Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W14 × 193
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 2400 in4) for the W14 × 193 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 2.51 × 10-6 6.72
200 2.60 × 10-6 6.97
300 3.91 × 10-6 10.4
400 5.21 × 10-6 13.9
500 6.51 × 10-6 17.4
600 7.81 × 10-6 20.9
700 9.11 × 10-6 24.4
800 1.04 × 10-5 27.9
900 1.17 × 10-5 31.3
1000 1.30 × 10-5 34.8
2000 2.60 × 10-5 69.7
3000 3.91 × 10-5 104
4000 5.21 × 10-5 139
5000 6.51 × 10-5 174
6000 7.81 × 10-5 209
7000 9.11 × 10-5 244
8000 1.04 × 10-4 279
9000 1.17 × 10-4 313
1.00 × 104 1.30 × 10-4 348
2.00 × 104 2.60 × 10-4 697
3.00 × 104 3.91 × 10-4 1040
4.00 × 104 5.21 × 10-4 1390
5.00 × 104 6.51 × 10-4 1740
6.00 × 104 7.81 × 10-4 2090
7.00 × 104 9.11 × 10-4 2440
8.00 × 104 0.00104 2790
9.00 × 104 0.00117 3130
1.00 × 105 0.00130 3480
2.00 × 105 0.00260 6970
3.00 × 105 0.00391 1.04 × 104
4.00 × 105 0.00521 1.39 × 104
5.00 × 105 0.00651 1.74 × 104
6.00 × 105 0.00781 2.09 × 104
7.00 × 105 0.00911 2.44 × 104
8.00 × 105 0.0104 2.79 × 104
9.00 × 105 0.0117 3.13 × 104
1.00 × 106 0.0130 3.48 × 104
2.00 × 106 0.0260 6.97 × 104
3.00 × 106 0.0391 1.04 × 105
4.00 × 106 0.0521 1.39 × 105
5.00 × 106 0.0651 1.74 × 105
6.00 × 106 0.0781 2.09 × 105
7.00 × 106 0.0911 2.44 × 105
8.00 × 106 0.104 2.79 × 105
8.53 × 106 0.111 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 1.94 × 10-5 18.7
200 2.01 × 10-5 19.4
300 3.01 × 10-5 29.0
400 4.02 × 10-5 38.7
500 5.02 × 10-5 48.4
600 6.03 × 10-5 58.0
700 7.03 × 10-5 67.7
800 8.04 × 10-5 77.4
900 9.04 × 10-5 87.1
1000 1.00 × 10-4 96.8
2000 2.01 × 10-4 194
3000 3.01 × 10-4 290
4000 4.02 × 10-4 387
5000 5.02 × 10-4 484
6000 6.03 × 10-4 581
7000 7.03 × 10-4 677
8000 8.04 × 10-4 774
9000 9.04 × 10-4 871
1.00 × 104 0.00100 968
2.00 × 104 0.00201 1940
3.00 × 104 0.00301 2900
4.00 × 104 0.00402 3870
5.00 × 104 0.00502 4840
6.00 × 104 0.00603 5810
7.00 × 104 0.00703 6770
8.00 × 104 0.00804 7740
9.00 × 104 0.00904 8710
1.00 × 105 0.0100 9680
2.00 × 105 0.0201 1.94 × 104
3.00 × 105 0.0301 2.90 × 104
4.00 × 105 0.0402 3.87 × 104
5.00 × 105 0.0502 4.84 × 104
6.00 × 105 0.0603 5.81 × 104
7.00 × 105 0.0703 6.77 × 104
8.00 × 105 0.0804 7.74 × 104
9.00 × 105 0.0904 8.71 × 104
1.00 × 106 0.100 9.68 × 104
2.00 × 106 0.201 1.94 × 105
3.00 × 106 0.301 2.90 × 105
3.07 × 106 0.308 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 3.10 × 10-4 74.7
200 3.21 × 10-4 77.4
300 4.82 × 10-4 116
400 6.43 × 10-4 155
500 8.04 × 10-4 194
600 9.64 × 10-4 232
700 0.00113 271
800 0.00129 310
900 0.00145 348
1000 0.00161 387
2000 0.00321 774
3000 0.00482 1160
4000 0.00643 1550
5000 0.00804 1940
6000 0.00964 2320
7000 0.0113 2710
8000 0.0129 3100
9000 0.0145 3480
1.00 × 104 0.0161 3870
2.00 × 104 0.0321 7740
