engineering fundamentals
Wide Flange Steel I Beam: W14 × 398
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 398
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 6000 in4) for the W14 × 398 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 3.97 × 10-6 8.19
400 3.99 × 10-6 8.23
500 4.99 × 10-6 10.3
600 5.98 × 10-6 12.3
700 6.98 × 10-6 14.4
800 7.98 × 10-6 16.5
900 8.98 × 10-6 18.5
1000 9.97 × 10-6 20.6
2000 1.99 × 10-5 41.2
3000 2.99 × 10-5 61.7
4000 3.99 × 10-5 82.3
5000 4.99 × 10-5 103
6000 5.98 × 10-5 123
7000 6.98 × 10-5 144
8000 7.98 × 10-5 165
9000 8.98 × 10-5 185
1.00 × 104 9.97 × 10-5 206
2.00 × 104 1.99 × 10-4 412
3.00 × 104 2.99 × 10-4 617
4.00 × 104 3.99 × 10-4 823
5.00 × 104 4.99 × 10-4 1030
6.00 × 104 5.98 × 10-4 1230
7.00 × 104 6.98 × 10-4 1440
8.00 × 104 7.98 × 10-4 1650
9.00 × 104 8.98 × 10-4 1850
1.00 × 105 9.97 × 10-4 2060
2.00 × 105 0.00199 4120
3.00 × 105 0.00299 6170
4.00 × 105 0.00399 8230
5.00 × 105 0.00499 1.03 × 104
6.00 × 105 0.00598 1.23 × 104
7.00 × 105 0.00698 1.44 × 104
8.00 × 105 0.00798 1.65 × 104
9.00 × 105 0.00898 1.85 × 104
1.00 × 106 0.00997 2.06 × 104
2.00 × 106 0.0199 4.12 × 104
3.00 × 106 0.0299 6.17 × 104
4.00 × 106 0.0399 8.23 × 104
5.00 × 106 0.0499 1.03 × 105
6.00 × 106 0.0598 1.23 × 105
7.00 × 106 0.0698 1.44 × 105
8.00 × 106 0.0798 1.65 × 105
9.00 × 106 0.0898 1.85 × 105
1.00 × 107 0.0997 2.06 × 105
1.44 × 107 0.144 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 3.06 × 10-5 22.7
400 3.08 × 10-5 22.9
500 3.85 × 10-5 28.6
600 4.62 × 10-5 34.3
700 5.39 × 10-5 40.0
800 6.16 × 10-5 45.7
900 6.93 × 10-5 51.4
1000 7.70 × 10-5 57.2
2000 1.54 × 10-4 114
3000 2.31 × 10-4 171
4000 3.08 × 10-4 229
5000 3.85 × 10-4 286
6000 4.62 × 10-4 343
7000 5.39 × 10-4 400
8000 6.16 × 10-4 457
9000 6.93 × 10-4 514
1.00 × 104 7.70 × 10-4 572
2.00 × 104 0.00154 1140
3.00 × 104 0.00231 1710
4.00 × 104 0.00308 2290
5.00 × 104 0.00385 2860
6.00 × 104 0.00462 3430
7.00 × 104 0.00539 4000
8.00 × 104 0.00616 4570
9.00 × 104 0.00693 5140
1.00 × 105 0.00770 5720
2.00 × 105 0.0154 1.14 × 104
3.00 × 105 0.0231 1.71 × 104
4.00 × 105 0.0308 2.29 × 104
5.00 × 105 0.0385 2.86 × 104
6.00 × 105 0.0462 3.43 × 104
7.00 × 105 0.0539 4.00 × 104
8.00 × 105 0.0616 4.57 × 104
9.00 × 105 0.0693 5.14 × 104
1.00 × 106 0.0770 5.72 × 104
2.00 × 106 0.154 1.14 × 105
3.00 × 106 0.231 1.71 × 105
4.00 × 106 0.308 2.29 × 105
5.00 × 106 0.385 2.86 × 105
5.20 × 106 0.400 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 4.90 × 10-4 91.0
400 4.92 × 10-4 91.5
500 6.16 × 10-4 114
600 7.39 × 10-4 137
700 8.62 × 10-4 160
800 9.85 × 10-4 183
900 0.00111 206
1000 0.00123 229
2000 0.00246 457
3000 0.00369 686
4000 0.00492 915
5000 0.00616 1140
6000 0.00739 1370
7000 0.00862 1600
8000 0.00985 1830
9000 0.0111 2060
1.00 × 104 0.0123 2290
2.00 × 104 0.0246 4570
3.00 × 104 0.0369 6860
