engineering fundamentals
Wide Flange Steel I Beam: W14 × 159
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W14 × 159
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 1900 in4) for the W14 × 159 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 2.00 × 10-6 8.46
200 2.52 × 10-6 10.6
300 3.78 × 10-6 16.0
400 5.04 × 10-6 21.3
500 6.30 × 10-6 26.6
600 7.56 × 10-6 31.9
700 8.82 × 10-6 37.3
800 1.01 × 10-5 42.6
900 1.13 × 10-5 47.9
1000 1.26 × 10-5 53.2
2000 2.52 × 10-5 106
3000 3.78 × 10-5 160
4000 5.04 × 10-5 213
5000 6.30 × 10-5 266
6000 7.56 × 10-5 319
7000 8.82 × 10-5 373
8000 1.01 × 10-4 426
9000 1.13 × 10-4 479
1.00 × 104 1.26 × 10-4 532
2.00 × 104 2.52 × 10-4 1060
3.00 × 104 3.78 × 10-4 1600
4.00 × 104 5.04 × 10-4 2130
5.00 × 104 6.30 × 10-4 2660
6.00 × 104 7.56 × 10-4 3190
7.00 × 104 8.82 × 10-4 3730
8.00 × 104 0.00101 4260
9.00 × 104 0.00113 4790
1.00 × 105 0.00126 5320
2.00 × 105 0.00252 1.06 × 104
3.00 × 105 0.00378 1.60 × 104
4.00 × 105 0.00504 2.13 × 104
5.00 × 105 0.00630 2.66 × 104
6.00 × 105 0.00756 3.19 × 104
7.00 × 105 0.00882 3.73 × 104
8.00 × 105 0.0101 4.26 × 104
9.00 × 105 0.0113 4.79 × 104
1.00 × 106 0.0126 5.32 × 104
2.00 × 106 0.0252 1.06 × 105
3.00 × 106 0.0378 1.60 × 105
4.00 × 106 0.0504 2.13 × 105
5.00 × 106 0.0630 2.66 × 105
5.58 × 106 0.0703 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 1.55 × 10-5 23.5
200 1.94 × 10-5 29.6
300 2.92 × 10-5 44.3
400 3.89 × 10-5 59.1
500 4.86 × 10-5 73.9
600 5.83 × 10-5 88.7
700 6.80 × 10-5 103
800 7.78 × 10-5 118
900 8.75 × 10-5 133
1000 9.72 × 10-5 148
2000 1.94 × 10-4 296
3000 2.92 × 10-4 443
4000 3.89 × 10-4 591
5000 4.86 × 10-4 739
6000 5.83 × 10-4 887
7000 6.80 × 10-4 1030
8000 7.78 × 10-4 1180
9000 8.75 × 10-4 1330
1.00 × 104 9.72 × 10-4 1480
2.00 × 104 0.00194 2960
3.00 × 104 0.00292 4430
4.00 × 104 0.00389 5910
5.00 × 104 0.00486 7390
6.00 × 104 0.00583 8870
7.00 × 104 0.00680 1.03 × 104
8.00 × 104 0.00778 1.18 × 104
9.00 × 104 0.00875 1.33 × 104
1.00 × 105 0.00972 1.48 × 104
2.00 × 105 0.0194 2.96 × 104
3.00 × 105 0.0292 4.43 × 104
4.00 × 105 0.0389 5.91 × 104
5.00 × 105 0.0486 7.39 × 104
6.00 × 105 0.0583 8.87 × 104
7.00 × 105 0.0680 1.03 × 105
8.00 × 105 0.0778 1.18 × 105
9.00 × 105 0.0875 1.33 × 105
1.00 × 106 0.0972 1.48 × 105
2.00 × 106 0.194 2.96 × 105
2.01 × 106 0.195 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 2.47 × 10-4 94.0
200 3.11 × 10-4 118
300 4.67 × 10-4 177
400 6.22 × 10-4 237
500 7.78 × 10-4 296
600 9.33 × 10-4 355
700 0.00109 414
800 0.00124 473
900 0.00140 532
1000 0.00156 591
2000 0.00311 1180
3000 0.00467 1770
4000 0.00622 2370
5000 0.00778 2960
6000 0.00933 3550
7000 0.0109 4140
8000 0.0124 4730
9000 0.0140 5320
1.00 × 104 0.0156 5910
2.00 × 104 0.0311 1.18 × 104
3.00 × 104 0.0467 1.77 × 104
