engineering fundamentals
Wide Flange Steel I Beam: W27 × 161
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Single Span » Wide Flange Steel I Beam » W27 × 161
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in a single span, the maximum displacement w_max and the maximum normal stress stress_max occur at the center of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 6280 in4) for the W27 × 161 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 1.53 × 10-6 4.77
200 1.91 × 10-6 5.93
300 2.86 × 10-6 8.90
400 3.81 × 10-6 11.9
500 4.76 × 10-6 14.8
600 5.72 × 10-6 17.8
700 6.67 × 10-6 20.8
800 7.62 × 10-6 23.7
900 8.58 × 10-6 26.7
1000 9.53 × 10-6 29.7
2000 1.91 × 10-5 59.3
3000 2.86 × 10-5 89.0
4000 3.81 × 10-5 119
5000 4.76 × 10-5 148
6000 5.72 × 10-5 178
7000 6.67 × 10-5 208
8000 7.62 × 10-5 237
9000 8.58 × 10-5 267
1.00 × 104 9.53 × 10-5 297
2.00 × 104 1.91 × 10-4 593
3.00 × 104 2.86 × 10-4 890
4.00 × 104 3.81 × 10-4 1190
5.00 × 104 4.76 × 10-4 1480
6.00 × 104 5.72 × 10-4 1780
7.00 × 104 6.67 × 10-4 2080
8.00 × 104 7.62 × 10-4 2370
9.00 × 104 8.58 × 10-4 2670
1.00 × 105 9.53 × 10-4 2970
2.00 × 105 0.00191 5930
3.00 × 105 0.00286 8900
4.00 × 105 0.00381 1.19 × 104
5.00 × 105 0.00476 1.48 × 104
6.00 × 105 0.00572 1.78 × 104
7.00 × 105 0.00667 2.08 × 104
8.00 × 105 0.00762 2.37 × 104
9.00 × 105 0.00858 2.67 × 104
1.00 × 106 0.00953 2.97 × 104
2.00 × 106 0.0191 5.93 × 104
3.00 × 106 0.0286 8.90 × 104
4.00 × 106 0.0381 1.19 × 105
5.00 × 106 0.0476 1.48 × 105
6.00 × 106 0.0572 1.78 × 105
7.00 × 106 0.0667 2.08 × 105
8.00 × 106 0.0762 2.37 × 105
9.00 × 106 0.0858 2.67 × 105
1.00 × 107 0.0953 2.97 × 105
1.00 × 107 0.0954 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 1.18 × 10-5 13.3
200 1.47 × 10-5 16.5
300 2.21 × 10-5 24.7
400 2.94 × 10-5 32.9
500 3.68 × 10-5 41.2
600 4.41 × 10-5 49.4
700 5.15 × 10-5 57.7
800 5.88 × 10-5 65.9
900 6.62 × 10-5 74.1
1000 7.35 × 10-5 82.4
2000 1.47 × 10-4 165
3000 2.21 × 10-4 247
4000 2.94 × 10-4 329
5000 3.68 × 10-4 412
6000 4.41 × 10-4 494
7000 5.15 × 10-4 577
8000 5.88 × 10-4 659
9000 6.62 × 10-4 741
1.00 × 104 7.35 × 10-4 824
2.00 × 104 0.00147 1650
3.00 × 104 0.00221 2470
4.00 × 104 0.00294 3290
5.00 × 104 0.00368 4120
6.00 × 104 0.00441 4940
7.00 × 104 0.00515 5770
8.00 × 104 0.00588 6590
9.00 × 104 0.00662 7410
1.00 × 105 0.00735 8240
2.00 × 105 0.0147 1.65 × 104
3.00 × 105 0.0221 2.47 × 104
4.00 × 105 0.0294 3.29 × 104
5.00 × 105 0.0368 4.12 × 104
6.00 × 105 0.0441 4.94 × 104
7.00 × 105 0.0515 5.77 × 104
8.00 × 105 0.0588 6.59 × 104
9.00 × 105 0.0662 7.41 × 104
1.00 × 106 0.0735 8.24 × 104
2.00 × 106 0.147 1.65 × 105
3.00 × 106 0.221 2.47 × 105
3.61 × 106 0.265 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 1.89 × 10-4 53.0
200 2.35 × 10-4 65.9
300 3.53 × 10-4 98.8
400 4.71 × 10-4 132
500 5.88 × 10-4 165
600 7.06 × 10-4 198
700 8.23 × 10-4 231
800 9.41 × 10-4 264
900 0.00106 297
1000 0.00118 329
2000 0.00235 659
3000 0.00353 988
4000 0.00471 1320
5000 0.00588 1650
6000 0.00706 1980
7000 0.00823 2310
8000 0.00941 2640
9000 0.0106 2970
1.00 × 104 0.0118 3290
2.00 × 104 0.0235 6590
3.00 × 104 0.0353 9880
4.00 × 104 0.0471 1.32 × 104
5.00 × 104 0.0588 1.65 × 104
