For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 6600 in4) for the W14 × 426 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 2.02 × 10-6 6.51
500 2.37 × 10-6 7.64
600 2.84 × 10-6 9.17
700 3.31 × 10-6 10.7
800 3.79 × 10-6 12.2
900 4.26 × 10-6 13.7
1000 4.73 × 10-6 15.3
2000 9.47 × 10-6 30.6
3000 1.42 × 10-5 45.8
4000 1.89 × 10-5 61.1
5000 2.37 × 10-5 76.4
6000 2.84 × 10-5 91.7
7000 3.31 × 10-5 107
8000 3.79 × 10-5 122
9000 4.26 × 10-5 137
1.00 × 104 4.73 × 10-5 153
2.00 × 104 9.47 × 10-5 306
3.00 × 104 1.42 × 10-4 458
4.00 × 104 1.89 × 10-4 611
5.00 × 104 2.37 × 10-4 764
6.00 × 104 2.84 × 10-4 917
7.00 × 104 3.31 × 10-4 1070
8.00 × 104 3.79 × 10-4 1220
9.00 × 104 4.26 × 10-4 1370
1.00 × 105 4.73 × 10-4 1530
2.00 × 105 9.47 × 10-4 3060
3.00 × 105 0.00142 4580
4.00 × 105 0.00189 6110
5.00 × 105 0.00237 7640
6.00 × 105 0.00284 9170
7.00 × 105 0.00331 1.07 × 104
8.00 × 105 0.00379 1.22 × 104
9.00 × 105 0.00426 1.37 × 104
1.00 × 106 0.00473 1.53 × 104
2.00 × 106 0.00947 3.06 × 104
3.00 × 106 0.0142 4.58 × 104
4.00 × 106 0.0189 6.11 × 104
5.00 × 106 0.0237 7.64 × 104
6.00 × 106 0.0284 9.17 × 104
7.00 × 106 0.0331 1.07 × 105
8.00 × 106 0.0379 1.22 × 105
9.00 × 106 0.0426 1.37 × 105
1.00 × 107 0.0473 1.53 × 105
1.94 × 107 0.0921 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 1.56 × 10-5 18.1
500 1.83 × 10-5 21.2
600 2.19 × 10-5 25.5
700 2.56 × 10-5 29.7
800 2.92 × 10-5 33.9
900 3.29 × 10-5 38.2
1000 3.65 × 10-5 42.4
2000 7.31 × 10-5 84.9
3000 1.10 × 10-4 127
4000 1.46 × 10-4 170
5000 1.83 × 10-4 212
6000 2.19 × 10-4 255
7000 2.56 × 10-4 297
8000 2.92 × 10-4 339
9000 3.29 × 10-4 382
1.00 × 104 3.65 × 10-4 424
2.00 × 104 7.31 × 10-4 849
3.00 × 104 0.00110 1270
4.00 × 104 0.00146 1700
5.00 × 104 0.00183 2120
6.00 × 104 0.00219 2550
7.00 × 104 0.00256 2970
8.00 × 104 0.00292 3390
9.00 × 104 0.00329 3820
1.00 × 105 0.00365 4240
2.00 × 105 0.00731 8490
3.00 × 105 0.0110 1.27 × 104
4.00 × 105 0.0146 1.70 × 104
5.00 × 105 0.0183 2.12 × 104
6.00 × 105 0.0219 2.55 × 104
7.00 × 105 0.0256 2.97 × 104
8.00 × 105 0.0292 3.39 × 104
9.00 × 105 0.0329 3.82 × 104
1.00 × 106 0.0365 4.24 × 104
2.00 × 106 0.0731 8.49 × 104
3.00 × 106 0.110 1.27 × 105
4.00 × 106 0.146 1.70 × 105
5.00 × 106 0.183 2.12 × 105
6.00 × 106 0.219 2.55 × 105
7.00 × 106 0.256 2.97 × 105
7.00 × 106 0.256 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 2.49 × 10-4 72.3
500 2.92 × 10-4 84.9
600 3.51 × 10-4 102
700 4.09 × 10-4 119
800 4.68 × 10-4 136
900 5.26 × 10-4 153
1000 5.85 × 10-4 170
2000 0.00117 339
3000 0.00175 509
4000 0.00234 679
5000 0.00292 849
6000 0.00351 1020
7000 0.00409 1190
8000 0.00468 1360
9000 0.00526 1530
1.00 × 104 0.00585 1700
2.00 × 104 0.0117 3390
3.00 × 104 0.0175 5090
4.00 × 104 0.0234 6790
5.00 × 104 0.0292 8490
6.00 × 104 0.0351 1.02 × 104
7.00 × 104 0.0409 1.19 × 104
8.00 × 104 0.0468 1.36 × 104
9.00 × 104 0.0526 1.53 × 104
1.00 × 105 0.0585 1.70 × 104
2.00 × 105 0.117 3.39 × 104
3.00 × 105 0.175 5.09 × 104
