engineering fundamentals
Wide Flange Steel I Beam: W14 × 99
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 99
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1110 in4) for the W14 × 99 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
  
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 5.34 × 10-6 8.52
100 5.39 × 10-6 8.61
200 1.08 × 10-5 17.2
300 1.62 × 10-5 25.8
400 2.16 × 10-5 34.4
500 2.70 × 10-5 43.1
600 3.23 × 10-5 51.7
700 3.77 × 10-5 60.3
800 4.31 × 10-5 68.9
900 4.85 × 10-5 77.5
1000 5.39 × 10-5 86.1
2000 1.08 × 10-4 172
3000 1.62 × 10-4 258
4000 2.16 × 10-4 344
5000 2.70 × 10-4 431
6000 3.23 × 10-4 517
7000 3.77 × 10-4 603
8000 4.31 × 10-4 689
9000 4.85 × 10-4 775
1.00 × 104 5.39 × 10-4 861
2.00 × 104 0.00108 1720
3.00 × 104 0.00162 2580
4.00 × 104 0.00216 3440
5.00 × 104 0.00270 4310
6.00 × 104 0.00323 5170
7.00 × 104 0.00377 6030
8.00 × 104 0.00431 6890
9.00 × 104 0.00485 7750
1.00 × 105 0.00539 8610
2.00 × 105 0.0108 1.72 × 104
3.00 × 105 0.0162 2.58 × 104
4.00 × 105 0.0216 3.44 × 104
5.00 × 105 0.0270 4.31 × 104
6.00 × 105 0.0323 5.17 × 104
7.00 × 105 0.0377 6.03 × 104
8.00 × 105 0.0431 6.89 × 104
9.00 × 105 0.0485 7.75 × 104
1.00 × 106 0.0539 8.61 × 104
2.00 × 106 0.108 1.72 × 105
3.00 × 106 0.162 2.58 × 105
3.45 × 106 0.186 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 4.12 × 10-5 23.7
100 4.16 × 10-5 23.9
200 8.32 × 10-5 47.8
300 1.25 × 10-4 71.8
400 1.66 × 10-4 95.7
500 2.08 × 10-4 120
600 2.50 × 10-4 144
700 2.91 × 10-4 167
800 3.33 × 10-4 191
900 3.74 × 10-4 215
1000 4.16 × 10-4 239
2000 8.32 × 10-4 478
3000 0.00125 718
4000 0.00166 957
5000 0.00208 1200
6000 0.00250 1440
7000 0.00291 1670
8000 0.00333 1910
9000 0.00374 2150
1.00 × 104 0.00416 2390
2.00 × 104 0.00832 4780
3.00 × 104 0.0125 7180
4.00 × 104 0.0166 9570
5.00 × 104 0.0208 1.20 × 104
6.00 × 104 0.0250 1.44 × 104
7.00 × 104 0.0291 1.67 × 104
8.00 × 104 0.0333 1.91 × 104
9.00 × 104 0.0374 2.15 × 104
1.00 × 105 0.0416 2.39 × 104
2.00 × 105 0.0832 4.78 × 104
3.00 × 105 0.125 7.18 × 104
4.00 × 105 0.166 9.57 × 104
5.00 × 105 0.208 1.20 × 105
6.00 × 105 0.250 1.44 × 105
7.00 × 105 0.291 1.67 × 105
8.00 × 105 0.333 1.91 × 105
9.00 × 105 0.374 2.15 × 105
1.00 × 106 0.416 2.39 × 105
1.24 × 106 0.517 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 6.59 × 10-4 94.7
100 6.66 × 10-4 95.7
200 0.00133 191
300 0.00200 287
400 0.00266 383
500 0.00333 478
600 0.00399 574
700 0.00466 670
800 0.00532 765
900 0.00599 861
1000 0.00666 957
2000 0.0133 1910
3000 0.0200 2870
4000 0.0266 3830
5000 0.0333 4780
6000 0.0399 5740
7000 0.0466 6700
8000 0.0532 7650
9000 0.0599 8610
1.00 × 104 0.0666 9570
2.00 × 104 0.133 1.91 × 104
3.00 × 104 0.200 2.87 × 104
4.00 × 104 0.266 3.83 × 104
5.00 × 104 0.333 4.78 × 104
6.00 × 104 0.399 5.74 × 104
7.00 × 104 0.466 6.70 × 104
8.00 × 104 0.532 7.65 × 104
9.00 × 104 0.599 8.61 × 104
1.00 × 105 0.666 9.57 × 104
2.00 × 105 1.33 1.91 × 105
3.00 × 105 2.00 2.87 × 105
3.10 × 105 2.07 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.00334 213
100 0.00337 215
200 0.00674 431
300 0.0101 646
400 0.0135 861
500 0.0168 1080
600 0.0202 1290
700 0.0236 1510
800 0.0270 1720
900 0.0303 1940
1000 0.0337 2150
2000 0.0674 4310
3000 0.101 6460
4000 0.135 8610
5000 0.168 1.08 × 104
6000 0.202 1.29 × 104
7000 0.236 1.51 × 104
8000 0.270 1.72 × 104
9000 0.303 1.94 × 104
1.00 × 104 0.337 2.15 × 104
2.00 × 104 0.674 4.31 × 104
3.00 × 104 1.01 6.46 × 104
4.00 × 104 1.35 8.61 × 104
5.00 × 104 1.68 1.08 × 105
