engineering fundamentals
Wide Flange Steel I Beam: W12 × 79
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W12 × 79
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 662 in4) for the W12 × 79 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
  
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 2.86 × 10-6 9.97
80.0 2.89 × 10-6 10.1
90.0 3.25 × 10-6 11.4
100 3.62 × 10-6 12.6
200 7.23 × 10-6 25.2
300 1.08 × 10-5 37.9
400 1.45 × 10-5 50.5
500 1.81 × 10-5 63.1
600 2.17 × 10-5 75.7
700 2.53 × 10-5 88.4
800 2.89 × 10-5 101
900 3.25 × 10-5 114
1000 3.62 × 10-5 126
2000 7.23 × 10-5 252
3000 1.08 × 10-4 379
4000 1.45 × 10-4 505
5000 1.81 × 10-4 631
6000 2.17 × 10-4 757
7000 2.53 × 10-4 884
8000 2.89 × 10-4 1010
9000 3.25 × 10-4 1140
1.00 × 104 3.62 × 10-4 1260
2.00 × 104 7.23 × 10-4 2520
3.00 × 104 0.00108 3790
4.00 × 104 0.00145 5050
5.00 × 104 0.00181 6310
6.00 × 104 0.00217 7570
7.00 × 104 0.00253 8840
8.00 × 104 0.00289 1.01 × 104
9.00 × 104 0.00325 1.14 × 104
1.00 × 105 0.00362 1.26 × 104
2.00 × 105 0.00723 2.52 × 104
3.00 × 105 0.0108 3.79 × 104
4.00 × 105 0.0145 5.05 × 104
5.00 × 105 0.0181 6.31 × 104
6.00 × 105 0.0217 7.57 × 104
7.00 × 105 0.0253 8.84 × 104
8.00 × 105 0.0289 1.01 × 105
9.00 × 105 0.0325 1.14 × 105
1.00 × 106 0.0362 1.26 × 105
2.00 × 106 0.0723 2.52 × 105
2.35 × 106 0.0851 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 2.20 × 10-5 27.7
80.0 2.23 × 10-5 28.1
90.0 2.51 × 10-5 31.6
100 2.79 × 10-5 35.1
200 5.58 × 10-5 70.1
300 8.37 × 10-5 105
400 1.12 × 10-4 140
500 1.39 × 10-4 175
600 1.67 × 10-4 210
700 1.95 × 10-4 245
800 2.23 × 10-4 281
900 2.51 × 10-4 316
1000 2.79 × 10-4 351
2000 5.58 × 10-4 701
3000 8.37 × 10-4 1050
4000 0.00112 1400
5000 0.00139 1750
6000 0.00167 2100
7000 0.00195 2450
8000 0.00223 2810
9000 0.00251 3160
1.00 × 104 0.00279 3510
2.00 × 104 0.00558 7010
3.00 × 104 0.00837 1.05 × 104
4.00 × 104 0.0112 1.40 × 104
5.00 × 104 0.0139 1.75 × 104
6.00 × 104 0.0167 2.10 × 104
7.00 × 104 0.0195 2.45 × 104
8.00 × 104 0.0223 2.81 × 104
9.00 × 104 0.0251 3.16 × 104
1.00 × 105 0.0279 3.51 × 104
2.00 × 105 0.0558 7.01 × 104
3.00 × 105 0.0837 1.05 × 105
4.00 × 105 0.112 1.40 × 105
5.00 × 105 0.139 1.75 × 105
6.00 × 105 0.167 2.10 × 105
7.00 × 105 0.195 2.45 × 105
8.00 × 105 0.223 2.81 × 105
8.47 × 105 0.236 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 3.53 × 10-4 111
80.0 3.57 × 10-4 112
90.0 4.02 × 10-4 126
100 4.46 × 10-4 140
200 8.93 × 10-4 281
300 0.00134 421
400 0.00179 561
500 0.00223 701
600 0.00268 842
700 0.00312 982
800 0.00357 1120
900 0.00402 1260
1000 0.00446 1400
