S Section Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1190 in4) for the S20 × 66 S Section Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 3.32 × 10-6 7.49
70.0 3.52 × 10-6 7.94
80.0 4.02 × 10-6 9.08
90.0 4.53 × 10-6 10.2
100 5.03 × 10-6 11.3
200 1.01 × 10-5 22.7
300 1.51 × 10-5 34.0
400 2.01 × 10-5 45.4
500 2.51 × 10-5 56.7
600 3.02 × 10-5 68.1
700 3.52 × 10-5 79.4
800 4.02 × 10-5 90.8
900 4.53 × 10-5 102
1000 5.03 × 10-5 113
2000 1.01 × 10-4 227
3000 1.51 × 10-4 340
4000 2.01 × 10-4 454
5000 2.51 × 10-4 567
6000 3.02 × 10-4 681
7000 3.52 × 10-4 794
8000 4.02 × 10-4 908
9000 4.53 × 10-4 1020
1.00 × 104 5.03 × 10-4 1130
2.00 × 104 0.00101 2270
3.00 × 104 0.00151 3400
4.00 × 104 0.00201 4540
5.00 × 104 0.00251 5670
6.00 × 104 0.00302 6810
7.00 × 104 0.00352 7940
8.00 × 104 0.00402 9080
9.00 × 104 0.00453 1.02 × 104
1.00 × 105 0.00503 1.13 × 104
2.00 × 105 0.0101 2.27 × 104
3.00 × 105 0.0151 3.40 × 104
4.00 × 105 0.0201 4.54 × 104
5.00 × 105 0.0251 5.67 × 104
6.00 × 105 0.0302 6.81 × 104
7.00 × 105 0.0352 7.94 × 104
8.00 × 105 0.0402 9.08 × 104
9.00 × 105 0.0453 1.02 × 105
1.00 × 106 0.0503 1.13 × 105
2.00 × 106 0.101 2.27 × 105
2.62 × 106 0.132 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 2.56 × 10-5 20.8
70.0 2.72 × 10-5 22.1
80.0 3.10 × 10-5 25.2
90.0 3.49 × 10-5 28.4
100 3.88 × 10-5 31.5
200 7.76 × 10-5 63.0
300 1.16 × 10-4 94.5
400 1.55 × 10-4 126
500 1.94 × 10-4 158
600 2.33 × 10-4 189
700 2.72 × 10-4 221
800 3.10 × 10-4 252
900 3.49 × 10-4 284
1000 3.88 × 10-4 315
2000 7.76 × 10-4 630
3000 0.00116 945
4000 0.00155 1260
5000 0.00194 1580
6000 0.00233 1890
7000 0.00272 2210
8000 0.00310 2520
9000 0.00349 2840
1.00 × 104 0.00388 3150
2.00 × 104 0.00776 6300
3.00 × 104 0.0116 9450
4.00 × 104 0.0155 1.26 × 104
5.00 × 104 0.0194 1.58 × 104
6.00 × 104 0.0233 1.89 × 104
7.00 × 104 0.0272 2.21 × 104
8.00 × 104 0.0310 2.52 × 104
9.00 × 104 0.0349 2.84 × 104
1.00 × 105 0.0388 3.15 × 104
2.00 × 105 0.0776 6.30 × 104
3.00 × 105 0.116 9.45 × 104
4.00 × 105 0.155 1.26 × 105
5.00 × 105 0.194 1.58 × 105
6.00 × 105 0.233 1.89 × 105
7.00 × 105 0.272 2.21 × 105
8.00 × 105 0.310 2.52 × 105
9.00 × 105 0.349 2.84 × 105
9.43 × 105 0.366 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 4.10 × 10-4 83.2
70.0 4.35 × 10-4 88.2
80.0 4.97 × 10-4 101
90.0 5.59 × 10-4 113
100 6.21 × 10-4 126
200 0.00124 252
300 0.00186 378
400 0.00248 504
500 0.00310 630
600 0.00372 756
700 0.00435 882
800 0.00497 1010
900 0.00559 1130
1000 0.00621 1260
2000 0.0124 2520
3000 0.0186 3780
4000 0.0248 5040
5000 0.0310 6300
6000 0.0372 7560
7000 0.0435 8820
8000 0.0497 1.01 × 104
9000 0.0559 1.13 × 104
