AA 5005 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 99.2% Aluminum (Al) and 0.8% Magnesium (Mg). It can be seen in forms of sheet, plate, and cold finished rod bar and wire.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type B
Glossary: Materials: Alloys: Magnesium Alloy: ASTM M1A-F Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1012 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1010 Glossary: Materials: Polymers: Polyphthalamide: 40% Glass / Mineral Reinforced Glossary: Materials: Polymers: Polyvinylidene Chloride: Copolymer: Injection Molding Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 404 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C70600 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 302 Glossary: Materials: Alloys: Aluminum Alloy: Cast: 850.0 Related Pages
Laminar Forced Convection Over an Isothermal Plate
The transition from laminar to turbulent for flow over a flat plate occurs in ... We are interested only in laminar flow, so it is assumed that the plate ...
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the displacement of a clamped rectangular plate under a uniform load.
eFunda: Listing of Coppers, High-Copper Alloys
UNS C11100, Wrought, Electrolytic tough pitch, anneal resistant copper alloy ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C18900, Wrought, High-copper alloy ... UNS C19100, Wrought, Copper-nickel-phosphorus-tellurium alloy ...
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
Cold Forging
This process is also known as Cold Heading. Bar stock or wire stock is fed ... screw drivers etc. the shaping rod stock by forming the head as in rivets, ...
efunda: Sheet metal gage Size Calculator
Calculator for the specification of sheet metal thickness.
eFunda: Properties of Aluminum Alloy AA 5005
eFunda: Properties of Aluminum Alloy AA 5005. ... Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx · AA 5xxx · AA 6xxx · AA 7xxx. Cast: ...
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys.
|
||||||||