engineering fundamentals
Wide Flange Steel I Beam: W14 × 257
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 257
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 3400 in4) for the W14 × 257 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 4.52 × 10-6 8.36
300 5.28 × 10-6 9.76
400 7.04 × 10-6 13.0
500 8.80 × 10-6 16.3
600 1.06 × 10-5 19.5
700 1.23 × 10-5 22.8
800 1.41 × 10-5 26.0
900 1.58 × 10-5 29.3
1000 1.76 × 10-5 32.5
2000 3.52 × 10-5 65.0
3000 5.28 × 10-5 97.6
4000 7.04 × 10-5 130
5000 8.80 × 10-5 163
6000 1.06 × 10-4 195
7000 1.23 × 10-4 228
8000 1.41 × 10-4 260
9000 1.58 × 10-4 293
1.00 × 104 1.76 × 10-4 325
2.00 × 104 3.52 × 10-4 650
3.00 × 104 5.28 × 10-4 976
4.00 × 104 7.04 × 10-4 1300
5.00 × 104 8.80 × 10-4 1630
6.00 × 104 0.00106 1950
7.00 × 104 0.00123 2280
8.00 × 104 0.00141 2600
9.00 × 104 0.00158 2930
1.00 × 105 0.00176 3250
2.00 × 105 0.00352 6500
3.00 × 105 0.00528 9760
4.00 × 105 0.00704 1.30 × 104
5.00 × 105 0.00880 1.63 × 104
6.00 × 105 0.0106 1.95 × 104
7.00 × 105 0.0123 2.28 × 104
8.00 × 105 0.0141 2.60 × 104
9.00 × 105 0.0158 2.93 × 104
1.00 × 106 0.0176 3.25 × 104
2.00 × 106 0.0352 6.50 × 104
3.00 × 106 0.0528 9.76 × 104
4.00 × 106 0.0704 1.30 × 105
5.00 × 106 0.0880 1.63 × 105
6.00 × 106 0.106 1.95 × 105
7.00 × 106 0.123 2.28 × 105
8.00 × 106 0.141 2.60 × 105
9.00 × 106 0.158 2.93 × 105
9.13 × 106 0.161 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 3.49 × 10-5 23.2
300 4.07 × 10-5 27.1
400 5.43 × 10-5 36.1
500 6.79 × 10-5 45.2
600 8.15 × 10-5 54.2
700 9.51 × 10-5 63.2
800 1.09 × 10-4 72.3
900 1.22 × 10-4 81.3
1000 1.36 × 10-4 90.3
2000 2.72 × 10-4 181
3000 4.07 × 10-4 271
4000 5.43 × 10-4 361
5000 6.79 × 10-4 452
6000 8.15 × 10-4 542
7000 9.51 × 10-4 632
8000 0.00109 723
9000 0.00122 813
1.00 × 104 0.00136 903
2.00 × 104 0.00272 1810
3.00 × 104 0.00407 2710
4.00 × 104 0.00543 3610
5.00 × 104 0.00679 4520
6.00 × 104 0.00815 5420
7.00 × 104 0.00951 6320
8.00 × 104 0.0109 7230
9.00 × 104 0.0122 8130
1.00 × 105 0.0136 9030
2.00 × 105 0.0272 1.81 × 104
3.00 × 105 0.0407 2.71 × 104
4.00 × 105 0.0543 3.61 × 104
5.00 × 105 0.0679 4.52 × 104
6.00 × 105 0.0815 5.42 × 104
7.00 × 105 0.0951 6.32 × 104
8.00 × 105 0.109 7.23 × 104
9.00 × 105 0.122 8.13 × 104
1.00 × 106 0.136 9.03 × 104
2.00 × 106 0.272 1.81 × 105
3.00 × 106 0.407 2.71 × 105
3.29 × 106 0.447 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 5.58 × 10-4 92.9
300 6.52 × 10-4 108
400 8.69 × 10-4 145
500 0.00109 181
600 0.00130 217
700 0.00152 253
800 0.00174 289
900 0.00196 325
1000 0.00217 361
2000 0.00435 723
3000 0.00652 1080
4000 0.00869 1450
5000 0.0109 1810
6000 0.0130 2170
7000 0.0152 2530
8000 0.0174 2890
