AA 2024 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 93.50% Aluminum (Al), 4.4% Copper (Cu), 0.6% Manganese (Mn), and 1.5% Magnesium (Mg). It can be seen in forms of sheet, plate, extruded rod bar and wire, extruded tubes, cold finished rod bar and wire, and drawn tube.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1038H
Glossary: Materials: Polymers: Polyvinylchloride: PVC and PVC-AMC: Unfilled: Sheets, Rods and Tubes; Flexible Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Nylon, Unreinforced Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 30% Glass Fiber Reinforced, Impact Modified Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-5 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C91300 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C90700 Glossary: Materials: Polymers: Polyethylene: Ethylene / Methyl Acrylate, Low Density Copolymer Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A387 Grade 12 Glossary: Materials: Alloys: Steel: Tool Steel: AISI H14 Related Pages
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
Polymers: Data Sheet terms (Plastics)
Descriptive polymer selection guidelines with emphasis on reading data sheets.
Stamping: Machining of Sheet Metals
Drilling, tapping, counterboring, and countersinking are the usual operations done in sheet metal.
eFunda: Listing of UNS C6xxxx Copper Alloys
Wrought Alloys. Cu Alloy List ... Name, Type, Common Name. UNS C60800, Wrought, Aluminum bronze, 5% ... UNS C65500, Wrought, High-silicon bronze, A ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C18900, Wrought, High-copper alloy ... UNS C19100, Wrought, Copper-nickel-phosphorus-tellurium alloy ...
eFunda: Listing of Brasses Copper Alloys
Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass. UNS C22600, Wrought, Copper-zinc brass. UNS C23000, Wrought, Copper-zinc brass ...
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the displacement of a clamped rectangular plate under a triangularly distributed load.
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
Welding
Plating of spot welded assemblies can cause problems when the sheet metal is overlapped. This can cause plating salts to be trapped-requiring special ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
|
||||||||