engineering fundamentals
Wide Flange Steel I Beam: W18 × 106
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W18 × 106
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1910 in4) for the W18 × 106 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.73 × 10-6 5.61
200 3.27 × 10-6 10.6
300 4.91 × 10-6 15.9
400 6.54 × 10-6 21.2
500 8.18 × 10-6 26.5
600 9.82 × 10-6 31.8
700 1.15 × 10-5 37.1
800 1.31 × 10-5 42.4
900 1.47 × 10-5 47.7
1000 1.64 × 10-5 53.0
2000 3.27 × 10-5 106
3000 4.91 × 10-5 159
4000 6.54 × 10-5 212
5000 8.18 × 10-5 265
6000 9.82 × 10-5 318
7000 1.15 × 10-4 371
8000 1.31 × 10-4 424
9000 1.47 × 10-4 477
1.00 × 104 1.64 × 10-4 530
2.00 × 104 3.27 × 10-4 1060
3.00 × 104 4.91 × 10-4 1590
4.00 × 104 6.54 × 10-4 2120
5.00 × 104 8.18 × 10-4 2650
6.00 × 104 9.82 × 10-4 3180
7.00 × 104 0.00115 3710
8.00 × 104 0.00131 4240
9.00 × 104 0.00147 4770
1.00 × 105 0.00164 5300
2.00 × 105 0.00327 1.06 × 104
3.00 × 105 0.00491 1.59 × 104
4.00 × 105 0.00654 2.12 × 104
5.00 × 105 0.00818 2.65 × 104
6.00 × 105 0.00982 3.18 × 104
7.00 × 105 0.0115 3.71 × 104
8.00 × 105 0.0131 4.24 × 104
9.00 × 105 0.0147 4.77 × 104
1.00 × 106 0.0164 5.30 × 104
2.00 × 106 0.0327 1.06 × 105
3.00 × 106 0.0491 1.59 × 105
4.00 × 106 0.0654 2.12 × 105
5.00 × 106 0.0818 2.65 × 105
5.61 × 106 0.0918 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.34 × 10-5 15.6
200 2.52 × 10-5 29.4
300 3.79 × 10-5 44.1
400 5.05 × 10-5 58.8
500 6.31 × 10-5 73.5
600 7.57 × 10-5 88.3
700 8.84 × 10-5 103
800 1.01 × 10-4 118
900 1.14 × 10-4 132
1000 1.26 × 10-4 147
2000 2.52 × 10-4 294
3000 3.79 × 10-4 441
4000 5.05 × 10-4 588
5000 6.31 × 10-4 735
6000 7.57 × 10-4 883
7000 8.84 × 10-4 1030
8000 0.00101 1180
9000 0.00114 1320
1.00 × 104 0.00126 1470
2.00 × 104 0.00252 2940
3.00 × 104 0.00379 4410
4.00 × 104 0.00505 5880
5.00 × 104 0.00631 7350
6.00 × 104 0.00757 8830
7.00 × 104 0.00884 1.03 × 104
8.00 × 104 0.0101 1.18 × 104
9.00 × 104 0.0114 1.32 × 104
1.00 × 105 0.0126 1.47 × 104
2.00 × 105 0.0252 2.94 × 104
3.00 × 105 0.0379 4.41 × 104
4.00 × 105 0.0505 5.88 × 104
5.00 × 105 0.0631 7.35 × 104
6.00 × 105 0.0757 8.83 × 104
7.00 × 105 0.0884 1.03 × 105
8.00 × 105 0.101 1.18 × 105
9.00 × 105 0.114 1.32 × 105
1.00 × 106 0.126 1.47 × 105
2.00 × 106 0.252 2.94 × 105
2.02 × 106 0.255 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.14 × 10-4 62.4
200 4.04 × 10-4 118
300 6.06 × 10-4 177
400 8.08 × 10-4 235
500 0.00101 294
600 0.00121 353
700 0.00141 412
800 0.00162 471
900 0.00182 530
1000 0.00202 588
2000 0.00404 1180
3000 0.00606 1770
4000 0.00808 2350
5000 0.0101 2940
6000 0.0121 3530
7000 0.0141 4120
8000 0.0162 4710
9000 0.0182 5300
1.00 × 104 0.0202 5880
2.00 × 104 0.0404 1.18 × 104
3.00 × 104 0.0606 1.77 × 104
