engineering fundamentals
Wide Flange Steel I Beam: W14 × 342
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W14 × 342
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 4900 in4) for the W14 × 342 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 2.18 × 10-6 6.61
400 2.55 × 10-6 7.73
500 3.19 × 10-6 9.66
600 3.83 × 10-6 11.6
700 4.46 × 10-6 13.5
800 5.10 × 10-6 15.5
900 5.74 × 10-6 17.4
1000 6.38 × 10-6 19.3
2000 1.28 × 10-5 38.7
3000 1.91 × 10-5 58.0
4000 2.55 × 10-5 77.3
5000 3.19 × 10-5 96.6
6000 3.83 × 10-5 116
7000 4.46 × 10-5 135
8000 5.10 × 10-5 155
9000 5.74 × 10-5 174
1.00 × 104 6.38 × 10-5 193
2.00 × 104 1.28 × 10-4 387
3.00 × 104 1.91 × 10-4 580
4.00 × 104 2.55 × 10-4 773
5.00 × 104 3.19 × 10-4 966
6.00 × 104 3.83 × 10-4 1160
7.00 × 104 4.46 × 10-4 1350
8.00 × 104 5.10 × 10-4 1550
9.00 × 104 5.74 × 10-4 1740
1.00 × 105 6.38 × 10-4 1930
2.00 × 105 0.00128 3870
3.00 × 105 0.00191 5800
4.00 × 105 0.00255 7730
5.00 × 105 0.00319 9660
6.00 × 105 0.00383 1.16 × 104
7.00 × 105 0.00446 1.35 × 104
8.00 × 105 0.00510 1.55 × 104
9.00 × 105 0.00574 1.74 × 104
1.00 × 106 0.00638 1.93 × 104
2.00 × 106 0.0128 3.87 × 104
3.00 × 106 0.0191 5.80 × 104
4.00 × 106 0.0255 7.73 × 104
5.00 × 106 0.0319 9.66 × 104
6.00 × 106 0.0383 1.16 × 105
7.00 × 106 0.0446 1.35 × 105
8.00 × 106 0.0510 1.55 × 105
9.00 × 106 0.0574 1.74 × 105
1.00 × 107 0.0638 1.93 × 105
1.54 × 107 0.0980 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 1.68 × 10-5 18.4
400 1.97 × 10-5 21.5
500 2.46 × 10-5 26.8
600 2.95 × 10-5 32.2
700 3.44 × 10-5 37.6
800 3.94 × 10-5 43.0
900 4.43 × 10-5 48.3
1000 4.92 × 10-5 53.7
2000 9.84 × 10-5 107
3000 1.48 × 10-4 161
4000 1.97 × 10-4 215
5000 2.46 × 10-4 268
6000 2.95 × 10-4 322
7000 3.44 × 10-4 376
8000 3.94 × 10-4 430
9000 4.43 × 10-4 483
1.00 × 104 4.92 × 10-4 537
2.00 × 104 9.84 × 10-4 1070
3.00 × 104 0.00148 1610
4.00 × 104 0.00197 2150
5.00 × 104 0.00246 2680
6.00 × 104 0.00295 3220
7.00 × 104 0.00344 3760
8.00 × 104 0.00394 4300
9.00 × 104 0.00443 4830
1.00 × 105 0.00492 5370
2.00 × 105 0.00984 1.07 × 104
3.00 × 105 0.0148 1.61 × 104
4.00 × 105 0.0197 2.15 × 104
5.00 × 105 0.0246 2.68 × 104
6.00 × 105 0.0295 3.22 × 104
7.00 × 105 0.0344 3.76 × 104
8.00 × 105 0.0394 4.30 × 104
9.00 × 105 0.0443 4.83 × 104
1.00 × 106 0.0492 5.37 × 104
2.00 × 106 0.0984 1.07 × 105
3.00 × 106 0.148 1.61 × 105
4.00 × 106 0.197 2.15 × 105
5.00 × 106 0.246 2.68 × 105
5.53 × 106 0.272 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 2.69 × 10-4 73.5
400 3.15 × 10-4 85.9
500 3.94 × 10-4 107
600 4.72 × 10-4 129
700 5.51 × 10-4 150
800 6.30 × 10-4 172
900 7.09 × 10-4 193
1000 7.87 × 10-4 215
2000 0.00157 430
3000 0.00236 644
4000 0.00315 859
5000 0.00394 1070
6000 0.00472 1290
7000 0.00551 1500
8000 0.00630 1720
9000 0.00709 1930
1.00 × 104 0.00787 2150
2.00 × 104 0.0157 4300
3.00 × 104 0.0236 6440
4.00 × 104 0.0315 8590
5.00 × 104 0.0394 1.07 × 104
6.00 × 104 0.0472 1.29 × 104
7.00 × 104 0.0551 1.50 × 104
