For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 758 in4) for the W16 × 57 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 1.80 × 10-6 8.34
60.0 1.89 × 10-6 8.78
70.0 2.21 × 10-6 10.2
80.0 2.53 × 10-6 11.7
90.0 2.84 × 10-6 13.2
100 3.16 × 10-6 14.6
200 6.32 × 10-6 29.3
300 9.47 × 10-6 43.9
400 1.26 × 10-5 58.5
500 1.58 × 10-5 73.2
600 1.89 × 10-5 87.8
700 2.21 × 10-5 102
800 2.53 × 10-5 117
900 2.84 × 10-5 132
1000 3.16 × 10-5 146
2000 6.32 × 10-5 293
3000 9.47 × 10-5 439
4000 1.26 × 10-4 585
5000 1.58 × 10-4 732
6000 1.89 × 10-4 878
7000 2.21 × 10-4 1020
8000 2.53 × 10-4 1170
9000 2.84 × 10-4 1320
1.00 × 104 3.16 × 10-4 1460
2.00 × 104 6.32 × 10-4 2930
3.00 × 104 9.47 × 10-4 4390
4.00 × 104 0.00126 5850
5.00 × 104 0.00158 7320
6.00 × 104 0.00189 8780
7.00 × 104 0.00221 1.02 × 104
8.00 × 104 0.00253 1.17 × 104
9.00 × 104 0.00284 1.32 × 104
1.00 × 105 0.00316 1.46 × 104
2.00 × 105 0.00632 2.93 × 104
3.00 × 105 0.00947 4.39 × 104
4.00 × 105 0.0126 5.85 × 104
5.00 × 105 0.0158 7.32 × 104
6.00 × 105 0.0189 8.78 × 104
7.00 × 105 0.0221 1.02 × 105
8.00 × 105 0.0253 1.17 × 105
9.00 × 105 0.0284 1.32 × 105
1.00 × 106 0.0316 1.46 × 105
2.00 × 106 0.0632 2.93 × 105
2.03 × 106 0.0641 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 1.39 × 10-5 23.2
60.0 1.46 × 10-5 24.4
70.0 1.71 × 10-5 28.4
80.0 1.95 × 10-5 32.5
90.0 2.19 × 10-5 36.6
100 2.44 × 10-5 40.6
200 4.87 × 10-5 81.3
300 7.31 × 10-5 122
400 9.75 × 10-5 163
500 1.22 × 10-4 203
600 1.46 × 10-4 244
700 1.71 × 10-4 284
800 1.95 × 10-4 325
900 2.19 × 10-4 366
1000 2.44 × 10-4 406
2000 4.87 × 10-4 813
3000 7.31 × 10-4 1220
4000 9.75 × 10-4 1630
5000 0.00122 2030
6000 0.00146 2440
7000 0.00171 2840
8000 0.00195 3250
9000 0.00219 3660
1.00 × 104 0.00244 4060
2.00 × 104 0.00487 8130
3.00 × 104 0.00731 1.22 × 104
4.00 × 104 0.00975 1.63 × 104
5.00 × 104 0.0122 2.03 × 104
6.00 × 104 0.0146 2.44 × 104
7.00 × 104 0.0171 2.84 × 104
8.00 × 104 0.0195 3.25 × 104
9.00 × 104 0.0219 3.66 × 104
1.00 × 105 0.0244 4.06 × 104
2.00 × 105 0.0487 8.13 × 104
3.00 × 105 0.0731 1.22 × 105
4.00 × 105 0.0975 1.63 × 105
5.00 × 105 0.122 2.03 × 105
6.00 × 105 0.146 2.44 × 105
7.00 × 105 0.171 2.84 × 105
7.31 × 105 0.178 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 2.22 × 10-4 92.7
60.0 2.34 × 10-4 97.5
70.0 2.73 × 10-4 114
80.0 3.12 × 10-4 130
90.0 3.51 × 10-4 146
100 3.90 × 10-4 163
200 7.80 × 10-4 325
300 0.00117 488
400 0.00156 650
500 0.00195 813
600 0.00234 975
700 0.00273 1140
800 0.00312 1300
900 0.00351 1460
1000 0.00390 1630
2000 0.00780 3250
3000 0.0117 4880
4000 0.0156 6500
5000 0.0195 8130
6000 0.0234 9750
7000 0.0273 1.14 × 104
8000 0.0312 1.30 × 104
9000 0.0351 1.46 × 104
1.00 × 104 0.0390 1.63 × 104
2.00 × 104 0.0780 3.25 × 104
3.00 × 104 0.117 4.88 × 104
4.00 × 104 0.156 6.50 × 104
