engineering fundamentals
Wide Flange Steel I Beam: W24 × 104
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W24 × 104
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 3100 in4) for the W24 × 104 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 2.01 × 10-6 5.45
200 3.86 × 10-6 10.5
300 5.79 × 10-6 15.7
400 7.72 × 10-6 21.0
500 9.65 × 10-6 26.2
600 1.16 × 10-5 31.4
700 1.35 × 10-5 36.7
800 1.54 × 10-5 41.9
900 1.74 × 10-5 47.1
1000 1.93 × 10-5 52.4
2000 3.86 × 10-5 105
3000 5.79 × 10-5 157
4000 7.72 × 10-5 210
5000 9.65 × 10-5 262
6000 1.16 × 10-4 314
7000 1.35 × 10-4 367
8000 1.54 × 10-4 419
9000 1.74 × 10-4 471
1.00 × 104 1.93 × 10-4 524
2.00 × 104 3.86 × 10-4 1050
3.00 × 104 5.79 × 10-4 1570
4.00 × 104 7.72 × 10-4 2100
5.00 × 104 9.65 × 10-4 2620
6.00 × 104 0.00116 3140
7.00 × 104 0.00135 3670
8.00 × 104 0.00154 4190
9.00 × 104 0.00174 4710
1.00 × 105 0.00193 5240
2.00 × 105 0.00386 1.05 × 104
3.00 × 105 0.00579 1.57 × 104
4.00 × 105 0.00772 2.10 × 104
5.00 × 105 0.00965 2.62 × 104
6.00 × 105 0.0116 3.14 × 104
7.00 × 105 0.0135 3.67 × 104
8.00 × 105 0.0154 4.19 × 104
9.00 × 105 0.0174 4.71 × 104
1.00 × 106 0.0193 5.24 × 104
2.00 × 106 0.0386 1.05 × 105
3.00 × 106 0.0579 1.57 × 105
4.00 × 106 0.0772 2.10 × 105
5.00 × 106 0.0965 2.62 × 105
5.67 × 106 0.109 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 1.55 × 10-5 15.1
200 2.98 × 10-5 29.1
300 4.47 × 10-5 43.7
400 5.96 × 10-5 58.2
500 7.45 × 10-5 72.8
600 8.94 × 10-5 87.3
700 1.04 × 10-4 102
800 1.19 × 10-4 116
900 1.34 × 10-4 131
1000 1.49 × 10-4 146
2000 2.98 × 10-4 291
3000 4.47 × 10-4 437
4000 5.96 × 10-4 582
5000 7.45 × 10-4 728
6000 8.94 × 10-4 873
7000 0.00104 1020
8000 0.00119 1160
9000 0.00134 1310
1.00 × 104 0.00149 1460
2.00 × 104 0.00298 2910
3.00 × 104 0.00447 4370
4.00 × 104 0.00596 5820
5.00 × 104 0.00745 7280
6.00 × 104 0.00894 8730
7.00 × 104 0.0104 1.02 × 104
8.00 × 104 0.0119 1.16 × 104
9.00 × 104 0.0134 1.31 × 104
1.00 × 105 0.0149 1.46 × 104
2.00 × 105 0.0298 2.91 × 104
3.00 × 105 0.0447 4.37 × 104
4.00 × 105 0.0596 5.82 × 104
5.00 × 105 0.0745 7.28 × 104
6.00 × 105 0.0894 8.73 × 104
7.00 × 105 0.104 1.02 × 105
8.00 × 105 0.119 1.16 × 105
9.00 × 105 0.134 1.31 × 105
1.00 × 106 0.149 1.46 × 105
2.00 × 106 0.298 2.91 × 105
2.04 × 106 0.304 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 2.48 × 10-4 60.5
200 4.77 × 10-4 116
300 7.15 × 10-4 175
400 9.53 × 10-4 233
500 0.00119 291
600 0.00143 349
700 0.00167 407
800 0.00191 466
900 0.00214 524
1000 0.00238 582
2000 0.00477 1160
3000 0.00715 1750
4000 0.00953 2330
5000 0.0119 2910
6000 0.0143 3490
7000 0.0167 4070
8000 0.0191 4660
9000 0.0214 5240
1.00 × 104 0.0238 5820
2.00 × 104 0.0477 1.16 × 104
3.00 × 104 0.0715 1.75 × 104
4.00 × 104 0.0953 2.33 × 104
