100 5.40 × 10-4 120
200 0.00108 240
300 0.00162 361
400 0.00216 481
500 0.00270 601
600 0.00324 721
700 0.00378 841
800 0.00432 961
900 0.00486 1080
1000 0.00540 1200
2000 0.0108 2400
3000 0.0162 3610
4000 0.0216 4810
5000 0.0270 6010
6000 0.0324 7210
7000 0.0378 8410
8000 0.0432 9610
9000 0.0486 1.08 × 104
1.00 × 104 0.0540 1.20 × 104
2.00 × 104 0.108 2.40 × 104
3.00 × 104 0.162 3.61 × 104
4.00 × 104 0.216 4.81 × 104
5.00 × 104 0.270 6.01 × 104
6.00 × 104 0.324 7.21 × 104
7.00 × 104 0.378 8.41 × 104
8.00 × 104 0.432 9.61 × 104
9.00 × 104 0.486 1.08 × 105
1.00 × 105 0.540 1.20 × 105
2.00 × 105 1.08 2.40 × 105
2.47 × 105 1.33 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.00216 214
80.0 0.00219 216
90.0 0.00246 243
100 0.00273 270
200 0.00547 541
300 0.00820 811
400 0.0109 1080
500 0.0137 1350
600 0.0164 1620
700 0.0191 1890
800 0.0219 2160
900 0.0246 2430
1000 0.0273 2700
2000 0.0547 5410
3000 0.0820 8110
4000 0.109 1.08 × 104
5000 0.137 1.35 × 104
6000 0.164 1.62 × 104
7000 0.191 1.89 × 104
8000 0.219 2.16 × 104
9000 0.246 2.43 × 104
1.00 × 104 0.273 2.70 × 104
2.00 × 104 0.547 5.41 × 104
3.00 × 104 0.820 8.11 × 104
4.00 × 104 1.09 1.08 × 105
5.00 × 104 1.37 1.35 × 105
6.00 × 104 1.64 1.62 × 105
7.00 × 104 1.91 1.89 × 105
8.00 × 104 2.19 2.16 × 105
9.00 × 104 2.46 2.43 × 105
1.00 × 105 2.73 2.70 × 105
1.10 × 105 3.00 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.00682 380
80.0 0.00691 385
90.0 0.00777 433
100 0.00864 481
200 0.0173 961
300 0.0259 1440
400 0.0346 1920
500 0.0432 2400
600 0.0518 2880
700 0.0605 3360
800 0.0691 3850
900 0.0777 4330
1000 0.0864 4810
2000 0.173 9610
3000 0.259 1.44 × 104
4000 0.346 1.92 × 104
5000 0.432 2.40 × 104
6000 0.518 2.88 × 104
7000 0.605 3.36 × 104
8000 0.691 3.85 × 104
9000 0.777 4.33 × 104
1.00 × 104 0.864 4.81 × 104
2.00 × 104 1.73 9.61 × 104
3.00 × 104 2.59 1.44 × 105
4.00 × 104 3.46 1.92 × 105
5.00 × 104 4.32 2.40 × 105
6.00 × 104 5.18 2.88 × 105
6.18 × 104 5.34 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.0167 593
80.0 0.0169 601
90.0 0.0190 676
100 0.0211 751
200 0.0422 1500
300 0.0633 2250
400 0.0844 3000
500 0.105 3760
600 0.127 4510
700 0.148 5260
800 0.169 6010
900 0.190 6760
1000 0.211 7510
2000 0.422 1.50 × 104
3000 0.633 2.25 × 104
4000 0.844 3.00 × 104
5000 1.05 3.76 × 104
6000 1.27 4.51 × 104
7000 1.48 5.26 × 104
8000 1.69 6.01 × 104
9000 1.90 6.76 × 104
1.00 × 104 2.11 7.51 × 104
2.00 × 104 4.22 1.50 × 105
3.00 × 104 6.33 2.25 × 105
3.95 × 104 8.34 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.0345 854
80.0 0.0350 865
90.0 0.0394 973
100 0.0437 1080
200 0.0875 2160
300 0.131 3240
400 0.175 4330
500 0.219 5410
600 0.262 6490
700 0.306 7570
800 0.350 8650
900 0.394 9730
1000 0.437 1.08 × 104
2000 0.875 2.16 × 104
3000 1.31 3.24 × 104
4000 1.75 4.33 × 104
5000 2.19 5.41 × 104
6000 2.62 6.49 × 104
7000 3.06 7.57 × 104
8000 3.50 8.65 × 104
9000 3.94 9.73 × 104
1.00 × 104 4.37 1.08 × 105
2.00 × 104 8.75 2.16 × 105
2.75 × 104 12.0 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.109 1520
80.0 0.111 1540
90.0 0.124 1730
100 0.138 1920
200 0.276 3850
300 0.415 5770
400 0.553 7690
500 0.691 9610
600 0.829 1.15 × 104
700 0.968 1.35 × 104
800 1.11 1.54 × 104
900 1.24 1.73 × 104
1000 1.38 1.92 × 104
2000 2.76 3.85 × 104
3000 4.15 5.77 × 104
4000 5.53 7.69 × 104
5000 6.91 9.61 × 104
6000 8.29 1.15 × 105
7000 9.68 1.35 × 105
8000 11.1 1.54 × 105
8960 12.4 1.72 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.267 2370
80.0 0.270 2400
90.0 0.304 2700
100 0.337 3000
200 0.675 6010
300 1.01 9010
400 1.35 1.20 × 104
500 1.69 1.50 × 104
600 2.02 1.80 × 104
700 2.36 2.10 × 104
800 2.70 2.40 × 104
900 3.04 2.70 × 104
1000 3.37 3.00 × 104
2000 6.75 6.01 × 104
3000 10.1 9.01 × 104
3670 12.4 1.10 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.553 3420
80.0 0.560 3460
90.0 0.630 3890
100 0.700 4330
200 1.40 8650
300 2.10 1.30 × 104
400 2.80 1.73 × 104
500 3.50 2.16 × 104
600 4.20 2.60 × 104
700 4.90 3.03 × 104
800 5.60 3.46 × 104
900 6.30 3.89 × 104
1000 7.00 4.33 × 104
1770 12.4 7.65 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 1.02 4650
80.0 1.04 4710
90.0 1.17 5300
100 1.30 5890
200 2.59 1.18 × 104
300 3.89 1.77 × 104
400 5.19 2.36 × 104
500 6.48 2.94 × 104
600 7.78 3.53 × 104
700 9.07 4.12 × 104
800 10.4 4.71 × 104
900 11.7 5.30 × 104
955 12.4 5.62 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 1.75 6080
80.0 1.77 6150
90.0 1.99 6920
100 2.21 7690
200 4.42 1.54 × 104
300 6.63 2.31 × 104
400 8.85 3.08 × 104
500 11.1 3.85 × 104
560 12.4 4.31 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 2.80 7690
80.0 2.83 7790
90.0 3.19 8760
100 3.54 9730
200 7.08 1.95 × 104
300 10.6 2.92 × 104
349 12.4 3.40 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 4.27 9490
80.0 4.32 9610
90.0 4.86 1.08 × 104
100 5.40 1.20 × 104
200 10.8 2.40 × 104
229 12.4 2.76 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 10.4 1.48 × 104
80.0 10.5 1.50 × 104
90.0 11.9 1.69 × 104
93.9 12.4 1.76 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.