2000 0.00893 2810
3000 0.0134 4210
4000 0.0179 5610
5000 0.0223 7010
6000 0.0268 8420
7000 0.0312 9820
8000 0.0357 1.12 × 104
9000 0.0402 1.26 × 104
1.00 × 104 0.0446 1.40 × 104
2.00 × 104 0.0893 2.81 × 104
3.00 × 104 0.134 4.21 × 104
4.00 × 104 0.179 5.61 × 104
5.00 × 104 0.223 7.01 × 104
6.00 × 104 0.268 8.42 × 104
7.00 × 104 0.312 9.82 × 104
8.00 × 104 0.357 1.12 × 105
9.00 × 104 0.402 1.26 × 105
1.00 × 105 0.446 1.40 × 105
2.00 × 105 0.893 2.81 × 105
2.12 × 105 0.945 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.00179 249
80.0 0.00181 252
90.0 0.00203 284
100 0.00226 316
200 0.00452 631
300 0.00678 947
400 0.00904 1260
500 0.0113 1580
600 0.0136 1890
700 0.0158 2210
800 0.0181 2520
900 0.0203 2840
1000 0.0226 3160
2000 0.0452 6310
3000 0.0678 9470
4000 0.0904 1.26 × 104
5000 0.113 1.58 × 104
6000 0.136 1.89 × 104
7000 0.158 2.21 × 104
8000 0.181 2.52 × 104
9000 0.203 2.84 × 104
1.00 × 104 0.226 3.16 × 104
2.00 × 104 0.452 6.31 × 104
3.00 × 104 0.678 9.47 × 104
4.00 × 104 0.904 1.26 × 105
5.00 × 104 1.13 1.58 × 105
6.00 × 104 1.36 1.89 × 105
7.00 × 104 1.58 2.21 × 105
8.00 × 104 1.81 2.52 × 105
9.00 × 104 2.03 2.84 × 105
9.41 × 104 2.13 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.00564 443
80.0 0.00571 449
90.0 0.00643 505
100 0.00714 561
200 0.0143 1120
300 0.0214 1680
400 0.0286 2240
500 0.0357 2810
600 0.0429 3370
700 0.0500 3930
800 0.0571 4490
900 0.0643 5050
1000 0.0714 5610
2000 0.143 1.12 × 104
3000 0.214 1.68 × 104
4000 0.286 2.24 × 104
5000 0.357 2.81 × 104
6000 0.429 3.37 × 104
7000 0.500 3.93 × 104
8000 0.571 4.49 × 104
9000 0.643 5.05 × 104
1.00 × 104 0.714 5.61 × 104
2.00 × 104 1.43 1.12 × 105
3.00 × 104 2.14 1.68 × 105
4.00 × 104 2.86 2.24 × 105
5.00 × 104 3.57 2.81 × 105
5.29 × 104 3.78 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.0138 693
80.0 0.0139 701
90.0 0.0157 789
100 0.0174 877
200 0.0349 1750
300 0.0523 2630
400 0.0697 3510
500 0.0872 4380
600 0.105 5260
700 0.122 6140
800 0.139 7010
900 0.157 7890
1000 0.174 8770
2000 0.349 1.75 × 104
3000 0.523 2.63 × 104
4000 0.697 3.51 × 104
5000 0.872 4.38 × 104
6000 1.05 5.26 × 104
7000 1.22 6.14 × 104
8000 1.39 7.01 × 104
9000 1.57 7.89 × 104
1.00 × 104 1.74 8.77 × 104
2.00 × 104 3.49 1.75 × 105
3.00 × 104 5.23 2.63 × 105
3.39 × 104 5.91 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.0286 997
80.0 0.0289 1010
90.0 0.0325 1140
100 0.0362 1260
200 0.0723 2520
300 0.108 3790
400 0.145 5050
500 0.181 6310
600 0.217 7570
700 0.253 8840
800 0.289 1.01 × 104
900 0.325 1.14 × 104
1000 0.362 1.26 × 104
2000 0.723 2.52 × 104
