Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W12 × 230
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 2420 in4) for the W12 × 230 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
  
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 5.69 × 10-6 9.66
300 7.42 × 10-6 12.6
400 9.89 × 10-6 16.8
500 1.24 × 10-5 21.0
600 1.48 × 10-5 25.2
700 1.73 × 10-5 29.4
800 1.98 × 10-5 33.6
900 2.23 × 10-5 37.8
1000 2.47 × 10-5 42.0
2000 4.95 × 10-5 84.0
3000 7.42 × 10-5 126
4000 9.89 × 10-5 168
5000 1.24 × 10-4 210
6000 1.48 × 10-4 252
7000 1.73 × 10-4 294
8000 1.98 × 10-4 336
9000 2.23 × 10-4 378
1.00 × 104 2.47 × 10-4 420
2.00 × 104 4.95 × 10-4 840
3.00 × 104 7.42 × 10-4 1260
4.00 × 104 9.89 × 10-4 1680
5.00 × 104 0.00124 2100
6.00 × 104 0.00148 2520
7.00 × 104 0.00173 2940
8.00 × 104 0.00198 3360
9.00 × 104 0.00223 3780
1.00 × 105 0.00247 4200
2.00 × 105 0.00495 8400
3.00 × 105 0.00742 1.26 × 104
4.00 × 105 0.00989 1.68 × 104
5.00 × 105 0.0124 2.10 × 104
6.00 × 105 0.0148 2.52 × 104
7.00 × 105 0.0173 2.94 × 104
8.00 × 105 0.0198 3.36 × 104
9.00 × 105 0.0223 3.78 × 104
1.00 × 106 0.0247 4.20 × 104
2.00 × 106 0.0495 8.40 × 104
3.00 × 106 0.0742 1.26 × 105
4.00 × 106 0.0989 1.68 × 105
5.00 × 106 0.124 2.10 × 105
6.00 × 106 0.148 2.52 × 105
7.00 × 106 0.173 2.94 × 105
7.08 × 106 0.175 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 4.39 × 10-5 26.8
300 5.72 × 10-5 35.0
400 7.63 × 10-5 46.6
500 9.54 × 10-5 58.3
600 1.14 × 10-4 70.0
700 1.34 × 10-4 81.6
800 1.53 × 10-4 93.3
900 1.72 × 10-4 105
1000 1.91 × 10-4 117
2000 3.82 × 10-4 233
3000 5.72 × 10-4 350
4000 7.63 × 10-4 466
5000 9.54 × 10-4 583
6000 0.00114 700
7000 0.00134 816
8000 0.00153 933
9000 0.00172 1050
1.00 × 104 0.00191 1170
2.00 × 104 0.00382 2330
3.00 × 104 0.00572 3500
4.00 × 104 0.00763 4660
5.00 × 104 0.00954 5830
6.00 × 104 0.0114 7000
7.00 × 104 0.0134 8160
8.00 × 104 0.0153 9330
9.00 × 104 0.0172 1.05 × 104
1.00 × 105 0.0191 1.17 × 104
2.00 × 105 0.0382 2.33 × 104
3.00 × 105 0.0572 3.50 × 104
4.00 × 105 0.0763 4.66 × 104
5.00 × 105 0.0954 5.83 × 104
6.00 × 105 0.114 7.00 × 104
7.00 × 105 0.134 8.16 × 104
8.00 × 105 0.153 9.33 × 104
9.00 × 105 0.172 1.05 × 105
1.00 × 106 0.191 1.17 × 105
2.00 × 106 0.382 2.33 × 105
2.55 × 106 0.486 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 7.02 × 10-4 107
300 9.16 × 10-4 140
400 0.00122 187
500 0.00153 233
600 0.00183 280
700 0.00214 326
800 0.00244 373
900 0.00275 420
1000 0.00305 466
2000 0.00611 933
3000 0.00916 1400
4000 0.0122 1870
5000 0.0153 2330
6000 0.0183 2800
7000 0.0214 3260
8000 0.0244 3730
9000 0.0275 4200
1.00 × 104 0.0305 4660
2.00 × 104 0.0611 9330
3.00 × 104 0.0916 1.40 × 104
4.00 × 104 0.122 1.87 × 104
5.00 × 104 0.153 2.33 × 104
6.00 × 104 0.183 2.80 × 104
7.00 × 104 0.214 3.26 × 104
8.00 × 104 0.244 3.73 × 104
9.00 × 104 0.275 4.20 × 104
1.00 × 105 0.305 4.66 × 104
2.00 × 105 0.611 9.33 × 104
3.00 × 105 0.916 1.40 × 105
4.00 × 105 1.22 1.87 × 105
5.00 × 105 1.53 2.33 × 105
6.00 × 105 1.83 2.80 × 105
6.37 × 105 1.94 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.00355 241
300 0.00464 315
400 0.00618 420
500 0.00773 525
600 0.00927 630
700 0.0108 735
800 0.0124 840
900 0.0139 945
1000 0.0155 1050
2000 0.0309 2100
3000 0.0464 3150
4000 0.0618 4200
5000 0.0773 5250
6000 0.0927 6300
7000 0.108 7350
8000 0.124 8400
9000 0.139 9450
1.00 × 104 0.155 1.05 × 104
2.00 × 104 0.309 2.10 × 104
3.00 × 104 0.464 3.15 × 104
4.00 × 104 0.618 4.20 × 104
5.00 × 104 0.773 5.25 × 104
6.00 × 104 0.927 6.30 × 104
7.00 × 104 1.08 7.35 × 104
8.00 × 104 1.24 8.40 × 104
9.00 × 104 1.39 9.45 × 104
1.00 × 105 1.55 1.05 × 105
2.00 × 105 3.09 2.10 × 105
2.83 × 105 4.37 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.0112 429
