Wide Flange Steel I Beam: W14 × 665
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W14 × 665
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 12400 in4) for the W14 × 665 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 3.21 × 10-6 7.83
700 3.38 × 10-6 8.25
800 3.86 × 10-6 9.42
900 4.34 × 10-6 10.6
1000 4.83 × 10-6 11.8
2000 9.65 × 10-6 23.6
3000 1.45 × 10-5 35.3
4000 1.93 × 10-5 47.1
5000 2.41 × 10-5 58.9
6000 2.90 × 10-5 70.7
7000 3.38 × 10-5 82.5
8000 3.86 × 10-5 94.2
9000 4.34 × 10-5 106
1.00 × 104 4.83 × 10-5 118
2.00 × 104 9.65 × 10-5 236
3.00 × 104 1.45 × 10-4 353
4.00 × 104 1.93 × 10-4 471
5.00 × 104 2.41 × 10-4 589
6.00 × 104 2.90 × 10-4 707
7.00 × 104 3.38 × 10-4 825
8.00 × 104 3.86 × 10-4 942
9.00 × 104 4.34 × 10-4 1060
1.00 × 105 4.83 × 10-4 1180
2.00 × 105 9.65 × 10-4 2360
3.00 × 105 0.00145 3530
4.00 × 105 0.00193 4710
5.00 × 105 0.00241 5890
6.00 × 105 0.00290 7070
7.00 × 105 0.00338 8250
8.00 × 105 0.00386 9420
9.00 × 105 0.00434 1.06 × 104
1.00 × 106 0.00483 1.18 × 104
2.00 × 106 0.00965 2.36 × 104
3.00 × 106 0.0145 3.53 × 104
4.00 × 106 0.0193 4.71 × 104
5.00 × 106 0.0241 5.89 × 104
6.00 × 106 0.0290 7.07 × 104
7.00 × 106 0.0338 8.25 × 104
8.00 × 106 0.0386 9.42 × 104
9.00 × 106 0.0434 1.06 × 105
1.00 × 107 0.0483 1.18 × 105
2.00 × 107 0.0965 2.36 × 105
2.52 × 107 0.122 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 2.48 × 10-5 21.8
700 2.61 × 10-5 22.9
800 2.98 × 10-5 26.2
900 3.35 × 10-5 29.4
1000 3.72 × 10-5 32.7
2000 7.45 × 10-5 65.4
3000 1.12 × 10-4 98.2
4000 1.49 × 10-4 131
5000 1.86 × 10-4 164
6000 2.23 × 10-4 196
7000 2.61 × 10-4 229
8000 2.98 × 10-4 262
9000 3.35 × 10-4 294
1.00 × 104 3.72 × 10-4 327
2.00 × 104 7.45 × 10-4 654
3.00 × 104 0.00112 982
4.00 × 104 0.00149 1310
5.00 × 104 0.00186 1640
6.00 × 104 0.00223 1960
7.00 × 104 0.00261 2290
8.00 × 104 0.00298 2620
9.00 × 104 0.00335 2940
1.00 × 105 0.00372 3270
2.00 × 105 0.00745 6540
3.00 × 105 0.0112 9820
4.00 × 105 0.0149 1.31 × 104
5.00 × 105 0.0186 1.64 × 104
6.00 × 105 0.0223 1.96 × 104
7.00 × 105 0.0261 2.29 × 104
8.00 × 105 0.0298 2.62 × 104
9.00 × 105 0.0335 2.94 × 104
1.00 × 106 0.0372 3.27 × 104
2.00 × 106 0.0745 6.54 × 104
3.00 × 106 0.112 9.82 × 104
4.00 × 106 0.149 1.31 × 105
5.00 × 106 0.186 1.64 × 105
6.00 × 106 0.223 1.96 × 105
7.00 × 106 0.261 2.29 × 105
8.00 × 106 0.298 2.62 × 105
9.00 × 106 0.335 2.94 × 105
9.08 × 106 0.338 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 3.96 × 10-4 87.0
700 4.17 × 10-4 91.6
800 4.77 × 10-4 105
900 5.36 × 10-4 118
1000 5.96 × 10-4 131
2000 0.00119 262
3000 0.00179 393
4000 0.00238 524
5000 0.00298 654
6000 0.00357 785
7000 0.00417 916
8000 0.00477 1050
9000 0.00536 1180
1.00 × 104 0.00596 1310
2.00 × 104 0.0119 2620
3.00 × 104 0.0179 3930
4.00 × 104 0.0238 5240
5.00 × 104 0.0298 6540
6.00 × 104 0.0357 7850
7.00 × 104 0.0417 9160
8.00 × 104 0.0477 1.05 × 104
9.00 × 104 0.0536 1.18 × 104