3000 1.08 3.79 × 104
4000 1.45 5.05 × 104
5000 1.81 6.31 × 104
6000 2.17 7.57 × 104
7000 2.53 8.84 × 104
8000 2.89 1.01 × 105
9000 3.25 1.14 × 105
1.00 × 104 3.62 1.26 × 105
2.00 × 104 7.23 2.52 × 105
2.35 × 104 8.51 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.0903 1770
80.0 0.0914 1800
90.0 0.103 2020
100 0.114 2240
200 0.229 4490
300 0.343 6730
400 0.457 8980
500 0.571 1.12 × 104
600 0.686 1.35 × 104
700 0.800 1.57 × 104
800 0.914 1.80 × 104
900 1.03 2.02 × 104
1000 1.14 2.24 × 104
2000 2.29 4.49 × 104
3000 3.43 6.73 × 104
4000 4.57 8.98 × 104
5000 5.71 1.12 × 105
6000 6.86 1.35 × 105
7000 8.00 1.57 × 105
8000 9.14 1.80 × 105
9000 10.3 2.02 × 105
1.00 × 104 11.4 2.24 × 105
1.32 × 104 15.1 2.97 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.220 2770
80.0 0.223 2810
90.0 0.251 3160
100 0.279 3510
200 0.558 7010
300 0.837 1.05 × 104
400 1.12 1.40 × 104
500 1.39 1.75 × 104
600 1.67 2.10 × 104
700 1.95 2.45 × 104
800 2.23 2.81 × 104
900 2.51 3.16 × 104
1000 2.79 3.51 × 104
2000 5.58 7.01 × 104
3000 8.37 1.05 × 105
4000 11.2 1.40 × 105
4440 12.4 1.56 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.457 3990
80.0 0.463 4040
90.0 0.521 4540
100 0.578 5050
200 1.16 1.01 × 104
300 1.74 1.51 × 104
400 2.31 2.02 × 104
500 2.89 2.52 × 104
600 3.47 3.03 × 104
700 4.05 3.53 × 104
800 4.63 4.04 × 104
900 5.21 4.54 × 104
1000 5.78 5.05 × 104
2000 11.6 1.01 × 105
2140 12.4 1.08 × 105
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 0.847 5430
80.0 0.857 5500
90.0 0.965 6190
100 1.07 6870
200 2.14 1.37 × 104
300 3.22 2.06 × 104
400 4.29 2.75 × 104
500 5.36 3.44 × 104
600 6.43 4.12 × 104
700 7.50 4.81 × 104
800 8.57 5.50 × 104
900 9.65 6.19 × 104
1000 10.7 6.87 × 104
1160 12.4 7.94 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 1.44 7090
80.0 1.46 7180
90.0 1.65 8080
100 1.83 8980
200 3.66 1.80 × 104
300 5.48 2.69 × 104
400 7.31 3.59 × 104
500 9.14 4.49 × 104
600 11.0 5.39 × 104
677 12.4 6.08 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 2.31 8980
80.0 2.34 9090
90.0 2.64 1.02 × 104
100 2.93 1.14 × 104
200 5.86 2.27 × 104
300 8.79 3.41 × 104
400 11.7 4.54 × 104
423 12.4 4.80 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 3.53 1.11 × 104
80.0 3.57 1.12 × 104
90.0 4.02 1.26 × 104
100 4.46 1.40 × 104
200 8.93 2.81 × 104
277 12.4 3.89 × 104
Steel I Beam: W12 × 79 (Wide Flange 12 inch tall × 79 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
79.0 8.61 1.73 × 104
80.0 8.72 1.75 × 104
90.0 9.81 1.97 × 104
100 10.9 2.19 × 104
114 12.4 2.49 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.