6.00 × 104 0.0706 1.98 × 104
7.00 × 104 0.0823 2.31 × 104
8.00 × 104 0.0941 2.64 × 104
9.00 × 104 0.106 2.97 × 104
1.00 × 105 0.118 3.29 × 104
2.00 × 105 0.235 6.59 × 104
3.00 × 105 0.353 9.88 × 104
4.00 × 105 0.471 1.32 × 105
5.00 × 105 0.588 1.65 × 105
6.00 × 105 0.706 1.98 × 105
7.00 × 105 0.823 2.31 × 105
8.00 × 105 0.941 2.64 × 105
9.00 × 105 1.06 2.97 × 105
9.01 × 105 1.06 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 9.59 × 10-4 119
200 0.00119 148
300 0.00179 222
400 0.00238 297
500 0.00298 371
600 0.00357 445
700 0.00417 519
800 0.00476 593
900 0.00536 667
1000 0.00596 741
2000 0.0119 1480
3000 0.0179 2220
4000 0.0238 2970
5000 0.0298 3710
6000 0.0357 4450
7000 0.0417 5190
8000 0.0476 5930
9000 0.0536 6670
1.00 × 104 0.0596 7410
2.00 × 104 0.119 1.48 × 104
3.00 × 104 0.179 2.22 × 104
4.00 × 104 0.238 2.97 × 104
5.00 × 104 0.298 3.71 × 104
6.00 × 104 0.357 4.45 × 104
7.00 × 104 0.417 5.19 × 104
8.00 × 104 0.476 5.93 × 104
9.00 × 104 0.536 6.67 × 104
1.00 × 105 0.596 7.41 × 104
2.00 × 105 1.19 1.48 × 105
3.00 × 105 1.79 2.22 × 105
4.00 × 105 2.38 2.97 × 105
4.01 × 105 2.39 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.00303 212
200 0.00376 264
300 0.00565 395
400 0.00753 527
500 0.00941 659
600 0.0113 791
700 0.0132 923
800 0.0151 1050
900 0.0169 1190
1000 0.0188 1320
2000 0.0376 2640
3000 0.0565 3950
4000 0.0753 5270
5000 0.0941 6590
6000 0.113 7910
7000 0.132 9230
8000 0.151 1.05 × 104
9000 0.169 1.19 × 104
1.00 × 104 0.188 1.32 × 104
2.00 × 104 0.376 2.64 × 104
3.00 × 104 0.565 3.95 × 104
4.00 × 104 0.753 5.27 × 104
5.00 × 104 0.941 6.59 × 104
6.00 × 104 1.13 7.91 × 104
7.00 × 104 1.32 9.23 × 104
8.00 × 104 1.51 1.05 × 105
9.00 × 104 1.69 1.19 × 105
1.00 × 105 1.88 1.32 × 105
2.00 × 105 3.76 2.64 × 105
2.25 × 105 4.24 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.00740 332
200 0.00919 412
300 0.0138 618
400 0.0184 824
500 0.0230 1030
600 0.0276 1240
700 0.0322 1440
800 0.0368 1650
900 0.0414 1850
1000 0.0459 2060
2000 0.0919 4120
3000 0.138 6180
4000 0.184 8240
5000 0.230 1.03 × 104
6000 0.276 1.24 × 104
7000 0.322 1.44 × 104
8000 0.368 1.65 × 104
9000 0.414 1.85 × 104
1.00 × 104 0.459 2.06 × 104
2.00 × 104 0.919 4.12 × 104
3.00 × 104 1.38 6.18 × 104
4.00 × 104 1.84 8.24 × 104
5.00 × 104 2.30 1.03 × 105
6.00 × 104 2.76 1.24 × 105
7.00 × 104 3.22 1.44 × 105
8.00 × 104 3.68 1.65 × 105
9.00 × 104 4.14 1.85 × 105
1.00 × 105 4.59 2.06 × 105
1.44 × 105 6.63 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.0153 477
200 0.0191 593
300 0.0286 890
400 0.0381 1190
500 0.0476 1480
600 0.0572 1780
700 0.0667 2080
800 0.0762 2370
900 0.0858 2670
1000 0.0953 2970
2000 0.191 5930
3000 0.286 8900
4000 0.381 1.19 × 104
5000 0.476 1.48 × 104
6000 0.572 1.78 × 104
7000 0.667 2.08 × 104
8000 0.762 2.37 × 104
9000 0.858 2.67 × 104
1.00 × 104 0.953 2.97 × 104
2.00 × 104 1.91 5.93 × 104
3.00 × 104 2.86 8.90 × 104
4.00 × 104 3.81 1.19 × 105
5.00 × 104 4.76 1.48 × 105
6.00 × 104 5.72 1.78 × 105
7.00 × 104 6.67 2.08 × 105
8.00 × 104 7.62 2.37 × 105
9.00 × 104 8.58 2.67 × 105
1.00 × 105 9.53 2.97 × 105
1.00 × 105 9.54 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.0485 849