4.00 × 104 0.0808 2.35 × 104
5.00 × 104 0.101 2.94 × 104
6.00 × 104 0.121 3.53 × 104
7.00 × 104 0.141 4.12 × 104
8.00 × 104 0.162 4.71 × 104
9.00 × 104 0.182 5.30 × 104
1.00 × 105 0.202 5.88 × 104
2.00 × 105 0.404 1.18 × 105
3.00 × 105 0.606 1.77 × 105
4.00 × 105 0.808 2.35 × 105
5.00 × 105 1.01 2.94 × 105
5.05 × 105 1.02 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00108 140
200 0.00205 265
300 0.00307 397
400 0.00409 530
500 0.00511 662
600 0.00614 794
700 0.00716 927
800 0.00818 1060
900 0.00920 1190
1000 0.0102 1320
2000 0.0205 2650
3000 0.0307 3970
4000 0.0409 5300
5000 0.0511 6620
6000 0.0614 7940
7000 0.0716 9270
8000 0.0818 1.06 × 104
9000 0.0920 1.19 × 104
1.00 × 104 0.102 1.32 × 104
2.00 × 104 0.205 2.65 × 104
3.00 × 104 0.307 3.97 × 104
4.00 × 104 0.409 5.30 × 104
5.00 × 104 0.511 6.62 × 104
6.00 × 104 0.614 7.94 × 104
7.00 × 104 0.716 9.27 × 104
8.00 × 104 0.818 1.06 × 105
9.00 × 104 0.920 1.19 × 105
1.00 × 105 1.02 1.32 × 105
2.00 × 105 2.05 2.65 × 105
2.24 × 105 2.29 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00343 249
200 0.00646 471
300 0.00970 706
400 0.0129 941
500 0.0162 1180
600 0.0194 1410
700 0.0226 1650
800 0.0259 1880
900 0.0291 2120
1000 0.0323 2350
2000 0.0646 4710
3000 0.0970 7060
4000 0.129 9410
5000 0.162 1.18 × 104
6000 0.194 1.41 × 104
7000 0.226 1.65 × 104
8000 0.259 1.88 × 104
9000 0.291 2.12 × 104
1.00 × 104 0.323 2.35 × 104
2.00 × 104 0.646 4.71 × 104
3.00 × 104 0.970 7.06 × 104
4.00 × 104 1.29 9.41 × 104
5.00 × 104 1.62 1.18 × 105
6.00 × 104 1.94 1.41 × 105
7.00 × 104 2.26 1.65 × 105
8.00 × 104 2.59 1.88 × 105
9.00 × 104 2.91 2.12 × 105
1.00 × 105 3.23 2.35 × 105
1.26 × 105 4.08 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.00836 390
200 0.0158 735
300 0.0237 1100
400 0.0316 1470
500 0.0395 1840
600 0.0473 2210
700 0.0552 2570
800 0.0631 2940
900 0.0710 3310
1000 0.0789 3680
2000 0.158 7350
3000 0.237 1.10 × 104
4000 0.316 1.47 × 104
5000 0.395 1.84 × 104
6000 0.473 2.21 × 104
7000 0.552 2.57 × 104
8000 0.631 2.94 × 104
9000 0.710 3.31 × 104
1.00 × 104 0.789 3.68 × 104
2.00 × 104 1.58 7.35 × 104
3.00 × 104 2.37 1.10 × 105
4.00 × 104 3.16 1.47 × 105
5.00 × 104 3.95 1.84 × 105
6.00 × 104 4.73 2.21 × 105
7.00 × 104 5.52 2.57 × 105
8.00 × 104 6.31 2.94 × 105
8.08 × 104 6.37 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0173 561
200 0.0327 1060
300 0.0491 1590
400 0.0654 2120
500 0.0818 2650
600 0.0982 3180
700 0.115 3710
800 0.131 4240
900 0.147 4770
1000 0.164 5300
2000 0.327 1.06 × 104
3000 0.491 1.59 × 104
4000 0.654 2.12 × 104
5000 0.818 2.65 × 104
6000 0.982 3.18 × 104
7000 1.15 3.71 × 104
8000 1.31 4.24 × 104
9000 1.47 4.77 × 104
1.00 × 104 1.64 5.30 × 104
2.00 × 104 3.27 1.06 × 105
