engineering fundamentals
Wide Flange Steel I Beam: W18 × 97
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Three Equal Spans » Wide Flange Steel I Beam » W18 × 97
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in three equal spans, we compute the displacement at the middle of the first and the third spans, and the maximum normal stress stress_max occuring at the second and third supports of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1750 in4) for the W18 × 97 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 1.73 × 10-6 5.56
100 1.79 × 10-6 5.74
200 3.57 × 10-6 11.5
300 5.36 × 10-6 17.2
400 7.14 × 10-6 22.9
500 8.93 × 10-6 28.7
600 1.07 × 10-5 34.4
700 1.25 × 10-5 40.2
800 1.43 × 10-5 45.9
900 1.61 × 10-5 51.6
1000 1.79 × 10-5 57.4
2000 3.57 × 10-5 115
3000 5.36 × 10-5 172
4000 7.14 × 10-5 229
5000 8.93 × 10-5 287
6000 1.07 × 10-4 344
7000 1.25 × 10-4 402
8000 1.43 × 10-4 459
9000 1.61 × 10-4 516
1.00 × 104 1.79 × 10-4 574
2.00 × 104 3.57 × 10-4 1150
3.00 × 104 5.36 × 10-4 1720
4.00 × 104 7.14 × 10-4 2290
5.00 × 104 8.93 × 10-4 2870
6.00 × 104 0.00107 3440
7.00 × 104 0.00125 4020
8.00 × 104 0.00143 4590
9.00 × 104 0.00161 5160
1.00 × 105 0.00179 5740
2.00 × 105 0.00357 1.15 × 104
3.00 × 105 0.00536 1.72 × 104
4.00 × 105 0.00714 2.29 × 104
5.00 × 105 0.00893 2.87 × 104
6.00 × 105 0.0107 3.44 × 104
7.00 × 105 0.0125 4.02 × 104
8.00 × 105 0.0143 4.59 × 104
9.00 × 105 0.0161 5.16 × 104
1.00 × 106 0.0179 5.74 × 104
2.00 × 106 0.0357 1.15 × 105
3.00 × 106 0.0536 1.72 × 105
4.00 × 106 0.0714 2.29 × 105
5.00 × 106 0.0893 2.87 × 105
5.18 × 106 0.0925 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 1.34 × 10-5 15.5
100 1.38 × 10-5 15.9
200 2.76 × 10-5 31.9
300 4.13 × 10-5 47.8
400 5.51 × 10-5 63.7
500 6.89 × 10-5 79.7
600 8.27 × 10-5 95.6
700 9.64 × 10-5 112
800 1.10 × 10-4 127
900 1.24 × 10-4 143
1000 1.38 × 10-4 159
2000 2.76 × 10-4 319
3000 4.13 × 10-4 478
4000 5.51 × 10-4 637
5000 6.89 × 10-4 797
6000 8.27 × 10-4 956
7000 9.64 × 10-4 1120
8000 0.00110 1270
9000 0.00124 1430
1.00 × 104 0.00138 1590
2.00 × 104 0.00276 3190
3.00 × 104 0.00413 4780
4.00 × 104 0.00551 6370
5.00 × 104 0.00689 7970
6.00 × 104 0.00827 9560
7.00 × 104 0.00964 1.12 × 104
8.00 × 104 0.0110 1.27 × 104
9.00 × 104 0.0124 1.43 × 104
1.00 × 105 0.0138 1.59 × 104
2.00 × 105 0.0276 3.19 × 104
3.00 × 105 0.0413 4.78 × 104
4.00 × 105 0.0551 6.37 × 104
5.00 × 105 0.0689 7.97 × 104
6.00 × 105 0.0827 9.56 × 104
7.00 × 105 0.0964 1.12 × 105
8.00 × 105 0.110 1.27 × 105
9.00 × 105 0.124 1.43 × 105
1.00 × 106 0.138 1.59 × 105
1.86 × 106 0.257 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 2.14 × 10-4 61.8
100 2.20 × 10-4 63.7
200 4.41 × 10-4 127
300 6.61 × 10-4 191
400 8.82 × 10-4 255
500 0.00110 319
600 0.00132 382
700 0.00154 446
800 0.00176 510
900 0.00198 574
1000 0.00220 637
2000 0.00441 1270
3000 0.00661 1910