4.00 × 104 0.0622 2.37 × 104
5.00 × 104 0.0778 2.96 × 104
6.00 × 104 0.0933 3.55 × 104
7.00 × 104 0.109 4.14 × 104
8.00 × 104 0.124 4.73 × 104
9.00 × 104 0.140 5.32 × 104
1.00 × 105 0.156 5.91 × 104
2.00 × 105 0.311 1.18 × 105
3.00 × 105 0.467 1.77 × 105
4.00 × 105 0.622 2.37 × 105
5.00 × 105 0.778 2.96 × 105
5.02 × 105 0.781 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.00125 212
200 0.00157 266
300 0.00236 399
400 0.00315 532
500 0.00394 665
600 0.00472 798
700 0.00551 931
800 0.00630 1060
900 0.00709 1200
1000 0.00787 1330
2000 0.0157 2660
3000 0.0236 3990
4000 0.0315 5320
5000 0.0394 6650
6000 0.0472 7980
7000 0.0551 9310
8000 0.0630 1.06 × 104
9000 0.0709 1.20 × 104
1.00 × 104 0.0787 1.33 × 104
2.00 × 104 0.157 2.66 × 104
3.00 × 104 0.236 3.99 × 104
4.00 × 104 0.315 5.32 × 104
5.00 × 104 0.394 6.65 × 104
6.00 × 104 0.472 7.98 × 104
7.00 × 104 0.551 9.31 × 104
8.00 × 104 0.630 1.06 × 105
9.00 × 104 0.709 1.20 × 105
1.00 × 105 0.787 1.33 × 105
2.00 × 105 1.57 2.66 × 105
2.23 × 105 1.76 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.00396 376
200 0.00498 473
300 0.00746 710
400 0.00995 946
500 0.0124 1180
600 0.0149 1420
700 0.0174 1660
800 0.0199 1890
900 0.0224 2130
1000 0.0249 2370
2000 0.0498 4730
3000 0.0746 7100
4000 0.0995 9460
5000 0.124 1.18 × 104
6000 0.149 1.42 × 104
7000 0.174 1.66 × 104
8000 0.199 1.89 × 104
9000 0.224 2.13 × 104
1.00 × 104 0.249 2.37 × 104
2.00 × 104 0.498 4.73 × 104
3.00 × 104 0.746 7.10 × 104
4.00 × 104 0.995 9.46 × 104
5.00 × 104 1.24 1.18 × 105
6.00 × 104 1.49 1.42 × 105
7.00 × 104 1.74 1.66 × 105
8.00 × 104 1.99 1.89 × 105
9.00 × 104 2.24 2.13 × 105
1.00 × 105 2.49 2.37 × 105
1.26 × 105 3.12 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.00966 588
200 0.0122 739
300 0.0182 1110
400 0.0243 1480
500 0.0304 1850
600 0.0365 2220
700 0.0425 2590
800 0.0486 2960
900 0.0547 3330
1000 0.0608 3700
2000 0.122 7390
3000 0.182 1.11 × 104
4000 0.243 1.48 × 104
5000 0.304 1.85 × 104
6000 0.365 2.22 × 104
7000 0.425 2.59 × 104
8000 0.486 2.96 × 104
9000 0.547 3.33 × 104
1.00 × 104 0.608 3.70 × 104
2.00 × 104 1.22 7.39 × 104
3.00 × 104 1.82 1.11 × 105
4.00 × 104 2.43 1.48 × 105
5.00 × 104 3.04 1.85 × 105
6.00 × 104 3.65 2.22 × 105
7.00 × 104 4.25 2.59 × 105
8.00 × 104 4.86 2.96 × 105
8.04 × 104 4.88 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.0200 846
200 0.0252 1060
300 0.0378 1600
400 0.0504 2130
500 0.0630 2660
600 0.0756 3190
700 0.0882 3730
800 0.101 4260
900 0.113 4790
1000 0.126 5320
2000 0.252 1.06 × 104
3000 0.378 1.60 × 104
4000 0.504 2.13 × 104
5000 0.630 2.66 × 104
6000 0.756 3.19 × 104
7000 0.882 3.73 × 104
8000 1.01 4.26 × 104
9000 1.13 4.79 × 104
1.00 × 104 1.26 5.32 × 104
2.00 × 104 2.52 1.06 × 105
3.00 × 104 3.78 1.60 × 105
4.00 × 104 5.04 2.13 × 105