9000 0.0196 3250
1.00 × 104 0.0217 3610
2.00 × 104 0.0435 7230
3.00 × 104 0.0652 1.08 × 104
4.00 × 104 0.0869 1.45 × 104
5.00 × 104 0.109 1.81 × 104
6.00 × 104 0.130 2.17 × 104
7.00 × 104 0.152 2.53 × 104
8.00 × 104 0.174 2.89 × 104
9.00 × 104 0.196 3.25 × 104
1.00 × 105 0.217 3.61 × 104
2.00 × 105 0.435 7.23 × 104
3.00 × 105 0.652 1.08 × 105
4.00 × 105 0.869 1.45 × 105
5.00 × 105 1.09 1.81 × 105
6.00 × 105 1.30 2.17 × 105
7.00 × 105 1.52 2.53 × 105
8.00 × 105 1.74 2.89 × 105
8.22 × 105 1.79 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.00283 209
300 0.00330 244
400 0.00440 325
500 0.00550 406
600 0.00660 488
700 0.00770 569
800 0.00880 650
900 0.00990 732
1000 0.0110 813
2000 0.0220 1630
3000 0.0330 2440
4000 0.0440 3250
5000 0.0550 4060
6000 0.0660 4880
7000 0.0770 5690
8000 0.0880 6500
9000 0.0990 7320
1.00 × 104 0.110 8130
2.00 × 104 0.220 1.63 × 104
3.00 × 104 0.330 2.44 × 104
4.00 × 104 0.440 3.25 × 104
5.00 × 104 0.550 4.06 × 104
6.00 × 104 0.660 4.88 × 104
7.00 × 104 0.770 5.69 × 104
8.00 × 104 0.880 6.50 × 104
9.00 × 104 0.990 7.32 × 104
1.00 × 105 1.10 8.13 × 104
2.00 × 105 2.20 1.63 × 105
3.00 × 105 3.30 2.44 × 105
3.65 × 105 4.02 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.00893 371
300 0.0104 434
400 0.0139 578
500 0.0174 723
600 0.0209 867
700 0.0243 1010
800 0.0278 1160
900 0.0313 1300
1000 0.0348 1450
2000 0.0695 2890
3000 0.104 4340
4000 0.139 5780
5000 0.174 7230
6000 0.209 8670
7000 0.243 1.01 × 104
8000 0.278 1.16 × 104
9000 0.313 1.30 × 104
1.00 × 104 0.348 1.45 × 104
2.00 × 104 0.695 2.89 × 104
3.00 × 104 1.04 4.34 × 104
4.00 × 104 1.39 5.78 × 104
5.00 × 104 1.74 7.23 × 104
6.00 × 104 2.09 8.67 × 104
7.00 × 104 2.43 1.01 × 105
8.00 × 104 2.78 1.16 × 105
9.00 × 104 3.13 1.30 × 105
1.00 × 105 3.48 1.45 × 105
2.00 × 105 6.95 2.89 × 105
2.06 × 105 7.14 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.0218 580
300 0.0255 677
400 0.0339 903
500 0.0424 1130
600 0.0509 1350
700 0.0594 1580
800 0.0679 1810
900 0.0764 2030
1000 0.0849 2260
2000 0.170 4520
3000 0.255 6770
4000 0.339 9030
5000 0.424 1.13 × 104
6000 0.509 1.35 × 104
7000 0.594 1.58 × 104
8000 0.679 1.81 × 104
9000 0.764 2.03 × 104
1.00 × 104 0.849 2.26 × 104
2.00 × 104 1.70 4.52 × 104
3.00 × 104 2.55 6.77 × 104
4.00 × 104 3.39 9.03 × 104
5.00 × 104 4.24 1.13 × 105
6.00 × 104 5.09 1.35 × 105
7.00 × 104 5.94 1.58 × 105
8.00 × 104 6.79 1.81 × 105
9.00 × 104 7.64 2.03 × 105
1.00 × 105 8.49 2.26 × 105
1.32 × 105 11.2 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.0452 836
300 0.0528 976
400 0.0704 1300
500 0.0880 1630
600 0.106 1950
700 0.123 2280
800 0.141 2600
900 0.158 2930
1000 0.176 3250
2000 0.352 6500
