engineering fundamentals
Wide Flange Steel I Beam: W14 × 90
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 90
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 999 in4) for the W14 × 90 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
  
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 5.39 × 10-6 8.53
100 5.99 × 10-6 9.47
200 1.20 × 10-5 18.9
300 1.80 × 10-5 28.4
400 2.40 × 10-5 37.9
500 2.99 × 10-5 47.4
600 3.59 × 10-5 56.8
700 4.19 × 10-5 66.3
800 4.79 × 10-5 75.8
900 5.39 × 10-5 85.3
1000 5.99 × 10-5 94.7
2000 1.20 × 10-4 189
3000 1.80 × 10-4 284
4000 2.40 × 10-4 379
5000 2.99 × 10-4 474
6000 3.59 × 10-4 568
7000 4.19 × 10-4 663
8000 4.79 × 10-4 758
9000 5.39 × 10-4 853
1.00 × 104 5.99 × 10-4 947
2.00 × 104 0.00120 1890
3.00 × 104 0.00180 2840
4.00 × 104 0.00240 3790
5.00 × 104 0.00299 4740
6.00 × 104 0.00359 5680
7.00 × 104 0.00419 6630
8.00 × 104 0.00479 7580
9.00 × 104 0.00539 8530
1.00 × 105 0.00599 9470
2.00 × 105 0.0120 1.89 × 104
3.00 × 105 0.0180 2.84 × 104
4.00 × 105 0.0240 3.79 × 104
5.00 × 105 0.0299 4.74 × 104
6.00 × 105 0.0359 5.68 × 104
7.00 × 105 0.0419 6.63 × 104
8.00 × 105 0.0479 7.58 × 104
9.00 × 105 0.0539 8.53 × 104
1.00 × 106 0.0599 9.47 × 104
2.00 × 106 0.120 1.89 × 105
3.00 × 106 0.180 2.84 × 105
3.14 × 106 0.188 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 4.16 × 10-5 23.7
100 4.62 × 10-5 26.3
200 9.24 × 10-5 52.6
300 1.39 × 10-4 78.9
400 1.85 × 10-4 105
500 2.31 × 10-4 132
600 2.77 × 10-4 158
700 3.24 × 10-4 184
800 3.70 × 10-4 211
900 4.16 × 10-4 237
1000 4.62 × 10-4 263
2000 9.24 × 10-4 526
3000 0.00139 789
4000 0.00185 1050
5000 0.00231 1320
6000 0.00277 1580
7000 0.00324 1840
8000 0.00370 2110
9000 0.00416 2370
1.00 × 104 0.00462 2630
2.00 × 104 0.00924 5260
3.00 × 104 0.0139 7890
4.00 × 104 0.0185 1.05 × 104
5.00 × 104 0.0231 1.32 × 104
6.00 × 104 0.0277 1.58 × 104
7.00 × 104 0.0324 1.84 × 104
8.00 × 104 0.0370 2.11 × 104
9.00 × 104 0.0416 2.37 × 104
1.00 × 105 0.0462 2.63 × 104
2.00 × 105 0.0924 5.26 × 104
3.00 × 105 0.139 7.89 × 104
4.00 × 105 0.185 1.05 × 105
5.00 × 105 0.231 1.32 × 105
6.00 × 105 0.277 1.58 × 105
7.00 × 105 0.324 1.84 × 105
8.00 × 105 0.370 2.11 × 105
9.00 × 105 0.416 2.37 × 105
1.00 × 106 0.462 2.63 × 105
1.13 × 106 0.522 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 6.66 × 10-4 94.7
100 7.39 × 10-4 105
200 0.00148 211
300 0.00222 316
400 0.00296 421
500 0.00370 526
600 0.00444 632
700 0.00518 737
800 0.00592 842
900 0.00666 947
1000 0.00739 1050
2000 0.0148 2110
3000 0.0222 3160
4000 0.0296 4210
5000 0.0370 5260
6000 0.0444 6320
7000 0.0518 7370
8000 0.0592 8420
9000 0.0666 9470
1.00 × 104 0.0739 1.05 × 104
2.00 × 104 0.148 2.11 × 104
3.00 × 104 0.222 3.16 × 104
4.00 × 104 0.296 4.21 × 104
5.00 × 104 0.370 5.26 × 104
6.00 × 104 0.444 6.32 × 104
7.00 × 104 0.518 7.37 × 104
8.00 × 104 0.592 8.42 × 104
9.00 × 104 0.666 9.47 × 104
1.00 × 105 0.739 1.05 × 105
2.00 × 105 1.48 2.11 × 105
2.82 × 105 2.09 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.00337 213
100 0.00374 237
200 0.00749 474
300 0.0112 710
400 0.0150 947
500 0.0187 1180
600 0.0225 1420
700 0.0262 1660
800 0.0299 1890
900 0.0337 2130
1000 0.0374 2370
2000 0.0749 4740
3000 0.112 7100
4000 0.150 9470
5000 0.187 1.18 × 104
6000 0.225 1.42 × 104
7000 0.262 1.66 × 104
8000 0.299 1.89 × 104
9000 0.337 2.13 × 104
1.00 × 104 0.374 2.37 × 104
2.00 × 104 0.749 4.74 × 104
3.00 × 104 1.12 7.10 × 104
4.00 × 104 1.50 9.47 × 104