8.00 × 104 0.0630 1.72 × 104
9.00 × 104 0.0709 1.93 × 104
1.00 × 105 0.0787 2.15 × 104
2.00 × 105 0.157 4.30 × 104
3.00 × 105 0.236 6.44 × 104
4.00 × 105 0.315 8.59 × 104
5.00 × 105 0.394 1.07 × 105
6.00 × 105 0.472 1.29 × 105
7.00 × 105 0.551 1.50 × 105
8.00 × 105 0.630 1.72 × 105
9.00 × 105 0.709 1.93 × 105
1.00 × 106 0.787 2.15 × 105
1.38 × 106 1.09 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.00136 165
400 0.00159 193
500 0.00199 242
600 0.00239 290
700 0.00279 338
800 0.00319 387
900 0.00359 435
1000 0.00399 483
2000 0.00797 966
3000 0.0120 1450
4000 0.0159 1930
5000 0.0199 2420
6000 0.0239 2900
7000 0.0279 3380
8000 0.0319 3870
9000 0.0359 4350
1.00 × 104 0.0399 4830
2.00 × 104 0.0797 9660
3.00 × 104 0.120 1.45 × 104
4.00 × 104 0.159 1.93 × 104
5.00 × 104 0.199 2.42 × 104
6.00 × 104 0.239 2.90 × 104
7.00 × 104 0.279 3.38 × 104
8.00 × 104 0.319 3.87 × 104
9.00 × 104 0.359 4.35 × 104
1.00 × 105 0.399 4.83 × 104
2.00 × 105 0.797 9.66 × 104
3.00 × 105 1.20 1.45 × 105
4.00 × 105 1.59 1.93 × 105
5.00 × 105 1.99 2.42 × 105
6.00 × 105 2.39 2.90 × 105
6.15 × 105 2.45 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.00431 294
400 0.00504 344
500 0.00630 430
600 0.00756 515
700 0.00882 601
800 0.0101 687
900 0.0113 773
1000 0.0126 859
2000 0.0252 1720
3000 0.0378 2580
4000 0.0504 3440
5000 0.0630 4300
6000 0.0756 5150
7000 0.0882 6010
8000 0.101 6870
9000 0.113 7730
1.00 × 104 0.126 8590
2.00 × 104 0.252 1.72 × 104
3.00 × 104 0.378 2.58 × 104
4.00 × 104 0.504 3.44 × 104
5.00 × 104 0.630 4.30 × 104
6.00 × 104 0.756 5.15 × 104
7.00 × 104 0.882 6.01 × 104
8.00 × 104 1.01 6.87 × 104
9.00 × 104 1.13 7.73 × 104
1.00 × 105 1.26 8.59 × 104
2.00 × 105 2.52 1.72 × 105
3.00 × 105 3.78 2.58 × 105
3.46 × 105 4.36 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.0105 459
400 0.0123 537
500 0.0154 671
600 0.0185 805
700 0.0215 940
800 0.0246 1070
900 0.0277 1210
1000 0.0308 1340
2000 0.0615 2680
3000 0.0923 4030
4000 0.123 5370
5000 0.154 6710
6000 0.185 8050
7000 0.215 9400
8000 0.246 1.07 × 104
9000 0.277 1.21 × 104
1.00 × 104 0.308 1.34 × 104
2.00 × 104 0.615 2.68 × 104
3.00 × 104 0.923 4.03 × 104
4.00 × 104 1.23 5.37 × 104
5.00 × 104 1.54 6.71 × 104
6.00 × 104 1.85 8.05 × 104
7.00 × 104 2.15 9.40 × 104
8.00 × 104 2.46 1.07 × 105
9.00 × 104 2.77 1.21 × 105
1.00 × 105 3.08 1.34 × 105
2.00 × 105 6.15 2.68 × 105
2.21 × 105 6.81 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.0218 661
400 0.0255 773
500 0.0319 966
600 0.0383 1160
700 0.0446 1350
800 0.0510 1550
900 0.0574 1740
1000 0.0638 1930
2000 0.128 3870
3000 0.191 5800
4000 0.255 7730
5000 0.319 9660
6000 0.383 1.16 × 104
7000 0.446 1.35 × 104
8000 0.510 1.55 × 104
9000 0.574 1.74 × 104
1.00 × 104 0.638 1.93 × 104
2.00 × 104 1.28 3.87 × 104
3.00 × 104 1.91 5.80 × 104
4.00 × 104 2.55 7.73 × 104
5.00 × 104 3.19 9.66 × 104
6.00 × 104 3.83 1.16 × 105
7.00 × 104 4.46 1.35 × 105
8.00 × 104 5.10 1.55 × 105
9.00 × 104 5.74 1.74 × 105
