295.0 is categorized as Cast Aluminum Alloy. It is composed of (in weight percentage) 94.70% Aluminum (Al), 4.50% Copper (Cu), and 0.80% Silicon (Si). It is usually used in sand casting.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Cast Aluminum Alloys include 201.0, 206.0, A206.0, 208.0, 242.0, 296.0, 308.0, 319.0, 336.0, 354.0, 355.0, C355.0, 356.0, A356.0, 357.0, A357.0, 359.0, 360.0, A360.0, 380.0, A380.0, 383.0, 384.0, A384.0, 390.0, A390.0, 413.0, A413.0, 443.0, A443.0, B443.0, C443.0, 514.0, 518.0, 520.0, 535.0, A535.0, B535.0, 712.0, 713.0, 771.0, and 850.0.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 40% Long Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 308L Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1080 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A414 Grade C Glossary: Materials: Alloys: Steel: Tool Steel: AISI T15 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1522H Glossary: Materials: Polymers: Thermoplastic Elastomers: Polyether/amide Block Copolymer Glossary: Materials: Polymers: Polyester: Glass Fiber Reinforced: SMC, BMC Low Density Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): Unreinforced, Toughened Glossary: Materials: Polymers: Polyphenylene Sulfide: 50% Long Glass Fiber Reinforced Related Pages
eFunda: Properties of Tool Steel 295.0
eFunda: Properties of Tool Steel 295.0. ... Tool Steel 295.0 About Us | Directory | Career | News | InfoStore | Industrial | Ask an Expert ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
Sand Casting: Allowance
Pattern finish allowance and wall thickness for various metals such as Aluminum, Copper Alloys, Cast Iron, Nickel Alloys, Steel, Magnesium Alloys, ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy 295.0. ... Aluminum Alloy Aluminum Alloy Aluminum Alloy 295.0 ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel 295.0
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel 295.0.
eFunda: Properties of Stainless Steel 295.0
eFunda: Properties of Stainless Steel 295.0. ... Stainless Steel 295.0 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Listing of Cast Aluminum Alloys
eFunda: Listing of Cast Aluminum Alloys. ... Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
Shell Mold Casting
Shell mold casting produces better surface finish, better dimensional tolerances
Investment Casting
Investment casting, lost wax casting process is used to make precision parts that may not need further machining. In ancient times this was used to make ...
|
||||||||