Aluminum Alloy: AA 4032
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 4032
AA 4032 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 85.0% Aluminum (Al), 12.20% Silicon (Si), 0.90% Copper (Cu), 1.0% Magnesium (Mg), and 0.9% Nickel (Ni). It can be seen in the form of forgings.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304L
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5254 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-29 Glossary: Materials: Polymers: Polyacrylates: Coated Sheet Glossary: Materials: Polymers: Polyphenylene Sulfide: Encapsulation Grades Glossary: Materials: Polymers: Liquid Crystal Polymer: Unfilled: Medium Melting Point Glossary: Materials: Alloys: Aluminum Alloy: Cast: 208.0 Glossary: Materials: Alloys: Steel: Tool Steel: AISI O2 Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 40% Glass: Flame-Retardant Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C84500 Related Pages
eFunda: Properties of Aluminum Alloy AA 4032
eFunda: Properties of Aluminum Alloy AA 4032. ... Aluminum Alloy AA 4032 About Us | Directory | Career | News | InfoStore | Industrial | Ask an Expert ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy AA 4032. ... AA 1xxx. AA 2xxx. AA 3xxx. AA 4xxx. AA 5xxx. AA 6xxx. AA 7xxx ...
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
eFunda: Listing of AA 2xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx. AA 2xxx ...
Forging
Forging is a process in which a metal is heated and placed in a die and a compressive force is applied. The metal takes the shape of the die and very strong ...
eFunda: Listing of Brasses Copper Alloys
Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass. UNS C22600, Wrought, Copper-zinc brass. UNS C23000, Wrought, Copper-zinc brass ...
eFunda: General Information on Titanium Alloys
Commercially produced titanium products are made in the following mill wrought forms; plate, tubing, sheet, wire, extrusions, and forgings. ...
eFunda: Listing of Coppers, High-Copper Alloys
UNS C11100, Wrought, Electrolytic tough pitch, anneal resistant copper alloy ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
|
||||||||