4000 0.00882 2550
5000 0.0110 3190
6000 0.0132 3820
7000 0.0154 4460
8000 0.0176 5100
9000 0.0198 5740
1.00 × 104 0.0220 6370
2.00 × 104 0.0441 1.27 × 104
3.00 × 104 0.0661 1.91 × 104
4.00 × 104 0.0882 2.55 × 104
5.00 × 104 0.110 3.19 × 104
6.00 × 104 0.132 3.82 × 104
7.00 × 104 0.154 4.46 × 104
8.00 × 104 0.176 5.10 × 104
9.00 × 104 0.198 5.74 × 104
1.00 × 105 0.220 6.37 × 104
2.00 × 105 0.441 1.27 × 105
3.00 × 105 0.661 1.91 × 105
4.00 × 105 0.882 2.55 × 105
4.66 × 105 1.03 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.00108 139
100 0.00112 143
200 0.00223 287
300 0.00335 430
400 0.00446 574
500 0.00558 717
600 0.00670 860
700 0.00781 1000
800 0.00893 1150
900 0.0100 1290
1000 0.0112 1430
2000 0.0223 2870
3000 0.0335 4300
4000 0.0446 5740
5000 0.0558 7170
6000 0.0670 8600
7000 0.0781 1.00 × 104
8000 0.0893 1.15 × 104
9000 0.100 1.29 × 104
1.00 × 104 0.112 1.43 × 104
2.00 × 104 0.223 2.87 × 104
3.00 × 104 0.335 4.30 × 104
4.00 × 104 0.446 5.74 × 104
5.00 × 104 0.558 7.17 × 104
6.00 × 104 0.670 8.60 × 104
7.00 × 104 0.781 1.00 × 105
8.00 × 104 0.893 1.15 × 105
9.00 × 104 1.00 1.29 × 105
1.00 × 105 1.12 1.43 × 105
2.00 × 105 2.23 2.87 × 105
2.07 × 105 2.31 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.00342 247
100 0.00353 255
200 0.00705 510
300 0.0106 765
400 0.0141 1020
500 0.0176 1270
600 0.0212 1530
700 0.0247 1780
800 0.0282 2040
900 0.0317 2290
1000 0.0353 2550
2000 0.0705 5100
3000 0.106 7650
4000 0.141 1.02 × 104
5000 0.176 1.27 × 104
6000 0.212 1.53 × 104
7000 0.247 1.78 × 104
8000 0.282 2.04 × 104
9000 0.317 2.29 × 104
1.00 × 104 0.353 2.55 × 104
2.00 × 104 0.705 5.10 × 104
3.00 × 104 1.06 7.65 × 104
4.00 × 104 1.41 1.02 × 105
5.00 × 104 1.76 1.27 × 105
6.00 × 104 2.12 1.53 × 105
7.00 × 104 2.47 1.78 × 105
8.00 × 104 2.82 2.04 × 105
9.00 × 104 3.17 2.29 × 105
1.00 × 105 3.53 2.55 × 105
1.17 × 105 4.11 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.00835 386
100 0.00861 398
200 0.0172 797
300 0.0258 1200
400 0.0344 1590
500 0.0431 1990
600 0.0517 2390
700 0.0603 2790
800 0.0689 3190
900 0.0775 3590
1000 0.0861 3980
2000 0.172 7970
3000 0.258 1.20 × 104
4000 0.344 1.59 × 104
5000 0.431 1.99 × 104
6000 0.517 2.39 × 104
7000 0.603 2.79 × 104
8000 0.689 3.19 × 104
9000 0.775 3.59 × 104
1.00 × 104 0.861 3.98 × 104
2.00 × 104 1.72 7.97 × 104
3.00 × 104 2.58 1.20 × 105
4.00 × 104 3.44 1.59 × 105
5.00 × 104 4.31 1.99 × 105
6.00 × 104 5.17 2.39 × 105
7.00 × 104 6.03 2.79 × 105
7.46 × 104 6.42 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.0173 556
100 0.0179 574
200 0.0357 1150
300 0.0536 1720
400 0.0714 2290
500 0.0893 2870
600 0.107 3440
700 0.125 4020
800 0.143 4590
900 0.161 5160
1000 0.179 5740
2000 0.357 1.15 × 104
3000 0.536 1.72 × 104
4000 0.714 2.29 × 104
5000 0.893 2.87 × 104
6000 1.07 3.44 × 104
7000 1.25 4.02 × 104
8000 1.43 4.59 × 104
9000 1.61 5.16 × 104
