engineering fundamentals
Wide Flange Steel I Beam: W18 × 65
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W18 × 65
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1070 in4) for the W18 × 65 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 3.63 × 10-6 7.52
70.0 3.91 × 10-6 8.10
80.0 4.47 × 10-6 9.26
90.0 5.03 × 10-6 10.4
100 5.59 × 10-6 11.6
200 1.12 × 10-5 23.2
300 1.68 × 10-5 34.7
400 2.24 × 10-5 46.3
500 2.80 × 10-5 57.9
600 3.36 × 10-5 69.5
700 3.91 × 10-5 81.0
800 4.47 × 10-5 92.6
900 5.03 × 10-5 104
1000 5.59 × 10-5 116
2000 1.12 × 10-4 232
3000 1.68 × 10-4 347
4000 2.24 × 10-4 463
5000 2.80 × 10-4 579
6000 3.36 × 10-4 695
7000 3.91 × 10-4 810
8000 4.47 × 10-4 926
9000 5.03 × 10-4 1040
1.00 × 104 5.59 × 10-4 1160
2.00 × 104 0.00112 2320
3.00 × 104 0.00168 3470
4.00 × 104 0.00224 4630
5.00 × 104 0.00280 5790
6.00 × 104 0.00336 6950
7.00 × 104 0.00391 8100
8.00 × 104 0.00447 9260
9.00 × 104 0.00503 1.04 × 104
1.00 × 105 0.00559 1.16 × 104
2.00 × 105 0.0112 2.32 × 104
3.00 × 105 0.0168 3.47 × 104
4.00 × 105 0.0224 4.63 × 104
5.00 × 105 0.0280 5.79 × 104
6.00 × 105 0.0336 6.95 × 104
7.00 × 105 0.0391 8.10 × 104
8.00 × 105 0.0447 9.26 × 104
9.00 × 105 0.0503 1.04 × 105
1.00 × 106 0.0559 1.16 × 105
2.00 × 106 0.112 2.32 × 105
2.57 × 106 0.143 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 2.80 × 10-5 20.9
70.0 3.02 × 10-5 22.5
80.0 3.45 × 10-5 25.7
90.0 3.88 × 10-5 28.9
100 4.31 × 10-5 32.2
200 8.63 × 10-5 64.3
300 1.29 × 10-4 96.5
400 1.73 × 10-4 129
500 2.16 × 10-4 161
600 2.59 × 10-4 193
700 3.02 × 10-4 225
800 3.45 × 10-4 257
900 3.88 × 10-4 289
1000 4.31 × 10-4 322
2000 8.63 × 10-4 643
3000 0.00129 965
4000 0.00173 1290
5000 0.00216 1610
6000 0.00259 1930
7000 0.00302 2250
8000 0.00345 2570
9000 0.00388 2890
1.00 × 104 0.00431 3220
2.00 × 104 0.00863 6430
3.00 × 104 0.0129 9650
4.00 × 104 0.0173 1.29 × 104
5.00 × 104 0.0216 1.61 × 104
6.00 × 104 0.0259 1.93 × 104
7.00 × 104 0.0302 2.25 × 104
8.00 × 104 0.0345 2.57 × 104
9.00 × 104 0.0388 2.89 × 104
1.00 × 105 0.0431 3.22 × 104
2.00 × 105 0.0863 6.43 × 104
3.00 × 105 0.129 9.65 × 104
4.00 × 105 0.173 1.29 × 105
5.00 × 105 0.216 1.61 × 105
6.00 × 105 0.259 1.93 × 105
7.00 × 105 0.302 2.25 × 105
8.00 × 105 0.345 2.57 × 105
9.00 × 105 0.388 2.89 × 105
9.24 × 105 0.399 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 4.49 × 10-4 83.6
70.0 4.83 × 10-4 90.0
80.0 5.52 × 10-4 103
90.0 6.21 × 10-4 116
100 6.90 × 10-4 129
200 0.00138 257
300 0.00207 386
400 0.00276 514
500 0.00345 643
600 0.00414 772
700 0.00483 900
800 0.00552 1030
900 0.00621 1160
1000 0.00690 1290
2000 0.0138 2570
3000 0.0207 3860
4000 0.0276 5140