4.00 × 104 0.0492 9150
5.00 × 104 0.0616 1.14 × 104
6.00 × 104 0.0739 1.37 × 104
7.00 × 104 0.0862 1.60 × 104
8.00 × 104 0.0985 1.83 × 104
9.00 × 104 0.111 2.06 × 104
1.00 × 105 0.123 2.29 × 104
2.00 × 105 0.246 4.57 × 104
3.00 × 105 0.369 6.86 × 104
4.00 × 105 0.492 9.15 × 104
5.00 × 105 0.616 1.14 × 105
6.00 × 105 0.739 1.37 × 105
7.00 × 105 0.862 1.60 × 105
8.00 × 105 0.985 1.83 × 105
9.00 × 105 1.11 2.06 × 105
1.00 × 106 1.23 2.29 × 105
1.30 × 106 1.60 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.00248 205
400 0.00249 206
500 0.00312 257
600 0.00374 309
700 0.00436 360
800 0.00499 412
900 0.00561 463
1000 0.00623 514
2000 0.0125 1030
3000 0.0187 1540
4000 0.0249 2060
5000 0.0312 2570
6000 0.0374 3090
7000 0.0436 3600
8000 0.0499 4120
9000 0.0561 4630
1.00 × 104 0.0623 5140
2.00 × 104 0.125 1.03 × 104
3.00 × 104 0.187 1.54 × 104
4.00 × 104 0.249 2.06 × 104
5.00 × 104 0.312 2.57 × 104
6.00 × 104 0.374 3.09 × 104
7.00 × 104 0.436 3.60 × 104
8.00 × 104 0.499 4.12 × 104
9.00 × 104 0.561 4.63 × 104
1.00 × 105 0.623 5.14 × 104
2.00 × 105 1.25 1.03 × 105
3.00 × 105 1.87 1.54 × 105
4.00 × 105 2.49 2.06 × 105
5.00 × 105 3.12 2.57 × 105
5.77 × 105 3.60 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.00784 364
400 0.00788 366
500 0.00985 457
600 0.0118 549
700 0.0138 640
800 0.0158 732
900 0.0177 823
1000 0.0197 915
2000 0.0394 1830
3000 0.0591 2740
4000 0.0788 3660
5000 0.0985 4570
6000 0.118 5490
7000 0.138 6400
8000 0.158 7320
9000 0.177 8230
1.00 × 104 0.197 9150
2.00 × 104 0.394 1.83 × 104
3.00 × 104 0.591 2.74 × 104
4.00 × 104 0.788 3.66 × 104
5.00 × 104 0.985 4.57 × 104
6.00 × 104 1.18 5.49 × 104
7.00 × 104 1.38 6.40 × 104
8.00 × 104 1.58 7.32 × 104
9.00 × 104 1.77 8.23 × 104
1.00 × 105 1.97 9.15 × 104
2.00 × 105 3.94 1.83 × 105
3.00 × 105 5.91 2.74 × 105
3.25 × 105 6.40 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.0191 569
400 0.0192 572
500 0.0240 714
600 0.0289 857
700 0.0337 1000
800 0.0385 1140
900 0.0433 1290
1000 0.0481 1430
2000 0.0962 2860
3000 0.144 4290
4000 0.192 5720
5000 0.240 7140
6000 0.289 8570
7000 0.337 1.00 × 104
8000 0.385 1.14 × 104
9000 0.433 1.29 × 104
1.00 × 104 0.481 1.43 × 104
2.00 × 104 0.962 2.86 × 104
3.00 × 104 1.44 4.29 × 104
4.00 × 104 1.92 5.72 × 104
5.00 × 104 2.40 7.14 × 104
6.00 × 104 2.89 8.57 × 104
7.00 × 104 3.37 1.00 × 105
8.00 × 104 3.85 1.14 × 105
9.00 × 104 4.33 1.29 × 105
1.00 × 105 4.81 1.43 × 105
2.00 × 105 9.62 2.86 × 105
2.08 × 105 10.0 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.0397 819
400 0.0399 823
500 0.0499 1030
600 0.0598 1230
700 0.0698 1440
800 0.0798 1650
900 0.0898 1850
1000 0.0997 2060
2000 0.199 4120
3000 0.299 6170
4000 0.399 8230
5000 0.499 1.03 × 104
6000 0.598 1.23 × 104
7000 0.698 1.44 × 104
8000 0.798 1.65 × 104
9000 0.898 1.85 × 104
1.00 × 104 0.997 2.06 × 104
2.00 × 104 1.99 4.12 × 104