1.00 × 104 0.0621 1.26 × 104
2.00 × 104 0.124 2.52 × 104
3.00 × 104 0.186 3.78 × 104
4.00 × 104 0.248 5.04 × 104
5.00 × 104 0.310 6.30 × 104
6.00 × 104 0.372 7.56 × 104
7.00 × 104 0.435 8.82 × 104
8.00 × 104 0.497 1.01 × 105
9.00 × 104 0.559 1.13 × 105
1.00 × 105 0.621 1.26 × 105
2.00 × 105 1.24 2.52 × 105
2.36 × 105 1.46 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.00207 187
70.0 0.00220 199
80.0 0.00251 227
90.0 0.00283 255
100 0.00314 284
200 0.00629 567
300 0.00943 851
400 0.0126 1130
500 0.0157 1420
600 0.0189 1700
700 0.0220 1990
800 0.0251 2270
900 0.0283 2550
1000 0.0314 2840
2000 0.0629 5670
3000 0.0943 8510
4000 0.126 1.13 × 104
5000 0.157 1.42 × 104
6000 0.189 1.70 × 104
7000 0.220 1.99 × 104
8000 0.251 2.27 × 104
9000 0.283 2.55 × 104
1.00 × 104 0.314 2.84 × 104
2.00 × 104 0.629 5.67 × 104
3.00 × 104 0.943 8.51 × 104
4.00 × 104 1.26 1.13 × 105
5.00 × 104 1.57 1.42 × 105
6.00 × 104 1.89 1.70 × 105
7.00 × 104 2.20 1.99 × 105
8.00 × 104 2.51 2.27 × 105
9.00 × 104 2.83 2.55 × 105
1.00 × 105 3.14 2.84 × 105
1.05 × 105 3.29 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.00656 333
70.0 0.00695 353
80.0 0.00795 403
90.0 0.00894 454
100 0.00993 504
200 0.0199 1010
300 0.0298 1510
400 0.0397 2020
500 0.0497 2520
600 0.0596 3030
700 0.0695 3530
800 0.0795 4030
900 0.0894 4540
1000 0.0993 5040
2000 0.199 1.01 × 104
3000 0.298 1.51 × 104
4000 0.397 2.02 × 104
5000 0.497 2.52 × 104
6000 0.596 3.03 × 104
7000 0.695 3.53 × 104
8000 0.795 4.03 × 104
9000 0.894 4.54 × 104
1.00 × 104 0.993 5.04 × 104
2.00 × 104 1.99 1.01 × 105
3.00 × 104 2.98 1.51 × 105
4.00 × 104 3.97 2.02 × 105
5.00 × 104 4.97 2.52 × 105
5.89 × 104 5.85 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.0160 520
70.0 0.0170 551
80.0 0.0194 630
90.0 0.0218 709
100 0.0242 788
200 0.0485 1580
300 0.0727 2360
400 0.0970 3150
500 0.121 3940
600 0.145 4730
700 0.170 5510
800 0.194 6300
900 0.218 7090
1000 0.242 7880
2000 0.485 1.58 × 104
3000 0.727 2.36 × 104
4000 0.970 3.15 × 104
5000 1.21 3.94 × 104
6000 1.45 4.73 × 104
7000 1.70 5.51 × 104
8000 1.94 6.30 × 104
9000 2.18 7.09 × 104
1.00 × 104 2.42 7.88 × 104
2.00 × 104 4.85 1.58 × 105
3.00 × 104 7.27 2.36 × 105
3.77 × 104 9.14 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.0332 749
70.0 0.0352 794
80.0 0.0402 908
90.0 0.0453 1020
100 0.0503 1130
200 0.101 2270
300 0.151 3400
400 0.201 4540
500 0.251 5670
600 0.302 6810
700 0.352 7940
800 0.402 9080
900 0.453 1.02 × 104
1000 0.503 1.13 × 104
2000 1.01 2.27 × 104
3000 1.51 3.40 × 104
4000 2.01 4.54 × 104
5000 2.51 5.67 × 104
6000 3.02 6.81 × 104
7000 3.52 7.94 × 104
8000 4.02 9.08 × 104
