and the maximum normal stress occuring at the center support of the beam.![]() of steels can range from 1.015 × 104 to 2.970 × 105 psi. The purpose of this page is to give a rough estimation of the load-bearing capacity of this particular beam, rather than a guideline for designing actual building structures. Please check your local building codes for regulatory requirements.
Note: The weight of the beam itself is not included in the calculation.
Additional Information
Related Glossary Pages
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W14 × 233
Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W21 × 122 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Two Equal Spans: Wide Flange Steel I Beam: W8 × 10 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span: Wide Flange Steel I Beam: W16 × 26 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans: Wide Flange Steel I Beam: W21 × 50 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans: Wide Flange Steel I Beam: W6 × 16 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: Wide Flange Steel I Beam: W14 × 53 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Single Span: Aluminum I Beam: 8.00 × 7.023 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Three Equal Spans: Wide Flange Steel I Beam: W10 × 45 Glossary: Beams: Simply Supported: Uniformly Distributed Load: Four Equal Spans: S Section Steel I Beam: S12 × 40.8 Related Pages
eFunda: Glossary: Beams: Simply Supported: Uniformly Distributed ...
eFunda Glossary for beams, Simply Supported, Uniformly Distributed Load, Single Span, Wide Flange Steel I Beam, W10 × 22.
eFunda: Glossary: Beams: Simply Supported: Uniformly Distributed ...
eFunda Glossary for beams, Simply Supported, Uniformly Distributed Load, Single Span, Wide Flange Steel I Beam, W14 × 257.
Specific Beam Loading Case: Cantilever: Triangular Load
Beams » Simply Supported » Uniformly Distributed Load » Single Span » Aluminum I Beam · Beams » Simply Supported » Uniformly Distributed Load » Single Span ...
Engineering Fundamentals: Standard Beams
Database of geometric properties for beams with common cross sections.
Specific Beam Loading Case: Simply Supported: Uniform Load
Specific Beam Loading Case: Simply Supported: Uniform Load.
eFunda: Classical Plate Case Study
Rectangular plate, simply-supported on all edges, uniform loading. ... Rectangular plate, free on one edge, simply-supported on other edges, uniform loading ...
Specific Beam Loading Case: Simply Supported: 2 Symmetric Loads
Specific Beam Loading Case: Simply Supported: 2 Symmetric Loads.
eFunda: Glossary: Beams: Simply Supported: Uniformly Distributed ...
The tabulated data listed in this page are calculated based on the area moment of inertia (Ixx = 26.2 in4) for the W5 × 19 Wide Flange Steel I Beam and the ...
eFunda: Glossary: Beams: Simply Supported: Uniformly Distributed ...
Steel I Beam: W18 × 97 (Wide Flange 18 inch tall × 97 lbf/ft) ..... Steel Wide Flange I-Beams ... For Example: W27 × 161 is an I-Beam with a Depth of 27 ...
W Type I-beam search page
W24 × 162, 47.7, 25.00, 12.955, 1.220, 0.705, 5170, 414, 10.4, 443, 68.4, 3.05. W24 × 146, 43.0, 24.74, 12.900, 1.090, 0.650, 4580, 371, 10.3, 391, 60.5 ...
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||