5.00 × 104 0.195 8.13 × 104
6.00 × 104 0.234 9.75 × 104
7.00 × 104 0.273 1.14 × 105
8.00 × 104 0.312 1.30 × 105
9.00 × 104 0.351 1.46 × 105
1.00 × 105 0.390 1.63 × 105
1.83 × 105 0.712 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.00112 208
60.0 0.00118 219
70.0 0.00138 256
80.0 0.00158 293
90.0 0.00178 329
100 0.00197 366
200 0.00395 732
300 0.00592 1100
400 0.00789 1460
500 0.00987 1830
600 0.0118 2190
700 0.0138 2560
800 0.0158 2930
900 0.0178 3290
1000 0.0197 3660
2000 0.0395 7320
3000 0.0592 1.10 × 104
4000 0.0789 1.46 × 104
5000 0.0987 1.83 × 104
6000 0.118 2.19 × 104
7000 0.138 2.56 × 104
8000 0.158 2.93 × 104
9000 0.178 3.29 × 104
1.00 × 104 0.197 3.66 × 104
2.00 × 104 0.395 7.32 × 104
3.00 × 104 0.592 1.10 × 105
4.00 × 104 0.789 1.46 × 105
5.00 × 104 0.987 1.83 × 105
6.00 × 104 1.18 2.19 × 105
7.00 × 104 1.38 2.56 × 105
8.00 × 104 1.58 2.93 × 105
8.12 × 104 1.60 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.00356 371
60.0 0.00374 390
70.0 0.00437 455
80.0 0.00499 520
90.0 0.00561 585
100 0.00624 650
200 0.0125 1300
300 0.0187 1950
400 0.0249 2600
500 0.0312 3250
600 0.0374 3900
700 0.0437 4550
800 0.0499 5200
900 0.0561 5850
1000 0.0624 6500
2000 0.125 1.30 × 104
3000 0.187 1.95 × 104
4000 0.249 2.60 × 104
5000 0.312 3.25 × 104
6000 0.374 3.90 × 104
7000 0.437 4.55 × 104
8000 0.499 5.20 × 104
9000 0.561 5.85 × 104
1.00 × 104 0.624 6.50 × 104
2.00 × 104 1.25 1.30 × 105
3.00 × 104 1.87 1.95 × 105
4.00 × 104 2.49 2.60 × 105
4.57 × 104 2.85 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.00868 579
60.0 0.00914 610
70.0 0.0107 711
80.0 0.0122 813
90.0 0.0137 914
100 0.0152 1020
200 0.0305 2030
300 0.0457 3050
400 0.0609 4060
500 0.0761 5080
600 0.0914 6100
700 0.107 7110
800 0.122 8130
900 0.137 9140
1000 0.152 1.02 × 104
2000 0.305 2.03 × 104
3000 0.457 3.05 × 104
4000 0.609 4.06 × 104
5000 0.761 5.08 × 104
6000 0.914 6.10 × 104
7000 1.07 7.11 × 104
8000 1.22 8.13 × 104
9000 1.37 9.14 × 104
1.00 × 104 1.52 1.02 × 105
2.00 × 104 3.05 2.03 × 105
2.92 × 104 4.45 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.0180 834
60.0 0.0189 878
70.0 0.0221 1020
80.0 0.0253 1170
90.0 0.0284 1320
100 0.0316 1460
200 0.0632 2930
300 0.0947 4390
400 0.126 5850
500 0.158 7320
600 0.189 8780
700 0.221 1.02 × 104
800 0.253 1.17 × 104
900 0.284 1.32 × 104
1000 0.316 1.46 × 104
2000 0.632 2.93 × 104
3000 0.947 4.39 × 104
4000 1.26 5.85 × 104
5000 1.58 7.32 × 104
6000 1.89 8.78 × 104
7000 2.21 1.02 × 105
8000 2.53 1.17 × 105
9000 2.84 1.32 × 105
1.00 × 104 3.16 1.46 × 105
2.00 × 104 6.32 2.93 × 105
2.03 × 104 6.41 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.0569 1480
60.0 0.0599 1560
70.0 0.0699 1820
80.0 0.0798 2080
90.0 0.0898 2340
100 0.0998 2600
200 0.200 5200
300 0.299 7800
400 0.399 1.04 × 104
500 0.499 1.30 × 104