1.00 × 104 1.79 5.74 × 104
2.00 × 104 3.57 1.15 × 105
3.00 × 104 5.36 1.72 × 105
4.00 × 104 7.14 2.29 × 105
5.00 × 104 8.93 2.87 × 105
5.18 × 104 9.25 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.0547 989
100 0.0564 1020
200 0.113 2040
300 0.169 3060
400 0.226 4080
500 0.282 5100
600 0.339 6120
700 0.395 7140
800 0.451 8160
900 0.508 9180
1000 0.564 1.02 × 104
2000 1.13 2.04 × 104
3000 1.69 3.06 × 104
4000 2.26 4.08 × 104
5000 2.82 5.10 × 104
6000 3.39 6.12 × 104
7000 3.95 7.14 × 104
8000 4.51 8.16 × 104
9000 5.08 9.18 × 104
1.00 × 104 5.64 1.02 × 105
2.00 × 104 11.3 2.04 × 105
2.91 × 104 16.4 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.134 1550
100 0.138 1590
200 0.276 3190
300 0.413 4780
400 0.551 6370
500 0.689 7970
600 0.827 9560
700 0.964 1.12 × 104
800 1.10 1.27 × 104
900 1.24 1.43 × 104
1000 1.38 1.59 × 104
2000 2.76 3.19 × 104
3000 4.13 4.78 × 104
4000 5.51 6.37 × 104
5000 6.89 7.97 × 104
6000 8.27 9.56 × 104
7000 9.64 1.12 × 105
8000 11.0 1.27 × 105
9000 12.4 1.43 × 105
1.00 × 104 13.8 1.59 × 105
1.86 × 104 25.7 2.97 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.277 2230
100 0.286 2290
200 0.571 4590
300 0.857 6880
400 1.14 9180
500 1.43 1.15 × 104
600 1.71 1.38 × 104
700 2.00 1.61 × 104
800 2.29 1.84 × 104
900 2.57 2.07 × 104
1000 2.86 2.29 × 104
2000 5.71 4.59 × 104
3000 8.57 6.88 × 104
4000 11.4 9.18 × 104
5000 14.3 1.15 × 105
6000 17.1 1.38 × 105
6510 18.6 1.49 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.513 3030
100 0.529 3120
200 1.06 6250
300 1.59 9370
400 2.12 1.25 × 104
500 2.65 1.56 × 104
600 3.18 1.87 × 104
700 3.71 2.19 × 104
800 4.23 2.50 × 104
900 4.76 2.81 × 104
1000 5.29 3.12 × 104
2000 10.6 6.25 × 104
3000 15.9 9.37 × 104
3510 18.6 1.10 × 105
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 0.876 3960
100 0.903 4080
200 1.81 8160
300 2.71 1.22 × 104
400 3.61 1.63 × 104
500 4.51 2.04 × 104
600 5.42 2.45 × 104
700 6.32 2.86 × 104
800 7.22 3.26 × 104
900 8.13 3.67 × 104
1000 9.03 4.08 × 104
2000 18.1 8.16 × 104
2060 18.6 8.40 × 104
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 1.40 5010
100 1.45 5160
200 2.89 1.03 × 104
300 4.34 1.55 × 104
400 5.79 2.07 × 104
500 7.23 2.58 × 104
600 8.68 3.10 × 104
700 10.1 3.61 × 104
800 11.6 4.13 × 104
900 13.0 4.65 × 104
1000 14.5 5.16 × 104
1290 18.6 6.64 × 104
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 2.14 6180
100 2.20 6370
200 4.41 1.27 × 104
300 6.61 1.91 × 104
400 8.82 2.55 × 104
500 11.0 3.19 × 104
600 13.2 3.82 × 104
700 15.4 4.46 × 104
800 17.6 5.10 × 104
843 18.6 5.37 × 104
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 5.22 9660
100 5.38 9960
200 10.8 1.99 × 104
300 16.1 2.99 × 104
345 18.6 3.44 × 104
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
97.0 10.8 1.39 × 104
100 11.2 1.43 × 104
167 18.6 2.39 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.