3.00 × 104 0.0482 1.16 × 104
4.00 × 104 0.0643 1.55 × 104
5.00 × 104 0.0804 1.94 × 104
6.00 × 104 0.0964 2.32 × 104
7.00 × 104 0.113 2.71 × 104
8.00 × 104 0.129 3.10 × 104
9.00 × 104 0.145 3.48 × 104
1.00 × 105 0.161 3.87 × 104
2.00 × 105 0.321 7.74 × 104
3.00 × 105 0.482 1.16 × 105
4.00 × 105 0.643 1.55 × 105
5.00 × 105 0.804 1.94 × 105
6.00 × 105 0.964 2.32 × 105
7.00 × 105 1.13 2.71 × 105
7.68 × 105 1.23 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.00157 168
200 0.00163 174
300 0.00244 261
400 0.00326 348
500 0.00407 435
600 0.00488 522
700 0.00570 610
800 0.00651 697
900 0.00732 784
1000 0.00814 871
2000 0.0163 1740
3000 0.0244 2610
4000 0.0326 3480
5000 0.0407 4350
6000 0.0488 5220
7000 0.0570 6100
8000 0.0651 6970
9000 0.0732 7840
1.00 × 104 0.0814 8710
2.00 × 104 0.163 1.74 × 104
3.00 × 104 0.244 2.61 × 104
4.00 × 104 0.326 3.48 × 104
5.00 × 104 0.407 4.35 × 104
6.00 × 104 0.488 5.22 × 104
7.00 × 104 0.570 6.10 × 104
8.00 × 104 0.651 6.97 × 104
9.00 × 104 0.732 7.84 × 104
1.00 × 105 0.814 8.71 × 104
2.00 × 105 1.63 1.74 × 105
3.00 × 105 2.44 2.61 × 105
3.41 × 105 2.78 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.00496 299
200 0.00514 310
300 0.00772 464
400 0.0103 619
500 0.0129 774
600 0.0154 929
700 0.0180 1080
800 0.0206 1240
900 0.0231 1390
1000 0.0257 1550
2000 0.0514 3100
3000 0.0772 4640
4000 0.103 6190
5000 0.129 7740
6000 0.154 9290
7000 0.180 1.08 × 104
8000 0.206 1.24 × 104
9000 0.231 1.39 × 104
1.00 × 104 0.257 1.55 × 104
2.00 × 104 0.514 3.10 × 104
3.00 × 104 0.772 4.64 × 104
4.00 × 104 1.03 6.19 × 104
5.00 × 104 1.29 7.74 × 104
6.00 × 104 1.54 9.29 × 104
7.00 × 104 1.80 1.08 × 105
8.00 × 104 2.06 1.24 × 105
9.00 × 104 2.31 1.39 × 105
1.00 × 105 2.57 1.55 × 105
1.92 × 105 4.94 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.0121 467
200 0.0126 484
300 0.0188 726
400 0.0251 968
500 0.0314 1210
600 0.0377 1450
700 0.0440 1690
800 0.0502 1940
900 0.0565 2180
1000 0.0628 2420
2000 0.126 4840
3000 0.188 7260
4000 0.251 9680
5000 0.314 1.21 × 104
6000 0.377 1.45 × 104
7000 0.440 1.69 × 104
8000 0.502 1.94 × 104
9000 0.565 2.18 × 104
1.00 × 104 0.628 2.42 × 104
2.00 × 104 1.26 4.84 × 104
3.00 × 104 1.88 7.26 × 104
4.00 × 104 2.51 9.68 × 104
5.00 × 104 3.14 1.21 × 105
6.00 × 104 3.77 1.45 × 105
7.00 × 104 4.40 1.69 × 105
8.00 × 104 5.02 1.94 × 105
9.00 × 104 5.65 2.18 × 105
1.00 × 105 6.28 2.42 × 105
1.23 × 105 7.71 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.0251 672
200 0.0260 697
300 0.0391 1040
400 0.0521 1390
500 0.0651 1740
600 0.0781 2090
700 0.0911 2440
800 0.104 2790
900 0.117 3130
1000 0.130 3480
2000 0.260 6970
3000 0.391 1.04 × 104
4000 0.521 1.39 × 104
5000 0.651 1.74 × 104
6000 0.781 2.09 × 104
7000 0.911 2.44 × 104
8000 1.04 2.79 × 104
9000 1.17 3.13 × 104
