AA 1060 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 99.60%(min) Aluminum (Al). It can be seen in forms of sheet, plate, extruded tubes, and drawn tube.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8627
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C70400 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C67500 Glossary: Materials: Polymers: Liquid Crystal Polymer: 30% Carbon Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C18900 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99400 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 86B30H Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade H Glossary: Materials: Polymers: Polyethylene: Crosslinked: Wire and Cable Grade Glossary: Materials: Polymers: Polyester: P / PC Blend: High Impact Related Pages
eFunda: Listing of Alloy Steels
A535.0, Cast. AA 1050, Wrought. AA 1060, Wrought. AA 1100, Wrought. AA 1145, Wrought. AA 1199, Wrought. AA 1350, Wrought. AA 2011, Wrought. AA 2014, Wrought ...
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel AA 1060
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel AA 1060.
eFunda: Listing of Bronzes Copper Alloys
Copper Alloy. Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass ... UNS C54400, Wrought, Free-cutting phosphor bronze ...
Polymers: Data Sheet terms (Plastics)
Descriptive polymer selection guidelines with emphasis on reading data sheets.
eFunda: Derivation of Classical Plate Equation -- Kinematics
Kinematics describes how the plate's displacements and strains relate: ... For the classical plate, the assumptions were given by Kirchoff and dictate how ...
Heat Transfer Resulting from Laminar Flow Over an Isothermal Plate
Air (or any other fluid) forced over a hot plate will remove heat from the plate according to the rules of forced convection. If the air's velocity is slow ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
eFunda: Classical Plate Equation
Classical plate equation, its derivation and associated assumptions.
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda: Properties of Aluminum Alloy AA 1060
eFunda: Properties of Aluminum Alloy AA 1060. ... Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx · AA 5xxx · AA 6xxx · AA 7xxx. Cast: ...
|
||||||||