1.00 × 105 0.0596 1.31 × 104
2.00 × 105 0.119 2.62 × 104
3.00 × 105 0.179 3.93 × 104
4.00 × 105 0.238 5.24 × 104
5.00 × 105 0.298 6.54 × 104
6.00 × 105 0.357 7.85 × 104
7.00 × 105 0.417 9.16 × 104
8.00 × 105 0.477 1.05 × 105
9.00 × 105 0.536 1.18 × 105
1.00 × 106 0.596 1.31 × 105
2.00 × 106 1.19 2.62 × 105
2.27 × 106 1.35 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.00201 196
700 0.00211 206
800 0.00241 236
900 0.00271 265
1000 0.00302 294
2000 0.00603 589
3000 0.00905 883
4000 0.0121 1180
5000 0.0151 1470
6000 0.0181 1770
7000 0.0211 2060
8000 0.0241 2360
9000 0.0271 2650
1.00 × 104 0.0302 2940
2.00 × 104 0.0603 5890
3.00 × 104 0.0905 8830
4.00 × 104 0.121 1.18 × 104
5.00 × 104 0.151 1.47 × 104
6.00 × 104 0.181 1.77 × 104
7.00 × 104 0.211 2.06 × 104
8.00 × 104 0.241 2.36 × 104
9.00 × 104 0.271 2.65 × 104
1.00 × 105 0.302 2.94 × 104
2.00 × 105 0.603 5.89 × 104
3.00 × 105 0.905 8.83 × 104
4.00 × 105 1.21 1.18 × 105
5.00 × 105 1.51 1.47 × 105
6.00 × 105 1.81 1.77 × 105
7.00 × 105 2.11 2.06 × 105
8.00 × 105 2.41 2.36 × 105
9.00 × 105 2.71 2.65 × 105
1.00 × 106 3.02 2.94 × 105
1.01 × 106 3.04 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.00634 348
700 0.00667 366
800 0.00763 419
900 0.00858 471
1000 0.00953 524
2000 0.0191 1050
3000 0.0286 1570
4000 0.0381 2090
5000 0.0477 2620
6000 0.0572 3140
7000 0.0667 3660
8000 0.0763 4190
9000 0.0858 4710
1.00 × 104 0.0953 5240
2.00 × 104 0.191 1.05 × 104
3.00 × 104 0.286 1.57 × 104
4.00 × 104 0.381 2.09 × 104
5.00 × 104 0.477 2.62 × 104
6.00 × 104 0.572 3.14 × 104
7.00 × 104 0.667 3.66 × 104
8.00 × 104 0.763 4.19 × 104
9.00 × 104 0.858 4.71 × 104
1.00 × 105 0.953 5.24 × 104
2.00 × 105 1.91 1.05 × 105
3.00 × 105 2.86 1.57 × 105
4.00 × 105 3.81 2.09 × 105
5.00 × 105 4.77 2.62 × 105
5.67 × 105 5.41 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.0155 544
700 0.0163 573
800 0.0186 654
900 0.0209 736
1000 0.0233 818
2000 0.0465 1640
3000 0.0698 2450
4000 0.0931 3270
5000 0.116 4090
6000 0.140 4910
7000 0.163 5730
8000 0.186 6540
9000 0.209 7360
1.00 × 104 0.233 8180
2.00 × 104 0.465 1.64 × 104
3.00 × 104 0.698 2.45 × 104
4.00 × 104 0.931 3.27 × 104
5.00 × 104 1.16 4.09 × 104
6.00 × 104 1.40 4.91 × 104
7.00 × 104 1.63 5.73 × 104
8.00 × 104 1.86 6.54 × 104
9.00 × 104 2.09 7.36 × 104
1.00 × 105 2.33 8.18 × 104
2.00 × 105 4.65 1.64 × 105
3.00 × 105 6.98 2.45 × 105
3.63 × 105 8.45 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.0321 783
700 0.0338 825
800 0.0386 942
900 0.0434 1060
1000 0.0483 1180
2000 0.0965 2360
3000 0.145 3530
4000 0.193 4710
5000 0.241 5890
6000 0.290 7070
7000 0.338 8250
8000 0.386 9420
9000 0.434 1.06 × 104
1.00 × 104 0.483 1.18 × 104
2.00 × 104 0.965 2.36 × 104
3.00 × 104 1.45 3.53 × 104
4.00 × 104 1.93 4.71 × 104
5.00 × 104 2.41 5.89 × 104
6.00 × 104 2.90 7.07 × 104
7.00 × 104 3.38 8.25 × 104
8.00 × 104 3.86 9.42 × 104
9.00 × 104 4.34 1.06 × 105
1.00 × 105 4.83 1.18 × 105