1.00 × 105 6.38 1.93 × 105
1.54 × 105 9.80 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.0689 1180
400 0.0806 1370
500 0.101 1720
600 0.121 2060
700 0.141 2410
800 0.161 2750
900 0.181 3090
1000 0.202 3440
2000 0.403 6870
3000 0.605 1.03 × 104
4000 0.806 1.37 × 104
5000 1.01 1.72 × 104
6000 1.21 2.06 × 104
7000 1.41 2.41 × 104
8000 1.61 2.75 × 104
9000 1.81 3.09 × 104
1.00 × 104 2.02 3.44 × 104
2.00 × 104 4.03 6.87 × 104
3.00 × 104 6.05 1.03 × 105
4.00 × 104 8.06 1.37 × 105
5.00 × 104 10.1 1.72 × 105
6.00 × 104 12.1 2.06 × 105
7.00 × 104 14.1 2.41 × 105
8.00 × 104 16.1 2.75 × 105
8.64 × 104 17.4 2.97 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.168 1840
400 0.197 2150
500 0.246 2680
600 0.295 3220
700 0.344 3760
800 0.394 4300
900 0.443 4830
1000 0.492 5370
2000 0.984 1.07 × 104
3000 1.48 1.61 × 104
4000 1.97 2.15 × 104
5000 2.46 2.68 × 104
6000 2.95 3.22 × 104
7000 3.44 3.76 × 104
8000 3.94 4.30 × 104
9000 4.43 4.83 × 104
1.00 × 104 4.92 5.37 × 104
2.00 × 104 9.84 1.07 × 105
3.00 × 104 14.8 1.61 × 105
3.56 × 104 17.5 1.91 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.349 2640
400 0.408 3090
500 0.510 3870
600 0.612 4640
700 0.714 5410
800 0.816 6190
900 0.918 6960
1000 1.02 7730
2000 2.04 1.55 × 104
3000 3.06 2.32 × 104
4000 4.08 3.09 × 104
5000 5.10 3.87 × 104
6000 6.12 4.64 × 104
7000 7.14 5.41 × 104
8000 8.16 6.19 × 104
9000 9.18 6.96 × 104
1.00 × 104 10.2 7.73 × 104
1.72 × 104 17.5 1.33 × 105
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 0.647 3600
400 0.756 4210
500 0.945 5260
600 1.13 6310
700 1.32 7370
800 1.51 8420
900 1.70 9470
1000 1.89 1.05 × 104
2000 3.78 2.10 × 104
3000 5.67 3.16 × 104
4000 7.56 4.21 × 104
5000 9.45 5.26 × 104
6000 11.3 6.31 × 104
7000 13.2 7.37 × 104
8000 15.1 8.42 × 104
9000 17.0 9.47 × 104
9280 17.5 9.76 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 1.10 4700
400 1.29 5500
500 1.61 6870
600 1.93 8250
700 2.26 9620
800 2.58 1.10 × 104
900 2.90 1.24 × 104
1000 3.22 1.37 × 104
2000 6.45 2.75 × 104
3000 9.67 4.12 × 104
4000 12.9 5.50 × 104
5000 16.1 6.87 × 104
5440 17.5 7.48 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 1.77 5950
400 2.07 6960
500 2.58 8700
600 3.10 1.04 × 104
700 3.62 1.22 × 104
800 4.13 1.39 × 104
900 4.65 1.57 × 104
1000 5.17 1.74 × 104
2000 10.3 3.48 × 104
3000 15.5 5.22 × 104
3400 17.5 5.91 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 2.69 7350
400 3.15 8590
500 3.94 1.07 × 104
600 4.72 1.29 × 104
700 5.51 1.50 × 104
800 6.30 1.72 × 104
900 7.09 1.93 × 104
1000 7.87 2.15 × 104
2000 15.7 4.30 × 104
2230 17.5 4.78 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 6.57 1.15 × 104
400 7.69 1.34 × 104
500 9.61 1.68 × 104
600 11.5 2.01 × 104
700 13.5 2.35 × 104
800 15.4 2.68 × 104
900 17.3 3.02 × 104
913 17.5 3.06 × 104
Steel I Beam: W14 × 342 (Wide Flange 14 inch tall × 342 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
342 13.6 1.65 × 104
400 15.9 1.93 × 104
440 17.5 2.13 × 104
Additional Information