3.00 × 104 4.91 1.59 × 105
4.00 × 104 6.54 2.12 × 105
5.00 × 104 8.18 2.65 × 105
5.61 × 104 9.18 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.0548 998
200 0.103 1880
300 0.155 2820
400 0.207 3770
500 0.259 4710
600 0.310 5650
700 0.362 6590
800 0.414 7530
900 0.465 8470
1000 0.517 9410
2000 1.03 1.88 × 104
3000 1.55 2.82 × 104
4000 2.07 3.77 × 104
5000 2.59 4.71 × 104
6000 3.10 5.65 × 104
7000 3.62 6.59 × 104
8000 4.14 7.53 × 104
9000 4.65 8.47 × 104
1.00 × 104 5.17 9.41 × 104
2.00 × 104 10.3 1.88 × 105
3.00 × 104 15.5 2.82 × 105
3.16 × 104 16.3 2.97 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.134 1560
200 0.252 2940
300 0.379 4410
400 0.505 5880
500 0.631 7350
600 0.757 8830
700 0.884 1.03 × 104
800 1.01 1.18 × 104
900 1.14 1.32 × 104
1000 1.26 1.47 × 104
2000 2.52 2.94 × 104
3000 3.79 4.41 × 104
4000 5.05 5.88 × 104
5000 6.31 7.35 × 104
6000 7.57 8.83 × 104
7000 8.84 1.03 × 105
8000 10.1 1.18 × 105
9000 11.4 1.32 × 105
1.00 × 104 12.6 1.47 × 105
1.48 × 104 18.7 2.18 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.277 2250
200 0.524 4240
300 0.785 6350
400 1.05 8470
500 1.31 1.06 × 104
600 1.57 1.27 × 104
700 1.83 1.48 × 104
800 2.09 1.69 × 104
900 2.36 1.91 × 104
1000 2.62 2.12 × 104
2000 5.24 4.24 × 104
3000 7.85 6.35 × 104
4000 10.5 8.47 × 104
5000 13.1 1.06 × 105
6000 15.7 1.27 × 105
7000 18.3 1.48 × 105
7160 18.7 1.52 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.514 3060
200 0.970 5770
300 1.45 8650
400 1.94 1.15 × 104
500 2.42 1.44 × 104
600 2.91 1.73 × 104
700 3.39 2.02 × 104
800 3.88 2.31 × 104
900 4.36 2.59 × 104
1000 4.85 2.88 × 104
2000 9.70 5.77 × 104
3000 14.5 8.65 × 104
3860 18.7 1.11 × 105
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 0.877 3990
200 1.65 7530
300 2.48 1.13 × 104
400 3.31 1.51 × 104
500 4.14 1.88 × 104
600 4.96 2.26 × 104
700 5.79 2.64 × 104
800 6.62 3.01 × 104
900 7.45 3.39 × 104
1000 8.27 3.77 × 104
2000 16.5 7.53 × 104
2260 18.7 8.53 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 1.40 5050
200 2.65 9530
300 3.98 1.43 × 104
400 5.30 1.91 × 104
500 6.63 2.38 × 104
600 7.95 2.86 × 104
700 9.28 3.34 × 104
800 10.6 3.81 × 104
900 11.9 4.29 × 104
1000 13.3 4.77 × 104
1410 18.7 6.74 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 2.14 6240
200 4.04 1.18 × 104
300 6.06 1.77 × 104
400 8.08 2.35 × 104
500 10.1 2.94 × 104
600 12.1 3.53 × 104
700 14.1 4.12 × 104
800 16.2 4.71 × 104
900 18.2 5.30 × 104
927 18.7 5.46 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 5.23 9740
200 9.86 1.84 × 104
300 14.8 2.76 × 104
380 18.7 3.49 × 104
Steel I Beam: W18 × 106 (Wide Flange 18 inch tall × 106 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
106 10.8 1.40 × 104
183 18.7 2.42 × 104
Additional Information