9000 4.53 1.02 × 105
1.00 × 104 5.03 1.13 × 105
2.00 × 104 10.1 2.27 × 105
2.62 × 104 13.2 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.105 1330
70.0 0.111 1410
80.0 0.127 1610
90.0 0.143 1820
100 0.159 2020
200 0.318 4030
300 0.477 6050
400 0.636 8070
500 0.795 1.01 × 104
600 0.954 1.21 × 104
700 1.11 1.41 × 104
800 1.27 1.61 × 104
900 1.43 1.82 × 104
1000 1.59 2.02 × 104
2000 3.18 4.03 × 104
3000 4.77 6.05 × 104
4000 6.36 8.07 × 104
5000 7.95 1.01 × 105
6000 9.54 1.21 × 105
7000 11.1 1.41 × 105
8000 12.7 1.61 × 105
9000 14.3 1.82 × 105
1.00 × 104 15.9 2.02 × 105
1.47 × 104 23.4 2.97 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.256 2080
70.0 0.272 2210
80.0 0.310 2520
90.0 0.349 2840
100 0.388 3150
200 0.776 6300
300 1.16 9450
400 1.55 1.26 × 104
500 1.94 1.58 × 104
600 2.33 1.89 × 104
700 2.72 2.21 × 104
800 3.10 2.52 × 104
900 3.49 2.84 × 104
1000 3.88 3.15 × 104
2000 7.76 6.30 × 104
3000 11.6 9.45 × 104
4000 15.5 1.26 × 105
5000 19.4 1.58 × 105
5150 20.0 1.62 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.531 2990
70.0 0.563 3180
80.0 0.644 3630
90.0 0.724 4080
100 0.805 4540
200 1.61 9080
300 2.41 1.36 × 104
400 3.22 1.82 × 104
500 4.02 2.27 × 104
600 4.83 2.72 × 104
700 5.63 3.18 × 104
800 6.44 3.63 × 104
900 7.24 4.08 × 104
1000 8.05 4.54 × 104
2000 16.1 9.08 × 104
2490 20.0 1.13 × 105
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 0.984 4080
70.0 1.04 4320
80.0 1.19 4940
90.0 1.34 5560
100 1.49 6180
200 2.98 1.24 × 104
300 4.47 1.85 × 104
400 5.96 2.47 × 104
500 7.45 3.09 × 104
600 8.94 3.71 × 104
700 10.4 4.32 × 104
800 11.9 4.94 × 104
900 13.4 5.56 × 104
1000 14.9 6.18 × 104
1340 20.0 8.29 × 104
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 1.68 5320
70.0 1.78 5650
80.0 2.03 6450
90.0 2.29 7260
100 2.54 8070
200 5.09 1.61 × 104
300 7.63 2.42 × 104
400 10.2 3.23 × 104
500 12.7 4.03 × 104
600 15.3 4.84 × 104
700 17.8 5.65 × 104
787 20.0 6.35 × 104
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 2.69 6740
70.0 2.85 7150
80.0 3.26 8170
90.0 3.67 9190
100 4.07 1.02 × 104
200 8.15 2.04 × 104
300 12.2 3.06 × 104
400 16.3 4.08 × 104
491 20.0 5.01 × 104
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 4.10 8320
70.0 4.35 8820
80.0 4.97 1.01 × 104
90.0 5.59 1.13 × 104
100 6.21 1.26 × 104
200 12.4 2.52 × 104
300 18.6 3.78 × 104
322 20.0 4.06 × 104
Steel I Beam: S20 × 66 (S Section 20 inch tall × 66 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
66.0 10.0 1.30 × 104
70.0 10.6 1.38 × 104
80.0 12.1 1.58 × 104
90.0 13.6 1.77 × 104
100 15.2 1.97 × 104
132 20.0 2.60 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.