engineering fundamentals
Wide Flange Steel I Beam: W21 × 44
Home | Directory | Career | News | Industrial




Materials

Design

Processes

Units

Formulas

Math
Glossary » Beams » Simply Supported » Uniformly Distributed Load » Two Equal Spans » Wide Flange Steel I Beam » W21 × 44
Wide Flange Steel I Beam | Single Span | Two Equal Spans | Three Equal Spans | Four Equal Spans

For a simply supported beam in two equal spans, we compute the displacement at the middle of each span w_mid and the maximum normal stress stress_max occuring at the center support of the beam.
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 843 in4) for the W21 × 44 Wide Flange Steel I Beam and the typical Young's modulus (E = 3.046 × 107 psi) of steels. Note that the typical yielding stress Yield of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.

Note: The weight of the beam itself is not included in the calculation.
L = 3 ft
L = 5 ft
L = 10 ft
L = 15 ft
L = 20 ft
L = 25 ft
L = 30 ft
L = 40 ft
L = 50 ft
L = 60 ft
L = 70 ft
L = 80 ft
L = 90 ft
L = 100 ft
L = 125 ft
L = 150 ft
  
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 3.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 1.25 × 10-6 7.28
50.0 1.42 × 10-6 8.27
60.0 1.70 × 10-6 9.93
70.0 1.99 × 10-6 11.6
80.0 2.27 × 10-6 13.2
90.0 2.56 × 10-6 14.9
100 2.84 × 10-6 16.5
200 5.68 × 10-6 33.1
300 8.52 × 10-6 49.6
400 1.14 × 10-5 66.2
500 1.42 × 10-5 82.7
600 1.70 × 10-5 99.3
700 1.99 × 10-5 116
800 2.27 × 10-5 132
900 2.56 × 10-5 149
1000 2.84 × 10-5 165
2000 5.68 × 10-5 331
3000 8.52 × 10-5 496
4000 1.14 × 10-4 662
5000 1.42 × 10-4 827
6000 1.70 × 10-4 993
7000 1.99 × 10-4 1160
8000 2.27 × 10-4 1320
9000 2.56 × 10-4 1490
1.00 × 104 2.84 × 10-4 1650
2.00 × 104 5.68 × 10-4 3310
3.00 × 104 8.52 × 10-4 4960
4.00 × 104 0.00114 6620
5.00 × 104 0.00142 8270
6.00 × 104 0.00170 9930
7.00 × 104 0.00199 1.16 × 104
8.00 × 104 0.00227 1.32 × 104
9.00 × 104 0.00256 1.49 × 104
1.00 × 105 0.00284 1.65 × 104
2.00 × 105 0.00568 3.31 × 104
3.00 × 105 0.00852 4.96 × 104
4.00 × 105 0.0114 6.62 × 104
5.00 × 105 0.0142 8.27 × 104
6.00 × 105 0.0170 9.93 × 104
7.00 × 105 0.0199 1.16 × 105
8.00 × 105 0.0227 1.32 × 105
9.00 × 105 0.0256 1.49 × 105
1.00 × 106 0.0284 1.65 × 105
1.80 × 106 0.0510 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 5.00 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 9.64 × 10-6 20.2
50.0 1.10 × 10-5 23.0
60.0 1.31 × 10-5 27.6
70.0 1.53 × 10-5 32.2
80.0 1.75 × 10-5 36.8
90.0 1.97 × 10-5 41.4
100 2.19 × 10-5 46.0
200 4.38 × 10-5 91.9
300 6.57 × 10-5 138
400 8.76 × 10-5 184
500 1.10 × 10-4 230
600 1.31 × 10-4 276
700 1.53 × 10-4 322
800 1.75 × 10-4 368
900 1.97 × 10-4 414
1000 2.19 × 10-4 460
2000 4.38 × 10-4 919
3000 6.57 × 10-4 1380
4000 8.76 × 10-4 1840
5000 0.00110 2300
6000 0.00131 2760
7000 0.00153 3220
8000 0.00175 3680
9000 0.00197 4140
1.00 × 104 0.00219 4600
2.00 × 104 0.00438 9190
3.00 × 104 0.00657 1.38 × 104
4.00 × 104 0.00876 1.84 × 104
5.00 × 104 0.0110 2.30 × 104
6.00 × 104 0.0131 2.76 × 104
7.00 × 104 0.0153 3.22 × 104
8.00 × 104 0.0175 3.68 × 104
9.00 × 104 0.0197 4.14 × 104
1.00 × 105 0.0219 4.60 × 104
2.00 × 105 0.0438 9.19 × 104
3.00 × 105 0.0657 1.38 × 105
4.00 × 105 0.0876 1.84 × 105
5.00 × 105 0.110 2.30 × 105
6.00 × 105 0.131 2.76 × 105
6.46 × 105 0.142 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 10.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 1.54 × 10-4 80.9
50.0 1.75 × 10-4 91.9
60.0 2.10 × 10-4 110
70.0 2.45 × 10-4 129
80.0 2.80 × 10-4 147
90.0 3.15 × 10-4 165
100 3.51 × 10-4 184