600 0.599 1.56 × 104
700 0.699 1.82 × 104
800 0.798 2.08 × 104
900 0.898 2.34 × 104
1000 0.998 2.60 × 104
2000 2.00 5.20 × 104
3000 2.99 7.80 × 104
4000 3.99 1.04 × 105
5000 4.99 1.30 × 105
6000 5.99 1.56 × 105
7000 6.99 1.82 × 105
8000 7.98 2.08 × 105
9000 8.98 2.34 × 105
1.00 × 104 9.98 2.60 × 105
1.14 × 104 11.4 2.97 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.139 2320
60.0 0.146 2440
70.0 0.171 2840
80.0 0.195 3250
90.0 0.219 3660
100 0.244 4060
200 0.487 8130
300 0.731 1.22 × 104
400 0.975 1.63 × 104
500 1.22 2.03 × 104
600 1.46 2.44 × 104
700 1.71 2.84 × 104
800 1.95 3.25 × 104
900 2.19 3.66 × 104
1000 2.44 4.06 × 104
2000 4.87 8.13 × 104
3000 7.31 1.22 × 105
4000 9.75 1.63 × 105
5000 12.2 2.03 × 105
6000 14.6 2.44 × 105
6740 16.4 2.74 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.288 3340
60.0 0.303 3510
70.0 0.354 4100
80.0 0.404 4680
90.0 0.455 5270
100 0.505 5850
200 1.01 1.17 × 104
300 1.52 1.76 × 104
400 2.02 2.34 × 104
500 2.53 2.93 × 104
600 3.03 3.51 × 104
700 3.54 4.10 × 104
800 4.04 4.68 × 104
900 4.55 5.27 × 104
1000 5.05 5.85 × 104
2000 10.1 1.17 × 105
3000 15.2 1.76 × 105
3250 16.4 1.90 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.534 4540
60.0 0.562 4780
70.0 0.655 5580
80.0 0.749 6370
90.0 0.842 7170
100 0.936 7970
200 1.87 1.59 × 104
300 2.81 2.39 × 104
400 3.74 3.19 × 104
500 4.68 3.98 × 104
600 5.62 4.78 × 104
700 6.55 5.58 × 104
800 7.49 6.37 × 104
900 8.42 7.17 × 104
1000 9.36 7.97 × 104
1760 16.4 1.40 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 0.910 5930
60.0 0.958 6240
70.0 1.12 7280
80.0 1.28 8320
90.0 1.44 9360
100 1.60 1.04 × 104
200 3.19 2.08 × 104
300 4.79 3.12 × 104
400 6.39 4.16 × 104
500 7.98 5.20 × 104
600 9.58 6.24 × 104
700 11.2 7.28 × 104
800 12.8 8.32 × 104
900 14.4 9.36 × 104
1000 16.0 1.04 × 105
1030 16.4 1.07 × 105
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 1.46 7510
60.0 1.53 7900
70.0 1.79 9220
80.0 2.05 1.05 × 104
90.0 2.30 1.19 × 104
100 2.56 1.32 × 104
200 5.12 2.63 × 104
300 7.67 3.95 × 104
400 10.2 5.27 × 104
500 12.8 6.58 × 104
600 15.3 7.90 × 104
642 16.4 8.46 × 104
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 2.22 9270
60.0 2.34 9750
70.0 2.73 1.14 × 104
80.0 3.12 1.30 × 104
90.0 3.51 1.46 × 104
100 3.90 1.63 × 104
200 7.80 3.25 × 104
300 11.7 4.88 × 104
400 15.6 6.50 × 104
421 16.4 6.85 × 104
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 5.42 1.45 × 104
60.0 5.71 1.52 × 104
70.0 6.66 1.78 × 104
80.0 7.61 2.03 × 104
90.0 8.57 2.29 × 104
100 9.52 2.54 × 104
173 16.4 4.39 × 104
Steel I Beam: W16 × 57 (Wide Flange 16 inch tall × 57 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
57.0 11.2 2.08 × 104
60.0 11.8 2.19 × 104
70.0 13.8 2.56 × 104
80.0 15.8 2.93 × 104
83.3 16.4 3.05 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.