6.00 × 104 2.02 1.29 × 105
7.00 × 104 2.36 1.51 × 105
8.00 × 104 2.70 1.72 × 105
9.00 × 104 3.03 1.94 × 105
1.00 × 105 3.37 2.15 × 105
1.38 × 105 4.65 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.0105 379
100 0.0106 383
200 0.0213 765
300 0.0319 1150
400 0.0426 1530
500 0.0532 1910
600 0.0639 2300
700 0.0745 2680
800 0.0852 3060
900 0.0958 3440
1000 0.106 3830
2000 0.213 7650
3000 0.319 1.15 × 104
4000 0.426 1.53 × 104
5000 0.532 1.91 × 104
6000 0.639 2.30 × 104
7000 0.745 2.68 × 104
8000 0.852 3.06 × 104
9000 0.958 3.44 × 104
1.00 × 104 1.06 3.83 × 104
2.00 × 104 2.13 7.65 × 104
3.00 × 104 3.19 1.15 × 105
4.00 × 104 4.26 1.53 × 105
5.00 × 104 5.32 1.91 × 105
6.00 × 104 6.39 2.30 × 105
7.00 × 104 7.45 2.68 × 105
7.76 × 104 8.26 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.0257 592
100 0.0260 598
200 0.0520 1200
300 0.0780 1790
400 0.104 2390
500 0.130 2990
600 0.156 3590
700 0.182 4190
800 0.208 4780
900 0.234 5380
1000 0.260 5980
2000 0.520 1.20 × 104
3000 0.780 1.79 × 104
4000 1.04 2.39 × 104
5000 1.30 2.99 × 104
6000 1.56 3.59 × 104
7000 1.82 4.19 × 104
8000 2.08 4.78 × 104
9000 2.34 5.38 × 104
1.00 × 104 2.60 5.98 × 104
2.00 × 104 5.20 1.20 × 105
3.00 × 104 7.80 1.79 × 105
4.00 × 104 10.4 2.39 × 105
4.97 × 104 12.9 2.97 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.0534 852
100 0.0539 861
200 0.108 1720
300 0.162 2580
400 0.216 3440
500 0.270 4310
600 0.323 5170
700 0.377 6030
800 0.431 6890
900 0.485 7750
1000 0.539 8610
2000 1.08 1.72 × 104
3000 1.62 2.58 × 104
4000 2.16 3.44 × 104
5000 2.70 4.31 × 104
6000 3.23 5.17 × 104
7000 3.77 6.03 × 104
8000 4.31 6.89 × 104
9000 4.85 7.75 × 104
1.00 × 104 5.39 8.61 × 104
2.00 × 104 10.8 1.72 × 105
2.63 × 104 14.2 2.26 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.169 1520
100 0.170 1530
200 0.341 3060
300 0.511 4590
400 0.681 6120
500 0.852 7650
600 1.02 9180
700 1.19 1.07 × 104
800 1.36 1.22 × 104
900 1.53 1.38 × 104
1000 1.70 1.53 × 104
2000 3.41 3.06 × 104
3000 5.11 4.59 × 104
4000 6.81 6.12 × 104
5000 8.52 7.65 × 104
6000 10.2 9.18 × 104
7000 11.9 1.07 × 105
8000 13.6 1.22 × 105
8310 14.2 1.27 × 105
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.412 2370
100 0.416 2390
200 0.832 4780
300 1.25 7180
400 1.66 9570
500 2.08 1.20 × 104
600 2.50 1.44 × 104
700 2.91 1.67 × 104
800 3.33 1.91 × 104
900 3.74 2.15 × 104
1000 4.16 2.39 × 104
2000 8.32 4.78 × 104
3000 12.5 7.18 × 104
3400 14.2 8.14 × 104
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 0.854 3410
100 0.863 3440
200 1.73 6890
300 2.59 1.03 × 104
400 3.45 1.38 × 104
500 4.31 1.72 × 104
600 5.18 2.07 × 104
700 6.04 2.41 × 104
800 6.90 2.76 × 104
900 7.76 3.10 × 104
1000 8.63 3.44 × 104
1640 14.2 5.65 × 104
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 1.58 4640
100 1.60 4690
200 3.20 9380
300 4.79 1.41 × 104
400 6.39 1.88 × 104
500 7.99 2.34 × 104
600 9.59 2.81 × 104
700 11.2 3.28 × 104
800 12.8 3.75 × 104
886 14.2 4.15 × 104
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 2.70 6060
100 2.73 6120
200 5.45 1.22 × 104
300 8.18 1.84 × 104
400 10.9 2.45 × 104
500 13.6 3.06 × 104
519 14.2 3.18 × 104
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 4.32 7670
100 4.37 7750
200 8.73 1.55 × 104
300 13.1 2.32 × 104
324 14.2 2.51 × 104
Steel I Beam: W14 × 99 (Wide Flange 14 inch tall × 99 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
99.0 6.59 9470
100 6.66 9570
200 13.3 1.91 × 104
213 14.2 2.04 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.