200 7.01 × 10-4 368
300 0.00105 551
400 0.00140 735
500 0.00175 919
600 0.00210 1100
700 0.00245 1290
800 0.00280 1470
900 0.00315 1650
1000 0.00351 1840
2000 0.00701 3680
3000 0.0105 5510
4000 0.0140 7350
5000 0.0175 9190
6000 0.0210 1.10 × 104
7000 0.0245 1.29 × 104
8000 0.0280 1.47 × 104
9000 0.0315 1.65 × 104
1.00 × 104 0.0351 1.84 × 104
2.00 × 104 0.0701 3.68 × 104
3.00 × 104 0.105 5.51 × 104
4.00 × 104 0.140 7.35 × 104
5.00 × 104 0.175 9.19 × 104
6.00 × 104 0.210 1.10 × 105
7.00 × 104 0.245 1.29 × 105
8.00 × 104 0.280 1.47 × 105
9.00 × 104 0.315 1.65 × 105
1.00 × 105 0.351 1.84 × 105
1.62 × 105 0.566 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 15.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 7.81 × 10-4 182
50.0 8.87 × 10-4 207
60.0 0.00106 248
70.0 0.00124 289
80.0 0.00142 331
90.0 0.00160 372
100 0.00177 414
200 0.00355 827
300 0.00532 1240
400 0.00710 1650
500 0.00887 2070
600 0.0106 2480
700 0.0124 2890
800 0.0142 3310
900 0.0160 3720
1000 0.0177 4140
2000 0.0355 8270
3000 0.0532 1.24 × 104
4000 0.0710 1.65 × 104
5000 0.0887 2.07 × 104
6000 0.106 2.48 × 104
7000 0.124 2.89 × 104
8000 0.142 3.31 × 104
9000 0.160 3.72 × 104
1.00 × 104 0.177 4.14 × 104
2.00 × 104 0.355 8.27 × 104
3.00 × 104 0.532 1.24 × 105
4.00 × 104 0.710 1.65 × 105
5.00 × 104 0.887 2.07 × 105
6.00 × 104 1.06 2.48 × 105
7.00 × 104 1.24 2.89 × 105
7.18 × 104 1.27 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 20.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.00247 324
50.0 0.00280 368
60.0 0.00337 441
70.0 0.00393 515
80.0 0.00449 588
90.0 0.00505 662
100 0.00561 735
200 0.0112 1470
300 0.0168 2210
400 0.0224 2940
500 0.0280 3680
600 0.0337 4410
700 0.0393 5150
800 0.0449 5880
900 0.0505 6620
1000 0.0561 7350
2000 0.112 1.47 × 104
3000 0.168 2.21 × 104
4000 0.224 2.94 × 104
5000 0.280 3.68 × 104
6000 0.337 4.41 × 104
7000 0.393 5.15 × 104
8000 0.449 5.88 × 104
9000 0.505 6.62 × 104
1.00 × 104 0.561 7.35 × 104
2.00 × 104 1.12 1.47 × 105
3.00 × 104 1.68 2.21 × 105
4.00 × 104 2.24 2.94 × 105
4.04 × 104 2.27 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 25.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.00602 505
50.0 0.00685 574
60.0 0.00822 689
70.0 0.00958 804
80.0 0.0110 919
90.0 0.0123 1030
100 0.0137 1150
200 0.0274 2300
300 0.0411 3450
400 0.0548 4600
500 0.0685 5740
600 0.0822 6890
700 0.0958 8040
800 0.110 9190
900 0.123 1.03 × 104
1000 0.137 1.15 × 104
2000 0.274 2.30 × 104
3000 0.411 3.45 × 104
4000 0.548 4.60 × 104
5000 0.685 5.74 × 104
6000 0.822 6.89 × 104
7000 0.958 8.04 × 104
8000 1.10 9.19 × 104
9000 1.23 1.03 × 105
1.00 × 104 1.37 1.15 × 105
2.00 × 104 2.74 2.30 × 105
2.59 × 104 3.54 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 30.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.0125 728
50.0 0.0142 827
60.0 0.0170 993
70.0 0.0199 1160
80.0 0.0227 1320
90.0 0.0256 1490
100 0.0284 1650
200 0.0568 3310
300 0.0852 4960
400 0.114 6620
500 0.142 8270
600 0.170 9930
700 0.199 1.16 × 104
800 0.227 1.32 × 104
900 0.256 1.49 × 104
1000 0.284 1.65 × 104
2000 0.568 3.31 × 104
3000 0.852 4.96 × 104
4000 1.14 6.62 × 104
5000 1.42 8.27 × 104
6000 1.70 9.93 × 104
7000 1.99 1.16 × 105
8000 2.27 1.32 × 105
9000 2.56 1.49 × 105
1.00 × 104 2.84 1.65 × 105
1.80 × 104 5.10 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 40.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.0395 1290
50.0 0.0449 1470
60.0 0.0538 1760
70.0 0.0628 2060
80.0 0.0718 2350
90.0 0.0808 2650
100 0.0897 2940
200 0.179 5880
300 0.269 8820
400 0.359 1.18 × 104
500 0.449 1.47 × 104
600 0.538 1.76 × 104