5.00 × 104 6.30 2.66 × 105
5.58 × 104 7.03 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.0633 1500
200 0.0796 1890
300 0.119 2840
400 0.159 3780
500 0.199 4730
600 0.239 5680
700 0.279 6620
800 0.319 7570
900 0.358 8510
1000 0.398 9460
2000 0.796 1.89 × 104
3000 1.19 2.84 × 104
4000 1.59 3.78 × 104
5000 1.99 4.73 × 104
6000 2.39 5.68 × 104
7000 2.79 6.62 × 104
8000 3.19 7.57 × 104
9000 3.58 8.51 × 104
1.00 × 104 3.98 9.46 × 104
2.00 × 104 7.96 1.89 × 105
3.00 × 104 11.9 2.84 × 105
3.14 × 104 12.5 2.97 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.155 2350
200 0.194 2960
300 0.292 4430
400 0.389 5910
500 0.486 7390
600 0.583 8870
700 0.680 1.03 × 104
800 0.778 1.18 × 104
900 0.875 1.33 × 104
1000 0.972 1.48 × 104
2000 1.94 2.96 × 104
3000 2.92 4.43 × 104
4000 3.89 5.91 × 104
5000 4.86 7.39 × 104
6000 5.83 8.87 × 104
7000 6.80 1.03 × 105
8000 7.78 1.18 × 105
9000 8.75 1.33 × 105
1.00 × 104 9.72 1.48 × 105
1.54 × 104 15.0 2.28 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.320 3380
200 0.403 4260
300 0.605 6390
400 0.806 8510
500 1.01 1.06 × 104
600 1.21 1.28 × 104
700 1.41 1.49 × 104
800 1.61 1.70 × 104
900 1.81 1.92 × 104
1000 2.02 2.13 × 104
2000 4.03 4.26 × 104
3000 6.05 6.39 × 104
4000 8.06 8.51 × 104
5000 10.1 1.06 × 105
6000 12.1 1.28 × 105
7000 14.1 1.49 × 105
7430 15.0 1.58 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 0.594 4610
200 0.747 5790
300 1.12 8690
400 1.49 1.16 × 104
500 1.87 1.45 × 104
600 2.24 1.74 × 104
700 2.61 2.03 × 104
800 2.99 2.32 × 104
900 3.36 2.61 × 104
1000 3.73 2.90 × 104
2000 7.47 5.79 × 104
3000 11.2 8.69 × 104
4000 14.9 1.16 × 105
4010 15.0 1.16 × 105
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 1.01 6020
200 1.27 7570
300 1.91 1.14 × 104
400 2.55 1.51 × 104
500 3.19 1.89 × 104
600 3.82 2.27 × 104
700 4.46 2.65 × 104
800 5.10 3.03 × 104
900 5.73 3.41 × 104
1000 6.37 3.78 × 104
2000 12.7 7.57 × 104
2350 15.0 8.90 × 104
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 1.62 7620
200 2.04 9580
300 3.06 1.44 × 104
400 4.08 1.92 × 104
500 5.10 2.39 × 104
600 6.12 2.87 × 104
700 7.14 3.35 × 104
800 8.16 3.83 × 104
900 9.18 4.31 × 104
1000 10.2 4.79 × 104
1470 15.0 7.03 × 104
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 2.47 9400
200 3.11 1.18 × 104
300 4.67 1.77 × 104
400 6.22 2.37 × 104
500 7.78 2.96 × 104
600 9.33 3.55 × 104
700 10.9 4.14 × 104
800 12.4 4.73 × 104
900 14.0 5.32 × 104
963 15.0 5.70 × 104
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 6.04 1.47 × 104
200 7.59 1.85 × 104
300 11.4 2.77 × 104
395 15.0 3.65 × 104
Steel I Beam: W14 × 159 (Wide Flange 14 inch tall × 159 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
159 12.5 2.12 × 104
190 15.0 2.53 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.