5.00 × 104 0.119 2.91 × 104
6.00 × 104 0.143 3.49 × 104
7.00 × 104 0.167 4.07 × 104
8.00 × 104 0.191 4.66 × 104
9.00 × 104 0.214 5.24 × 104
1.00 × 105 0.238 5.82 × 104
2.00 × 105 0.477 1.16 × 105
3.00 × 105 0.715 1.75 × 105
4.00 × 105 0.953 2.33 × 105
5.00 × 105 1.19 2.91 × 105
5.10 × 105 1.22 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.00125 136
200 0.00241 262
300 0.00362 393
400 0.00483 524
500 0.00603 655
600 0.00724 786
700 0.00844 917
800 0.00965 1050
900 0.0109 1180
1000 0.0121 1310
2000 0.0241 2620
3000 0.0362 3930
4000 0.0483 5240
5000 0.0603 6550
6000 0.0724 7860
7000 0.0844 9170
8000 0.0965 1.05 × 104
9000 0.109 1.18 × 104
1.00 × 104 0.121 1.31 × 104
2.00 × 104 0.241 2.62 × 104
3.00 × 104 0.362 3.93 × 104
4.00 × 104 0.483 5.24 × 104
5.00 × 104 0.603 6.55 × 104
6.00 × 104 0.724 7.86 × 104
7.00 × 104 0.844 9.17 × 104
8.00 × 104 0.965 1.05 × 105
9.00 × 104 1.09 1.18 × 105
1.00 × 105 1.21 1.31 × 105
2.00 × 105 2.41 2.62 × 105
2.27 × 105 2.74 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.00397 242
200 0.00763 466
300 0.0114 699
400 0.0153 931
500 0.0191 1160
600 0.0229 1400
700 0.0267 1630
800 0.0305 1860
900 0.0343 2100
1000 0.0381 2330
2000 0.0763 4660
3000 0.114 6990
4000 0.153 9310
5000 0.191 1.16 × 104
6000 0.229 1.40 × 104
7000 0.267 1.63 × 104
8000 0.305 1.86 × 104
9000 0.343 2.10 × 104
1.00 × 104 0.381 2.33 × 104
2.00 × 104 0.763 4.66 × 104
3.00 × 104 1.14 6.99 × 104
4.00 × 104 1.53 9.31 × 104
5.00 × 104 1.91 1.16 × 105
6.00 × 104 2.29 1.40 × 105
7.00 × 104 2.67 1.63 × 105
8.00 × 104 3.05 1.86 × 105
9.00 × 104 3.43 2.10 × 105
1.00 × 105 3.81 2.33 × 105
1.28 × 105 4.86 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.00968 378
200 0.0186 728
300 0.0279 1090
400 0.0372 1460
500 0.0465 1820
600 0.0559 2180
700 0.0652 2550
800 0.0745 2910
900 0.0838 3270
1000 0.0931 3640
2000 0.186 7280
3000 0.279 1.09 × 104
4000 0.372 1.46 × 104
5000 0.465 1.82 × 104
6000 0.559 2.18 × 104
7000 0.652 2.55 × 104
8000 0.745 2.91 × 104
9000 0.838 3.27 × 104
1.00 × 104 0.931 3.64 × 104
2.00 × 104 1.86 7.28 × 104
3.00 × 104 2.79 1.09 × 105
4.00 × 104 3.72 1.46 × 105
5.00 × 104 4.65 1.82 × 105
6.00 × 104 5.59 2.18 × 105
7.00 × 104 6.52 2.55 × 105
8.00 × 104 7.45 2.91 × 105
8.16 × 104 7.60 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.0201 545
200 0.0386 1050
300 0.0579 1570
400 0.0772 2100
500 0.0965 2620
600 0.116 3140
700 0.135 3670
800 0.154 4190
900 0.174 4710
1000 0.193 5240
2000 0.386 1.05 × 104
3000 0.579 1.57 × 104
4000 0.772 2.10 × 104
5000 0.965 2.62 × 104
6000 1.16 3.14 × 104
7000 1.35 3.67 × 104
8000 1.54 4.19 × 104
9000 1.74 4.71 × 104
1.00 × 104 1.93 5.24 × 104
2.00 × 104 3.86 1.05 × 105
3.00 × 104 5.79 1.57 × 105
4.00 × 104 7.72 2.10 × 105
5.00 × 104 9.65 2.62 × 105