3.00 × 104 2.99 6.17 × 104
4.00 × 104 3.99 8.23 × 104
5.00 × 104 4.99 1.03 × 105
6.00 × 104 5.98 1.23 × 105
7.00 × 104 6.98 1.44 × 105
8.00 × 104 7.98 1.65 × 105
9.00 × 104 8.98 1.85 × 105
1.00 × 105 9.97 2.06 × 105
1.44 × 105 14.4 2.97 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.125 1460
400 0.126 1460
500 0.158 1830
600 0.189 2190
700 0.221 2560
800 0.252 2930
900 0.284 3290
1000 0.315 3660
2000 0.630 7320
3000 0.946 1.10 × 104
4000 1.26 1.46 × 104
5000 1.58 1.83 × 104
6000 1.89 2.19 × 104
7000 2.21 2.56 × 104
8000 2.52 2.93 × 104
9000 2.84 3.29 × 104
1.00 × 104 3.15 3.66 × 104
2.00 × 104 6.30 7.32 × 104
3.00 × 104 9.46 1.10 × 105
4.00 × 104 12.6 1.46 × 105
5.00 × 104 15.8 1.83 × 105
5.80 × 104 18.3 2.12 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.306 2270
400 0.308 2290
500 0.385 2860
600 0.462 3430
700 0.539 4000
800 0.616 4570
900 0.693 5140
1000 0.770 5720
2000 1.54 1.14 × 104
3000 2.31 1.71 × 104
4000 3.08 2.29 × 104
5000 3.85 2.86 × 104
6000 4.62 3.43 × 104
7000 5.39 4.00 × 104
8000 6.16 4.57 × 104
9000 6.93 5.14 × 104
1.00 × 104 7.70 5.72 × 104
2.00 × 104 15.4 1.14 × 105
2.38 × 104 18.3 1.36 × 105
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 0.635 3280
400 0.638 3290
500 0.798 4120
600 0.957 4940
700 1.12 5760
800 1.28 6580
900 1.44 7410
1000 1.60 8230
2000 3.19 1.65 × 104
3000 4.79 2.47 × 104
4000 6.38 3.29 × 104
5000 7.98 4.12 × 104
6000 9.57 4.94 × 104
7000 11.2 5.76 × 104
8000 12.8 6.58 × 104
9000 14.4 7.41 × 104
1.00 × 104 16.0 8.23 × 104
1.15 × 104 18.3 9.43 × 104
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 1.18 4460
400 1.18 4480
500 1.48 5600
600 1.77 6720
700 2.07 7840
800 2.36 8960
900 2.66 1.01 × 104
1000 2.96 1.12 × 104
2000 5.91 2.24 × 104
3000 8.87 3.36 × 104
4000 11.8 4.48 × 104
5000 14.8 5.60 × 104
6000 17.7 6.72 × 104
6190 18.3 6.93 × 104
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 2.01 5820
400 2.02 5850
500 2.52 7320
600 3.03 8780
700 3.53 1.02 × 104
800 4.03 1.17 × 104
900 4.54 1.32 × 104
1000 5.04 1.46 × 104
2000 10.1 2.93 × 104
3000 15.1 4.39 × 104
3630 18.3 5.31 × 104
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 3.22 7370
400 3.23 7410
500 4.04 9260
600 4.85 1.11 × 104
700 5.65 1.30 × 104
800 6.46 1.48 × 104
900 7.27 1.67 × 104
1000 8.08 1.85 × 104
2000 16.2 3.70 × 104
2260 18.3 4.19 × 104
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 4.90 9100
400 4.92 9150
500 6.16 1.14 × 104
600 7.39 1.37 × 104
700 8.62 1.60 × 104
800 9.85 1.83 × 104
900 11.1 2.06 × 104
1000 12.3 2.29 × 104
1490 18.3 3.40 × 104
Steel I Beam: W14 × 398 (Wide Flange 14 inch tall × 398 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
398 12.0 1.42 × 104
400 12.0 1.43 × 104
500 15.0 1.79 × 104
600 18.0 2.14 × 104
608 18.3 2.17 × 104
Additional Information
Home  About Us  Privacy  Disclaimer  Contact 

Copyright © 2020 eFunda, Inc.