300 0.0147 560
400 0.0195 746
500 0.0244 933
600 0.0293 1120
700 0.0342 1310
800 0.0391 1490
900 0.0440 1680
1000 0.0488 1870
2000 0.0977 3730
3000 0.147 5600
4000 0.195 7460
5000 0.244 9330
6000 0.293 1.12 × 104
7000 0.342 1.31 × 104
8000 0.391 1.49 × 104
9000 0.440 1.68 × 104
1.00 × 104 0.488 1.87 × 104
2.00 × 104 0.977 3.73 × 104
3.00 × 104 1.47 5.60 × 104
4.00 × 104 1.95 7.46 × 104
5.00 × 104 2.44 9.33 × 104
6.00 × 104 2.93 1.12 × 105
7.00 × 104 3.42 1.31 × 105
8.00 × 104 3.91 1.49 × 105
9.00 × 104 4.40 1.68 × 105
1.00 × 105 4.88 1.87 × 105
1.59 × 105 7.78 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.0274 670
300 0.0358 875
400 0.0477 1170
500 0.0596 1460
600 0.0715 1750
700 0.0835 2040
800 0.0954 2330
900 0.107 2620
1000 0.119 2920
2000 0.238 5830
3000 0.358 8750
4000 0.477 1.17 × 104
5000 0.596 1.46 × 104
6000 0.715 1.75 × 104
7000 0.835 2.04 × 104
8000 0.954 2.33 × 104
9000 1.07 2.62 × 104
1.00 × 104 1.19 2.92 × 104
2.00 × 104 2.38 5.83 × 104
3.00 × 104 3.58 8.75 × 104
4.00 × 104 4.77 1.17 × 105
5.00 × 104 5.96 1.46 × 105
6.00 × 104 7.15 1.75 × 105
7.00 × 104 8.35 2.04 × 105
8.00 × 104 9.54 2.33 × 105
9.00 × 104 10.7 2.62 × 105
1.00 × 105 11.9 2.92 × 105
1.02 × 105 12.1 2.97 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.0569 966
300 0.0742 1260
400 0.0989 1680
500 0.124 2100
600 0.148 2520
700 0.173 2940
800 0.198 3360
900 0.223 3780
1000 0.247 4200
2000 0.495 8400
3000 0.742 1.26 × 104
4000 0.989 1.68 × 104
5000 1.24 2.10 × 104
6000 1.48 2.52 × 104
7000 1.73 2.94 × 104
8000 1.98 3.36 × 104
9000 2.23 3.78 × 104
1.00 × 104 2.47 4.20 × 104
2.00 × 104 4.95 8.40 × 104
3.00 × 104 7.42 1.26 × 105
4.00 × 104 9.89 1.68 × 105
5.00 × 104 12.4 2.10 × 105
6.00 × 104 14.8 2.52 × 105
6.09 × 104 15.1 2.56 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.180 1720
300 0.234 2240
400 0.313 2990
500 0.391 3730
600 0.469 4480
700 0.547 5220
800 0.625 5970
900 0.703 6720
1000 0.781 7460
2000 1.56 1.49 × 104
3000 2.34 2.24 × 104
4000 3.13 2.99 × 104
5000 3.91 3.73 × 104
6000 4.69 4.48 × 104
7000 5.47 5.22 × 104
8000 6.25 5.97 × 104
9000 7.03 6.72 × 104
1.00 × 104 7.81 7.46 × 104
1.93 × 104 15.1 1.44 × 105
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.439 2680
300 0.572 3500
400 0.763 4660
500 0.954 5830
600 1.14 7000
700 1.34 8160
800 1.53 9330
900 1.72 1.05 × 104
1000 1.91 1.17 × 104
2000 3.82 2.33 × 104
3000 5.72 3.50 × 104
4000 7.63 4.66 × 104
5000 9.54 5.83 × 104
6000 11.4 7.00 × 104
7000 13.4 8.16 × 104
7890 15.1 9.20 × 104
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 0.910 3860
300 1.19 5040
400 1.58 6720
500 1.98 8400
600 2.37 1.01 × 104
700 2.77 1.18 × 104
800 3.16 1.34 × 104
900 3.56 1.51 × 104
1000 3.96 1.68 × 104
2000 7.91 3.36 × 104
3000 11.9 5.04 × 104
3800 15.1 6.39 × 104
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 1.69 5260
300 2.20 6860
400 2.93 9140
500 3.66 1.14 × 104
600 4.40 1.37 × 104
700 5.13 1.60 × 104
800 5.86 1.83 × 104
900 6.60 2.06 × 104
1000 7.33 2.29 × 104
2000 14.7 4.57 × 104
2050 15.1 4.69 × 104
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 2.88 6870
300 3.75 8960
400 5.00 1.19 × 104
500 6.25 1.49 × 104
600 7.50 1.79 × 104
700 8.75 2.09 × 104
800 10.0 2.39 × 104
900 11.3 2.69 × 104
1000 12.5 2.99 × 104
1200 15.1 3.59 × 104
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 4.61 8690
300 6.01 1.13 × 104
400 8.01 1.51 × 104
500 10.0 1.89 × 104
600 12.0 2.27 × 104
700 14.0 2.64 × 104
751 15.1 2.84 × 104
Steel I Beam: W12 × 230 (Wide Flange 12 inch tall × 230 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
230 7.02 1.07 × 104
300 9.16 1.40 × 104
400 12.2 1.87 × 104
493 15.1 2.30 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.