4.00 × 105 0.234 6.79 × 104
5.00 × 105 0.292 8.49 × 104
6.00 × 105 0.351 1.02 × 105
7.00 × 105 0.409 1.19 × 105
8.00 × 105 0.468 1.36 × 105
9.00 × 105 0.526 1.53 × 105
1.00 × 106 0.585 1.70 × 105
1.75 × 106 1.02 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.00126 163
500 0.00148 191
600 0.00178 229
700 0.00207 267
800 0.00237 306
900 0.00266 344
1000 0.00296 382
2000 0.00592 764
3000 0.00888 1150
4000 0.0118 1530
5000 0.0148 1910
6000 0.0178 2290
7000 0.0207 2670
8000 0.0237 3060
9000 0.0266 3440
1.00 × 104 0.0296 3820
2.00 × 104 0.0592 7640
3.00 × 104 0.0888 1.15 × 104
4.00 × 104 0.118 1.53 × 104
5.00 × 104 0.148 1.91 × 104
6.00 × 104 0.178 2.29 × 104
7.00 × 104 0.207 2.67 × 104
8.00 × 104 0.237 3.06 × 104
9.00 × 104 0.266 3.44 × 104
1.00 × 105 0.296 3.82 × 104
2.00 × 105 0.592 7.64 × 104
3.00 × 105 0.888 1.15 × 105
4.00 × 105 1.18 1.53 × 105
5.00 × 105 1.48 1.91 × 105
6.00 × 105 1.78 2.29 × 105
7.00 × 105 2.07 2.67 × 105
7.78 × 105 2.30 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.00398 289
500 0.00468 339
600 0.00561 407
700 0.00655 475
800 0.00748 543
900 0.00842 611
1000 0.00935 679
2000 0.0187 1360
3000 0.0281 2040
4000 0.0374 2720
5000 0.0468 3390
6000 0.0561 4070
7000 0.0655 4750
8000 0.0748 5430
9000 0.0842 6110
1.00 × 104 0.0935 6790
2.00 × 104 0.187 1.36 × 104
3.00 × 104 0.281 2.04 × 104
4.00 × 104 0.374 2.72 × 104
5.00 × 104 0.468 3.39 × 104
6.00 × 104 0.561 4.07 × 104
7.00 × 104 0.655 4.75 × 104
8.00 × 104 0.748 5.43 × 104
9.00 × 104 0.842 6.11 × 104
1.00 × 105 0.935 6.79 × 104
2.00 × 105 1.87 1.36 × 105
3.00 × 105 2.81 2.04 × 105
4.00 × 105 3.74 2.72 × 105
4.38 × 105 4.09 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.00973 452
500 0.0114 530
600 0.0137 636
700 0.0160 743
800 0.0183 849
900 0.0205 955
1000 0.0228 1060
2000 0.0457 2120
3000 0.0685 3180
4000 0.0913 4240
5000 0.114 5300
6000 0.137 6360
7000 0.160 7430
8000 0.183 8490
9000 0.205 9550
1.00 × 104 0.228 1.06 × 104
2.00 × 104 0.457 2.12 × 104
3.00 × 104 0.685 3.18 × 104
4.00 × 104 0.913 4.24 × 104
5.00 × 104 1.14 5.30 × 104
6.00 × 104 1.37 6.36 × 104
7.00 × 104 1.60 7.43 × 104
8.00 × 104 1.83 8.49 × 104
9.00 × 104 2.05 9.55 × 104
1.00 × 105 2.28 1.06 × 105
2.00 × 105 4.57 2.12 × 105
2.80 × 105 6.39 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.0202 651
500 0.0237 764
600 0.0284 917
700 0.0331 1070
800 0.0379 1220
900 0.0426 1370
1000 0.0473 1530
2000 0.0947 3060
3000 0.142 4580
4000 0.189 6110
5000 0.237 7640
6000 0.284 9170
7000 0.331 1.07 × 104
8000 0.379 1.22 × 104
9000 0.426 1.37 × 104
1.00 × 104 0.473 1.53 × 104
2.00 × 104 0.947 3.06 × 104
3.00 × 104 1.42 4.58 × 104
4.00 × 104 1.89 6.11 × 104
5.00 × 104 2.37 7.64 × 104
6.00 × 104 2.84 9.17 × 104
7.00 × 104 3.31 1.07 × 105
8.00 × 104 3.79 1.22 × 105
9.00 × 104 4.26 1.37 × 105
1.00 × 105 4.73 1.53 × 105
1.94 × 105 9.21 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.0637 1160
500 0.0748 1360
600 0.0898 1630
700 0.105 1900
800 0.120 2170
900 0.135 2440