200 0.0602 1050
300 0.0903 1580
400 0.120 2110
500 0.151 2640
600 0.181 3160
700 0.211 3690
800 0.241 4220
900 0.271 4740
1000 0.301 5270
2000 0.602 1.05 × 104
3000 0.903 1.58 × 104
4000 1.20 2.11 × 104
5000 1.51 2.64 × 104
6000 1.81 3.16 × 104
7000 2.11 3.69 × 104
8000 2.41 4.22 × 104
9000 2.71 4.74 × 104
1.00 × 104 3.01 5.27 × 104
2.00 × 104 6.02 1.05 × 105
3.00 × 104 9.03 1.58 × 105
4.00 × 104 12.0 2.11 × 105
5.00 × 104 15.1 2.64 × 105
5.63 × 104 17.0 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.118 1330
200 0.147 1650
300 0.221 2470
400 0.294 3290
500 0.368 4120
600 0.441 4940
700 0.515 5770
800 0.588 6590
900 0.662 7410
1000 0.735 8240
2000 1.47 1.65 × 104
3000 2.21 2.47 × 104
4000 2.94 3.29 × 104
5000 3.68 4.12 × 104
6000 4.41 4.94 × 104
7000 5.15 5.77 × 104
8000 5.88 6.59 × 104
9000 6.62 7.41 × 104
1.00 × 104 7.35 8.24 × 104
2.00 × 104 14.7 1.65 × 105
3.00 × 104 22.1 2.47 × 105
3.61 × 104 26.5 2.97 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.245 1910
200 0.305 2370
300 0.457 3560
400 0.610 4740
500 0.762 5930
600 0.915 7120
700 1.07 8300
800 1.22 9490
900 1.37 1.07 × 104
1000 1.52 1.19 × 104
2000 3.05 2.37 × 104
3000 4.57 3.56 × 104
4000 6.10 4.74 × 104
5000 7.62 5.93 × 104
6000 9.15 7.12 × 104
7000 10.7 8.30 × 104
8000 12.2 9.49 × 104
9000 13.7 1.07 × 105
1.00 × 104 15.2 1.19 × 105
1.81 × 104 27.6 2.15 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.455 2600
200 0.565 3230
300 0.847 4840
400 1.13 6460
500 1.41 8070
600 1.69 9690
700 1.98 1.13 × 104
800 2.26 1.29 × 104
900 2.54 1.45 × 104
1000 2.82 1.61 × 104
2000 5.65 3.23 × 104
3000 8.47 4.84 × 104
4000 11.3 6.46 × 104
5000 14.1 8.07 × 104
6000 16.9 9.69 × 104
7000 19.8 1.13 × 105
8000 22.6 1.29 × 105
9000 25.4 1.45 × 105
9770 27.6 1.58 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 0.776 3400
200 0.964 4220
300 1.45 6330
400 1.93 8440
500 2.41 1.05 × 104
600 2.89 1.27 × 104
700 3.37 1.48 × 104
800 3.85 1.69 × 104
900 4.34 1.90 × 104
1000 4.82 2.11 × 104
2000 9.64 4.22 × 104
3000 14.5 6.33 × 104
4000 19.3 8.44 × 104
5000 24.1 1.05 × 105
5730 27.6 1.21 × 105
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 1.24 4300
200 1.54 5340
300 2.32 8010
400 3.09 1.07 × 104
500 3.86 1.33 × 104
600 4.63 1.60 × 104
700 5.40 1.87 × 104
800 6.17 2.14 × 104
900 6.95 2.40 × 104
1000 7.72 2.67 × 104
2000 15.4 5.34 × 104
3000 23.2 8.01 × 104
3570 27.6 9.54 × 104
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 1.89 5300
200 2.35 6590
300 3.53 9880
400 4.71 1.32 × 104
500 5.88 1.65 × 104
600 7.06 1.98 × 104
700 8.23 2.31 × 104
800 9.41 2.64 × 104
900 10.6 2.97 × 104
1000 11.8 3.29 × 104
2000 23.5 6.59 × 104
2350 27.6 7.73 × 104
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 4.62 8290
200 5.74 1.03 × 104
300 8.62 1.54 × 104
400 11.5 2.06 × 104
500 14.4 2.57 × 104
600 17.2 3.09 × 104
700 20.1 3.60 × 104
800 23.0 4.12 × 104
900 25.8 4.63 × 104
961 27.6 4.95 × 104
Steel I Beam: W27 × 161 (Wide Flange 27 inch tall × 161 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
161 9.59 1.19 × 104
200 11.9 1.48 × 104
300 17.9 2.22 × 104
400 23.8 2.97 × 104
463 27.6 3.43 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2009 eFunda, Inc.