3000 0.528 9760
4000 0.704 1.30 × 104
5000 0.880 1.63 × 104
6000 1.06 1.95 × 104
7000 1.23 2.28 × 104
8000 1.41 2.60 × 104
9000 1.58 2.93 × 104
1.00 × 104 1.76 3.25 × 104
2.00 × 104 3.52 6.50 × 104
3.00 × 104 5.28 9.76 × 104
4.00 × 104 7.04 1.30 × 105
5.00 × 104 8.80 1.63 × 105
6.00 × 104 10.6 1.95 × 105
7.00 × 104 12.3 2.28 × 105
8.00 × 104 14.1 2.60 × 105
9.00 × 104 15.8 2.93 × 105
9.13 × 104 16.1 2.97 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.143 1490
300 0.167 1730
400 0.222 2310
500 0.278 2890
600 0.334 3470
700 0.389 4050
800 0.445 4620
900 0.501 5200
1000 0.556 5780
2000 1.11 1.16 × 104
3000 1.67 1.73 × 104
4000 2.22 2.31 × 104
5000 2.78 2.89 × 104
6000 3.34 3.47 × 104
7000 3.89 4.05 × 104
8000 4.45 4.62 × 104
9000 5.01 5.20 × 104
1.00 × 104 5.56 5.78 × 104
2.00 × 104 11.1 1.16 × 105
2.94 × 104 16.4 1.70 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.349 2320
300 0.407 2710
400 0.543 3610
500 0.679 4520
600 0.815 5420
700 0.951 6320
800 1.09 7230
900 1.22 8130
1000 1.36 9030
2000 2.72 1.81 × 104
3000 4.07 2.71 × 104
4000 5.43 3.61 × 104
5000 6.79 4.52 × 104
6000 8.15 5.42 × 104
7000 9.51 6.32 × 104
8000 10.9 7.23 × 104
9000 12.2 8.13 × 104
1.00 × 104 13.6 9.03 × 104
1.21 × 104 16.4 1.09 × 105
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 0.724 3340
300 0.845 3900
400 1.13 5200
500 1.41 6500
600 1.69 7800
700 1.97 9110
800 2.25 1.04 × 104
900 2.53 1.17 × 104
1000 2.82 1.30 × 104
2000 5.63 2.60 × 104
3000 8.45 3.90 × 104
4000 11.3 5.20 × 104
5000 14.1 6.50 × 104
5820 16.4 7.57 × 104
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 1.34 4550
300 1.57 5310
400 2.09 7080
500 2.61 8850
600 3.13 1.06 × 104
700 3.65 1.24 × 104
800 4.17 1.42 × 104
900 4.70 1.59 × 104
1000 5.22 1.77 × 104
2000 10.4 3.54 × 104
3000 15.7 5.31 × 104
3140 16.4 5.56 × 104
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 2.29 5940
300 2.67 6940
400 3.56 9250
500 4.45 1.16 × 104
600 5.34 1.39 × 104
700 6.23 1.62 × 104
800 7.12 1.85 × 104
900 8.01 2.08 × 104
1000 8.90 2.31 × 104
1840 16.4 4.26 × 104
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 3.66 7520
300 4.28 8780
400 5.70 1.17 × 104
500 7.13 1.46 × 104
600 8.55 1.76 × 104
700 9.98 2.05 × 104
800 11.4 2.34 × 104
900 12.8 2.63 × 104
1000 14.3 2.93 × 104
1150 16.4 3.36 × 104
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 5.58 9290
300 6.52 1.08 × 104
400 8.69 1.45 × 104
500 10.9 1.81 × 104
600 13.0 2.17 × 104
700 15.2 2.53 × 104
754 16.4 2.72 × 104
Steel I Beam: W14 × 257 (Wide Flange 14 inch tall × 257 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
257 13.6 1.45 × 104
300 15.9 1.69 × 104
309 16.4 1.74 × 104
Additional Information