5000 0.0345 6430
6000 0.0414 7720
7000 0.0483 9000
8000 0.0552 1.03 × 104
9000 0.0621 1.16 × 104
1.00 × 104 0.0690 1.29 × 104
2.00 × 104 0.138 2.57 × 104
3.00 × 104 0.207 3.86 × 104
4.00 × 104 0.276 5.14 × 104
5.00 × 104 0.345 6.43 × 104
6.00 × 104 0.414 7.72 × 104
7.00 × 104 0.483 9.00 × 104
8.00 × 104 0.552 1.03 × 105
9.00 × 104 0.621 1.16 × 105
1.00 × 105 0.690 1.29 × 105
2.00 × 105 1.38 2.57 × 105
2.31 × 105 1.59 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.00227 188
70.0 0.00245 203
80.0 0.00280 232
90.0 0.00315 260
100 0.00350 289
200 0.00699 579
300 0.0105 868
400 0.0140 1160
500 0.0175 1450
600 0.0210 1740
700 0.0245 2030
800 0.0280 2320
900 0.0315 2600
1000 0.0350 2890
2000 0.0699 5790
3000 0.105 8680
4000 0.140 1.16 × 104
5000 0.175 1.45 × 104
6000 0.210 1.74 × 104
7000 0.245 2.03 × 104
8000 0.280 2.32 × 104
9000 0.315 2.60 × 104
1.00 × 104 0.350 2.89 × 104
2.00 × 104 0.699 5.79 × 104
3.00 × 104 1.05 8.68 × 104
4.00 × 104 1.40 1.16 × 105
5.00 × 104 1.75 1.45 × 105
6.00 × 104 2.10 1.74 × 105
7.00 × 104 2.45 2.03 × 105
8.00 × 104 2.80 2.32 × 105
9.00 × 104 3.15 2.60 × 105
1.00 × 105 3.50 2.89 × 105
1.03 × 105 3.59 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.00718 334
70.0 0.00773 360
80.0 0.00884 412
90.0 0.00994 463
100 0.0110 514
200 0.0221 1030
300 0.0331 1540
400 0.0442 2060
500 0.0552 2570
600 0.0663 3090
700 0.0773 3600
800 0.0884 4120
900 0.0994 4630
1000 0.110 5140
2000 0.221 1.03 × 104
3000 0.331 1.54 × 104
4000 0.442 2.06 × 104
5000 0.552 2.57 × 104
6000 0.663 3.09 × 104
7000 0.773 3.60 × 104
8000 0.884 4.12 × 104
9000 0.994 4.63 × 104
1.00 × 104 1.10 5.14 × 104
2.00 × 104 2.21 1.03 × 105
3.00 × 104 3.31 1.54 × 105
4.00 × 104 4.42 2.06 × 105
5.00 × 104 5.52 2.57 × 105
5.77 × 104 6.38 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.0175 523
70.0 0.0189 563
80.0 0.0216 643
90.0 0.0243 723
100 0.0270 804
200 0.0539 1610
300 0.0809 2410
400 0.108 3220
500 0.135 4020
600 0.162 4820
700 0.189 5630
800 0.216 6430
900 0.243 7230
1000 0.270 8040
2000 0.539 1.61 × 104
3000 0.809 2.41 × 104
4000 1.08 3.22 × 104
5000 1.35 4.02 × 104
6000 1.62 4.82 × 104
7000 1.89 5.63 × 104
8000 2.16 6.43 × 104
9000 2.43 7.23 × 104
1.00 × 104 2.70 8.04 × 104
2.00 × 104 5.39 1.61 × 105
3.00 × 104 8.09 2.41 × 105
3.70 × 104 9.96 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.0363 752
70.0 0.0391 810
80.0 0.0447 926
90.0 0.0503 1040
100 0.0559 1160
200 0.112 2320
300 0.168 3470
400 0.224 4630
500 0.280 5790
600 0.336 6950
700 0.391 8100
800 0.447 9260
900 0.503 1.04 × 104
1000 0.559 1.16 × 104
2000 1.12 2.32 × 104
3000 1.68 3.47 × 104
4000 2.24 4.63 × 104
5000 2.80 5.79 × 104