1000 0.150 2720
2000 0.299 5430
3000 0.449 8150
4000 0.599 1.09 × 104
5000 0.748 1.36 × 104
6000 0.898 1.63 × 104
7000 1.05 1.90 × 104
8000 1.20 2.17 × 104
9000 1.35 2.44 × 104
1.00 × 104 1.50 2.72 × 104
2.00 × 104 2.99 5.43 × 104
3.00 × 104 4.49 8.15 × 104
4.00 × 104 5.99 1.09 × 105
5.00 × 104 7.48 1.36 × 105
6.00 × 104 8.98 1.63 × 105
7.00 × 104 10.5 1.90 × 105
8.00 × 104 12.0 2.17 × 105
9.00 × 104 13.5 2.44 × 105
1.00 × 105 15.0 2.72 × 105
1.09 × 105 16.4 2.97 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.156 1810
500 0.183 2120
600 0.219 2550
700 0.256 2970
800 0.292 3390
900 0.329 3820
1000 0.365 4240
2000 0.731 8490
3000 1.10 1.27 × 104
4000 1.46 1.70 × 104
5000 1.83 2.12 × 104
6000 2.19 2.55 × 104
7000 2.56 2.97 × 104
8000 2.92 3.39 × 104
9000 3.29 3.82 × 104
1.00 × 104 3.65 4.24 × 104
2.00 × 104 7.31 8.49 × 104
3.00 × 104 11.0 1.27 × 105
4.00 × 104 14.6 1.70 × 105
5.00 × 104 18.3 2.12 × 105
5.11 × 104 18.7 2.17 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.323 2600
500 0.379 3060
600 0.455 3670
700 0.530 4280
800 0.606 4890
900 0.682 5500
1000 0.758 6110
2000 1.52 1.22 × 104
3000 2.27 1.83 × 104
4000 3.03 2.44 × 104
5000 3.79 3.06 × 104
6000 4.55 3.67 × 104
7000 5.30 4.28 × 104
8000 6.06 4.89 × 104
9000 6.82 5.50 × 104
1.00 × 104 7.58 6.11 × 104
2.00 × 104 15.2 1.22 × 105
2.46 × 104 18.7 1.51 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 0.598 3540
500 0.702 4160
600 0.842 4990
700 0.982 5820
800 1.12 6650
900 1.26 7480
1000 1.40 8320
2000 2.81 1.66 × 104
3000 4.21 2.49 × 104
4000 5.61 3.33 × 104
5000 7.02 4.16 × 104
6000 8.42 4.99 × 104
7000 9.82 5.82 × 104
8000 11.2 6.65 × 104
9000 12.6 7.48 × 104
1.00 × 104 14.0 8.32 × 104
1.33 × 104 18.7 1.11 × 105
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 1.02 4630
500 1.20 5430
600 1.44 6520
700 1.68 7600
800 1.92 8690
900 2.15 9780
1000 2.39 1.09 × 104
2000 4.79 2.17 × 104
3000 7.18 3.26 × 104
4000 9.58 4.35 × 104
5000 12.0 5.43 × 104
6000 14.4 6.52 × 104
7000 16.8 7.60 × 104
7800 18.7 8.47 × 104
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 1.63 5860
500 1.92 6870
600 2.30 8250
700 2.68 9620
800 3.07 1.10 × 104
900 3.45 1.24 × 104
1000 3.84 1.37 × 104
2000 7.67 2.75 × 104
3000 11.5 4.12 × 104
4000 15.3 5.50 × 104
4870 18.7 6.69 × 104
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 2.49 7230
500 2.92 8490
600 3.51 1.02 × 104
700 4.09 1.19 × 104
800 4.68 1.36 × 104
900 5.26 1.53 × 104
1000 5.85 1.70 × 104
2000 11.7 3.39 × 104
3000 17.5 5.09 × 104
3190 18.7 5.42 × 104
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 6.08 1.13 × 104
500 7.14 1.33 × 104
600 8.56 1.59 × 104
700 9.99 1.86 × 104
800 11.4 2.12 × 104
900 12.8 2.39 × 104
1000 14.3 2.65 × 104
1310 18.7 3.47 × 104
Steel I Beam: W14 × 426 (Wide Flange 14 inch tall × 426 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
426 12.6 1.63 × 104
500 14.8 1.91 × 104
600 17.8 2.29 × 104
631 18.7 2.41 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.