5.67 × 104 10.9 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.0634 969
200 0.122 1860
300 0.183 2790
400 0.244 3730
500 0.305 4660
600 0.366 5590
700 0.427 6520
800 0.488 7450
900 0.549 8380
1000 0.610 9310
2000 1.22 1.86 × 104
3000 1.83 2.79 × 104
4000 2.44 3.73 × 104
5000 3.05 4.66 × 104
6000 3.66 5.59 × 104
7000 4.27 6.52 × 104
8000 4.88 7.45 × 104
9000 5.49 8.38 × 104
1.00 × 104 6.10 9.31 × 104
2.00 × 104 12.2 1.86 × 105
3.00 × 104 18.3 2.79 × 105
3.19 × 104 19.5 2.97 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.155 1510
200 0.298 2910
300 0.447 4370
400 0.596 5820
500 0.745 7280
600 0.894 8730
700 1.04 1.02 × 104
800 1.19 1.16 × 104
900 1.34 1.31 × 104
1000 1.49 1.46 × 104
2000 2.98 2.91 × 104
3000 4.47 4.37 × 104
4000 5.96 5.82 × 104
5000 7.45 7.28 × 104
6000 8.94 8.73 × 104
7000 10.4 1.02 × 105
8000 11.9 1.16 × 105
9000 13.4 1.31 × 105
1.00 × 104 14.9 1.46 × 105
1.62 × 104 24.1 2.35 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.321 2180
200 0.618 4190
300 0.927 6290
400 1.24 8380
500 1.54 1.05 × 104
600 1.85 1.26 × 104
700 2.16 1.47 × 104
800 2.47 1.68 × 104
900 2.78 1.89 × 104
1000 3.09 2.10 × 104
2000 6.18 4.19 × 104
3000 9.27 6.29 × 104
4000 12.4 8.38 × 104
5000 15.4 1.05 × 105
6000 18.5 1.26 × 105
7000 21.6 1.47 × 105
7790 24.1 1.63 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 0.595 2970
200 1.14 5700
300 1.72 8560
400 2.29 1.14 × 104
500 2.86 1.43 × 104
600 3.43 1.71 × 104
700 4.01 2.00 × 104
800 4.58 2.28 × 104
900 5.15 2.57 × 104
1000 5.72 2.85 × 104
2000 11.4 5.70 × 104
3000 17.2 8.56 × 104
4000 22.9 1.14 × 105
4210 24.1 1.20 × 105
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 1.02 3870
200 1.95 7450
300 2.93 1.12 × 104
400 3.90 1.49 × 104
500 4.88 1.86 × 104
600 5.86 2.24 × 104
700 6.83 2.61 × 104
800 7.81 2.98 × 104
900 8.78 3.35 × 104
1000 9.76 3.73 × 104
2000 19.5 7.45 × 104
2460 24.1 9.18 × 104
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 1.63 4900
200 3.13 9430
300 4.69 1.41 × 104
400 6.25 1.89 × 104
500 7.82 2.36 × 104
600 9.38 2.83 × 104
700 10.9 3.30 × 104
800 12.5 3.77 × 104
900 14.1 4.24 × 104
1000 15.6 4.71 × 104
1540 24.1 7.26 × 104
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 2.48 6050
200 4.77 1.16 × 104
300 7.15 1.75 × 104
400 9.53 2.33 × 104
500 11.9 2.91 × 104
600 14.3 3.49 × 104
700 16.7 4.07 × 104
800 19.1 4.66 × 104
900 21.4 5.24 × 104
1000 23.8 5.82 × 104
1010 24.1 5.88 × 104
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 6.05 9460
200 11.6 1.82 × 104
300 17.5 2.73 × 104
400 23.3 3.64 × 104
414 24.1 3.76 × 104
Steel I Beam: W24 × 104 (Wide Flange 24 inch tall × 104 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
104 12.5 1.36 × 104
199 24.1 2.61 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.