6000 3.36 6.95 × 104
7000 3.91 8.10 × 104
8000 4.47 9.26 × 104
9000 5.03 1.04 × 105
1.00 × 104 5.59 1.16 × 105
2.00 × 104 11.2 2.32 × 105
2.57 × 104 14.3 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.115 1340
70.0 0.124 1440
80.0 0.141 1650
90.0 0.159 1850
100 0.177 2060
200 0.353 4120
300 0.530 6170
400 0.707 8230
500 0.884 1.03 × 104
600 1.06 1.23 × 104
700 1.24 1.44 × 104
800 1.41 1.65 × 104
900 1.59 1.85 × 104
1000 1.77 2.06 × 104
2000 3.53 4.12 × 104
3000 5.30 6.17 × 104
4000 7.07 8.23 × 104
5000 8.84 1.03 × 105
6000 10.6 1.23 × 105
7000 12.4 1.44 × 105
8000 14.1 1.65 × 105
9000 15.9 1.85 × 105
1.00 × 104 17.7 2.06 × 105
1.44 × 104 25.5 2.97 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.280 2090
70.0 0.302 2250
80.0 0.345 2570
90.0 0.388 2890
100 0.431 3220
200 0.863 6430
300 1.29 9650
400 1.73 1.29 × 104
500 2.16 1.61 × 104
600 2.59 1.93 × 104
700 3.02 2.25 × 104
800 3.45 2.57 × 104
900 3.88 2.89 × 104
1000 4.31 3.22 × 104
2000 8.63 6.43 × 104
3000 12.9 9.65 × 104
4000 17.3 1.29 × 105
4250 18.4 1.37 × 105
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 0.582 3010
70.0 0.626 3240
80.0 0.716 3700
90.0 0.805 4170
100 0.895 4630
200 1.79 9260
300 2.68 1.39 × 104
400 3.58 1.85 × 104
500 4.47 2.32 × 104
600 5.37 2.78 × 104
700 6.26 3.24 × 104
800 7.16 3.70 × 104
900 8.05 4.17 × 104
1000 8.95 4.63 × 104
2000 17.9 9.26 × 104
2050 18.4 9.50 × 104
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 1.08 4100
70.0 1.16 4410
80.0 1.33 5040
90.0 1.49 5670
100 1.66 6300
200 3.32 1.26 × 104
300 4.97 1.89 × 104
400 6.63 2.52 × 104
500 8.29 3.15 × 104
600 9.95 3.78 × 104
700 11.6 4.41 × 104
800 13.3 5.04 × 104
900 14.9 5.67 × 104
1000 16.6 6.30 × 104
1110 18.4 6.98 × 104
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 1.84 5350
70.0 1.98 5760
80.0 2.26 6590
90.0 2.55 7410
100 2.83 8230
200 5.66 1.65 × 104
300 8.48 2.47 × 104
400 11.3 3.29 × 104
500 14.1 4.12 × 104
600 17.0 4.94 × 104
649 18.4 5.34 × 104
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 2.94 6770
70.0 3.17 7290
80.0 3.62 8330
90.0 4.08 9380
100 4.53 1.04 × 104
200 9.06 2.08 × 104
300 13.6 3.13 × 104
400 18.1 4.17 × 104
405 18.4 4.22 × 104
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 4.49 8360
70.0 4.83 9000
80.0 5.52 1.03 × 104
90.0 6.21 1.16 × 104
100 6.90 1.29 × 104
200 13.8 2.57 × 104
266 18.4 3.42 × 104
Steel I Beam: W18 × 65 (Wide Flange 18 inch tall × 65 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
65.0 11.0 1.31 × 104
70.0 11.8 1.41 × 104
80.0 13.5 1.61 × 104
90.0 15.2 1.81 × 104
100 16.9 2.01 × 104
109 18.4 2.19 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2009 eFunda, Inc.