1.00 × 104 1.30 3.48 × 104
2.00 × 104 2.60 6.97 × 104
3.00 × 104 3.91 1.04 × 105
4.00 × 104 5.21 1.39 × 105
5.00 × 104 6.51 1.74 × 105
6.00 × 104 7.81 2.09 × 105
7.00 × 104 9.11 2.44 × 105
8.00 × 104 10.4 2.79 × 105
8.53 × 104 11.1 2.97 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.0794 1200
200 0.0823 1240
300 0.123 1860
400 0.165 2480
500 0.206 3100
600 0.247 3720
700 0.288 4330
800 0.329 4950
900 0.370 5570
1000 0.412 6190
2000 0.823 1.24 × 104
3000 1.23 1.86 × 104
4000 1.65 2.48 × 104
5000 2.06 3.10 × 104
6000 2.47 3.72 × 104
7000 2.88 4.33 × 104
8000 3.29 4.95 × 104
9000 3.70 5.57 × 104
1.00 × 104 4.12 6.19 × 104
2.00 × 104 8.23 1.24 × 105
3.00 × 104 12.3 1.86 × 105
3.76 × 104 15.5 2.33 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.194 1870
200 0.201 1940
300 0.301 2900
400 0.402 3870
500 0.502 4840
600 0.603 5810
700 0.703 6770
800 0.804 7740
900 0.904 8710
1000 1.00 9680
2000 2.01 1.94 × 104
3000 3.01 2.90 × 104
4000 4.02 3.87 × 104
5000 5.02 4.84 × 104
6000 6.03 5.81 × 104
7000 7.03 6.77 × 104
8000 8.04 7.74 × 104
9000 9.04 8.71 × 104
1.00 × 104 10.0 9.68 × 104
1.54 × 104 15.5 1.49 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.402 2690
200 0.417 2790
300 0.625 4180
400 0.833 5570
500 1.04 6970
600 1.25 8360
700 1.46 9750
800 1.67 1.11 × 104
900 1.87 1.25 × 104
1000 2.08 1.39 × 104
2000 4.17 2.79 × 104
3000 6.25 4.18 × 104
4000 8.33 5.57 × 104
5000 10.4 6.97 × 104
6000 12.5 8.36 × 104
7000 14.6 9.75 × 104
7430 15.5 1.04 × 105
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 0.745 3660
200 0.772 3790
300 1.16 5690
400 1.54 7590
500 1.93 9480
600 2.32 1.14 × 104
700 2.70 1.33 × 104
800 3.09 1.52 × 104
900 3.47 1.71 × 104
1000 3.86 1.90 × 104
2000 7.72 3.79 × 104
3000 11.6 5.69 × 104
4000 15.4 7.59 × 104
4010 15.5 7.61 × 104
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 1.27 4780
200 1.32 4950
300 1.98 7430
400 2.63 9910
500 3.29 1.24 × 104
600 3.95 1.49 × 104
700 4.61 1.73 × 104
800 5.27 1.98 × 104
900 5.93 2.23 × 104
1000 6.58 2.48 × 104
2000 13.2 4.95 × 104
2350 15.5 5.82 × 104
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 2.04 6050
200 2.11 6270
300 3.16 9400
400 4.22 1.25 × 104
500 5.27 1.57 × 104
600 6.33 1.88 × 104
700 7.38 2.19 × 104
800 8.44 2.51 × 104
900 9.49 2.82 × 104
1000 10.5 3.13 × 104
1470 15.5 4.60 × 104
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 3.10 7470
200 3.21 7740
300 4.82 1.16 × 104
400 6.43 1.55 × 104
500 8.04 1.94 × 104
600 9.64 2.32 × 104
700 11.3 2.71 × 104
800 12.9 3.10 × 104
900 14.5 3.48 × 104
963 15.5 3.73 × 104
Steel I Beam: W14 × 193 (Wide Flange 14 inch tall × 193 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
193 7.57 1.17 × 104
200 7.85 1.21 × 104
300 11.8 1.81 × 104
394 15.5 2.39 × 104
Additional Information