700 0.628 2.06 × 104
800 0.718 2.35 × 104
900 0.808 2.65 × 104
1000 0.897 2.94 × 104
2000 1.79 5.88 × 104
3000 2.69 8.82 × 104
4000 3.59 1.18 × 105
5000 4.49 1.47 × 105
6000 5.38 1.76 × 105
7000 6.28 2.06 × 105
8000 7.18 2.35 × 105
9000 8.08 2.65 × 105
1.00 × 104 8.97 2.94 × 105
1.01 × 104 9.06 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 50.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.0964 2020
50.0 0.110 2300
60.0 0.131 2760
70.0 0.153 3220
80.0 0.175 3680
90.0 0.197 4140
100 0.219 4600
200 0.438 9190
300 0.657 1.38 × 104
400 0.876 1.84 × 104
500 1.10 2.30 × 104
600 1.31 2.76 × 104
700 1.53 3.22 × 104
800 1.75 3.68 × 104
900 1.97 4.14 × 104
1000 2.19 4.60 × 104
2000 4.38 9.19 × 104
3000 6.57 1.38 × 105
4000 8.76 1.84 × 105
5000 11.0 2.30 × 105
6000 13.1 2.76 × 105
6460 14.2 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 60.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.200 2910
50.0 0.227 3310
60.0 0.273 3970
70.0 0.318 4630
80.0 0.363 5290
90.0 0.409 5960
100 0.454 6620
200 0.909 1.32 × 104
300 1.36 1.99 × 104
400 1.82 2.65 × 104
500 2.27 3.31 × 104
600 2.73 3.97 × 104
700 3.18 4.63 × 104
800 3.63 5.29 × 104
900 4.09 5.96 × 104
1000 4.54 6.62 × 104
2000 9.09 1.32 × 105
3000 13.6 1.99 × 105
4000 18.2 2.65 × 105
4490 20.4 2.97 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 70.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.370 3960
50.0 0.421 4500
60.0 0.505 5400
70.0 0.589 6300
80.0 0.673 7210
90.0 0.757 8110
100 0.842 9010
200 1.68 1.80 × 104
300 2.52 2.70 × 104
400 3.37 3.60 × 104
500 4.21 4.50 × 104
600 5.05 5.40 × 104
700 5.89 6.30 × 104
800 6.73 7.21 × 104
900 7.57 8.11 × 104
1000 8.42 9.01 × 104
2000 16.8 1.80 × 105
2450 20.7 2.21 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 80.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 0.632 5180
50.0 0.718 5880
60.0 0.861 7060
70.0 1.01 8230
80.0 1.15 9410
90.0 1.29 1.06 × 104
100 1.44 1.18 × 104
200 2.87 2.35 × 104
300 4.31 3.53 × 104
400 5.74 4.71 × 104
500 7.18 5.88 × 104
600 8.61 7.06 × 104
700 10.1 8.23 × 104
800 11.5 9.41 × 104
900 12.9 1.06 × 105
1000 14.4 1.18 × 105
1440 20.7 1.69 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 90.0 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 1.01 6550
50.0 1.15 7440
60.0 1.38 8930
70.0 1.61 1.04 × 104
80.0 1.84 1.19 × 104
90.0 2.07 1.34 × 104
100 2.30 1.49 × 104
200 4.60 2.98 × 104
300 6.90 4.47 × 104
400 9.20 5.96 × 104
500 11.5 7.44 × 104
600 13.8 8.93 × 104
700 16.1 1.04 × 105
800 18.4 1.19 × 105
898 20.7 1.34 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 100 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 1.54 8090
50.0 1.75 9190
60.0 2.10 1.10 × 104
70.0 2.45 1.29 × 104
80.0 2.80 1.47 × 104
90.0 3.15 1.65 × 104
100 3.51 1.84 × 104
200 7.01 3.68 × 104
300 10.5 5.51 × 104
400 14.0 7.35 × 104
500 17.5 9.19 × 104
589 20.7 1.08 × 105
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 125 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 3.77 1.26 × 104
50.0 4.28 1.44 × 104
60.0 5.13 1.72 × 104
70.0 5.99 2.01 × 104
80.0 6.85 2.30 × 104
90.0 7.70 2.58 × 104
100 8.56 2.87 × 104
200 17.1 5.74 × 104
241 20.7 6.93 × 104
Steel I Beam: W21 × 44 (Wide Flange 21 inch tall × 44 lbf/ft)
L = 150 ft
P (lbf/ft) w_max (in) stress_max (psi)
44.0 7.81 1.82 × 104
50.0 8.87 2.07 × 104
60.0 10.6 2.48 × 104
70.0 12.4 2.89 × 104
80.0 14.2 3.31 × 104
90.0 16.0 3.72 × 104
100 17.7 4.14 × 104
116 20.7 4.82 × 104
Additional Information
Related Pages
Home  About Us  Privacy  Disclaimer  Contact  Copyright © 2012 eFunda, Inc.