Aluminum Alloy: AA 1199
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 1199
AA 1199 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 99.99%(min) Aluminum (Al). It can be seen in the form of foil.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C15500
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 303PlusX Glossary: Materials: Polymers: Polyurethane: Thermoplastic: Long Glass Reinforced: Molding Compound Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6066 Glossary: Materials: Polymers: Polyphenylene Sulfide: Unfilled Glossary: Materials: Polymers: Cellulosic: Ethyl Cellulose: Molding Compound and Sheet Glossary: Materials: Polymers: Polystyrene: Homopolymer: Heat Resistant Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: 6% Stainless Steel Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C23000 Glossary: Materials: Polymers: Liquid Crystal Polymer: Glass Fiber Reinforced: Used for SMT Related Pages
eFunda: Properties of Aluminum Alloy AA 3004
eFunda: Properties of Aluminum Alloy AA 3004. ... Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys ...
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys.
eFunda: Temper Designations of Aluminum Alloys
A list of temper designations and their definitions for aluminum alloys.
Strain Gage: Installation
The tape-assisted installation method is the most popular method to install metal-foil strain gages. Its procedures can be summarized as follows. ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
eFunda: Listing of Bronzes Copper Alloys
Copper Alloy. Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass ... UNS C54400, Wrought, Free-cutting phosphor bronze ...
eFunda: Listing of Titanium Alloys
Ti-5Al-2.5Sn, Wrought, Alpha alloy. Ti-5Al-2.5Sn-ELI (low O2), Wrought, Alpha alloy. Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Wrought, Near alpha alloy ...
eFunda: Listing of Wrought Aluminum Alloys
AA 1199, Wrought. AA 1350, Wrought. AA 2011, Wrought. AA 2014, Wrought. AA 2024, Wrought. AA 2036, Wrought. AA 2048, Wrought. AA 2124, Wrought. AA 2218 ...
eFunda: Listing of Brasses Copper Alloys
Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass. UNS C22600, Wrought, Copper-zinc brass. UNS C23000, Wrought, Copper-zinc brass ...
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
|
||||||||