5.00 × 104 1.87 1.18 × 105
6.00 × 104 2.25 1.42 × 105
7.00 × 104 2.62 1.66 × 105
8.00 × 104 2.99 1.89 × 105
9.00 × 104 3.37 2.13 × 105
1.00 × 105 3.74 2.37 × 105
1.25 × 105 4.70 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.0106 379
100 0.0118 421
200 0.0237 842
300 0.0355 1260
400 0.0473 1680
500 0.0592 2110
600 0.0710 2530
700 0.0828 2950
800 0.0947 3370
900 0.106 3790
1000 0.118 4210
2000 0.237 8420
3000 0.355 1.26 × 104
4000 0.473 1.68 × 104
5000 0.592 2.11 × 104
6000 0.710 2.53 × 104
7000 0.828 2.95 × 104
8000 0.947 3.37 × 104
9000 1.06 3.79 × 104
1.00 × 104 1.18 4.21 × 104
2.00 × 104 2.37 8.42 × 104
3.00 × 104 3.55 1.26 × 105
4.00 × 104 4.73 1.68 × 105
5.00 × 104 5.92 2.11 × 105
6.00 × 104 7.10 2.53 × 105
7.00 × 104 8.28 2.95 × 105
7.06 × 104 8.35 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.0260 592
100 0.0289 658
200 0.0578 1320
300 0.0867 1970
400 0.116 2630
500 0.144 3290
600 0.173 3950
700 0.202 4600
800 0.231 5260
900 0.260 5920
1000 0.289 6580
2000 0.578 1.32 × 104
3000 0.867 1.97 × 104
4000 1.16 2.63 × 104
5000 1.44 3.29 × 104
6000 1.73 3.95 × 104
7000 2.02 4.60 × 104
8000 2.31 5.26 × 104
9000 2.60 5.92 × 104
1.00 × 104 2.89 6.58 × 104
2.00 × 104 5.78 1.32 × 105
3.00 × 104 8.67 1.97 × 105
4.00 × 104 11.6 2.63 × 105
4.52 × 104 13.0 2.97 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.0539 853
100 0.0599 947
200 0.120 1890
300 0.180 2840
400 0.240 3790
500 0.299 4740
600 0.359 5680
700 0.419 6630
800 0.479 7580
900 0.539 8530
1000 0.599 9470
2000 1.20 1.89 × 104
3000 1.80 2.84 × 104
4000 2.40 3.79 × 104
5000 2.99 4.74 × 104
6000 3.59 5.68 × 104
7000 4.19 6.63 × 104
8000 4.79 7.58 × 104
9000 5.39 8.53 × 104
1.00 × 104 5.99 9.47 × 104
2.00 × 104 12.0 1.89 × 105
2.34 × 104 14.0 2.22 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.170 1520
100 0.189 1680
200 0.379 3370
300 0.568 5050
400 0.757 6740
500 0.947 8420
600 1.14 1.01 × 104
700 1.33 1.18 × 104
800 1.51 1.35 × 104
900 1.70 1.52 × 104
1000 1.89 1.68 × 104
2000 3.79 3.37 × 104
3000 5.68 5.05 × 104
4000 7.57 6.74 × 104
5000 9.47 8.42 × 104
6000 11.4 1.01 × 105
7000 13.3 1.18 × 105
7410 14.0 1.25 × 105
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.416 2370
100 0.462 2630
200 0.924 5260
300 1.39 7890
400 1.85 1.05 × 104
500 2.31 1.32 × 104
600 2.77 1.58 × 104
700 3.24 1.84 × 104
800 3.70 2.11 × 104
900 4.16 2.37 × 104
1000 4.62 2.63 × 104
2000 9.24 5.26 × 104
3000 13.9 7.89 × 104
3030 14.0 7.98 × 104
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 0.863 3410
100 0.958 3790
200 1.92 7580
300 2.88 1.14 × 104
400 3.83 1.52 × 104
500 4.79 1.89 × 104
600 5.75 2.27 × 104
700 6.71 2.65 × 104
800 7.67 3.03 × 104
900 8.63 3.41 × 104
1000 9.58 3.79 × 104
1460 14.0 5.54 × 104
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 1.60 4640
100 1.78 5160
200 3.55 1.03 × 104
300 5.33 1.55 × 104
400 7.10 2.06 × 104
500 8.88 2.58 × 104
600 10.7 3.09 × 104
700 12.4 3.61 × 104
790 14.0 4.07 × 104
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 2.73 6060
100 3.03 6740
200 6.06 1.35 × 104
300 9.09 2.02 × 104
400 12.1 2.69 × 104
463 14.0 3.12 × 104
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 4.37 7670
100 4.85 8530
200 9.70 1.71 × 104
289 14.0 2.46 × 104
Steel I Beam: W14 × 90 (Wide Flange 14 inch tall × 90 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
90.0 6.66 9470
100 7.39 1.05 × 104
190 14.0 2.00 × 104
Additional Information
Home  About Us  Privacy  Disclaimer  Contact 