2.00 × 105 9.65 2.36 × 105
2.52 × 105 12.2 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.101 1390
700 0.107 1470
800 0.122 1680
900 0.137 1880
1000 0.153 2090
2000 0.305 4190
3000 0.458 6280
4000 0.610 8380
5000 0.763 1.05 × 104
6000 0.915 1.26 × 104
7000 1.07 1.47 × 104
8000 1.22 1.68 × 104
9000 1.37 1.88 × 104
1.00 × 104 1.53 2.09 × 104
2.00 × 104 3.05 4.19 × 104
3.00 × 104 4.58 6.28 × 104
4.00 × 104 6.10 8.38 × 104
5.00 × 104 7.63 1.05 × 105
6.00 × 104 9.15 1.26 × 105
7.00 × 104 10.7 1.47 × 105
8.00 × 104 12.2 1.68 × 105
9.00 × 104 13.7 1.88 × 105
1.00 × 105 15.3 2.09 × 105
1.42 × 105 21.6 2.97 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.248 2180
700 0.261 2290
800 0.298 2620
900 0.335 2940
1000 0.372 3270
2000 0.745 6540
3000 1.12 9820
4000 1.49 1.31 × 104
5000 1.86 1.64 × 104
6000 2.23 1.96 × 104
7000 2.61 2.29 × 104
8000 2.98 2.62 × 104
9000 3.35 2.94 × 104
1.00 × 104 3.72 3.27 × 104
2.00 × 104 7.45 6.54 × 104
3.00 × 104 11.2 9.82 × 104
4.00 × 104 14.9 1.31 × 105
5.00 × 104 18.6 1.64 × 105
5.81 × 104 21.6 1.90 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.513 3130
700 0.540 3300
800 0.618 3770
900 0.695 4240
1000 0.772 4710
2000 1.54 9420
3000 2.32 1.41 × 104
4000 3.09 1.88 × 104
5000 3.86 2.36 × 104
6000 4.63 2.83 × 104
7000 5.40 3.30 × 104
8000 6.18 3.77 × 104
9000 6.95 4.24 × 104
1.00 × 104 7.72 4.71 × 104
2.00 × 104 15.4 9.42 × 104
2.80 × 104 21.6 1.32 × 105
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 0.951 4260
700 1.00 4490
800 1.14 5130
900 1.29 5770
1000 1.43 6410
2000 2.86 1.28 × 104
3000 4.29 1.92 × 104
4000 5.72 2.57 × 104
5000 7.15 3.21 × 104
6000 8.58 3.85 × 104
7000 10.0 4.49 × 104
8000 11.4 5.13 × 104
9000 12.9 5.77 × 104
1.00 × 104 14.3 6.41 × 104
1.51 × 104 21.6 9.70 × 104
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 1.62 5570
700 1.71 5860
800 1.95 6700
900 2.20 7540
1000 2.44 8380
2000 4.88 1.68 × 104
3000 7.32 2.51 × 104
4000 9.76 3.35 × 104
5000 12.2 4.19 × 104
6000 14.6 5.03 × 104
7000 17.1 5.86 × 104
8000 19.5 6.70 × 104
8870 21.6 7.43 × 104
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 2.60 7050
700 2.74 7420
800 3.13 8480
900 3.52 9540
1000 3.91 1.06 × 104
2000 7.82 2.12 × 104
3000 11.7 3.18 × 104
4000 15.6 4.24 × 104
5000 19.5 5.30 × 104
5540 21.6 5.87 × 104
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 3.96 8700
700 4.17 9160
800 4.77 1.05 × 104
900 5.36 1.18 × 104
1000 5.96 1.31 × 104
2000 11.9 2.62 × 104
3000 17.9 3.93 × 104
3630 21.6 4.75 × 104
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 9.67 1.36 × 104
700 10.2 1.43 × 104
800 11.6 1.64 × 104
900 13.1 1.84 × 104
1000 14.5 2.05 × 104
1490 21.6 3.04 × 104
Steel I Beam: W14 × 665 (Wide Flange 14 inch tall × 665 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
665 20.1 1.96 × 104
700 21.1 2.06 × 104
718 21.6 2.11 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2010 eFunda, Inc.