Aluminum Alloy: AA 5086
Home |
Directory |
Career |
News |
Industrial
|
|
![]() ![]()
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 5086
AA 5086 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 95.4% Aluminum (Al), 0.4% Manganese (Mn), 4.0% Magnesium (Mg), and 0.15% Chromium (Cr). It can be seen in forms of sheet, plate, extruded rod bar and wire, extruded shapes, extruded tubes, and drawn tube.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C62500
Glossary: Materials: Polymers: Polyetherimide: 30% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B15 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4820H Glossary: Materials: Polymers: Thermoplastic Elastomers: Polyurethane: Polyester Compound: Molding and Extrusion Compounds, Low and Medium Hardness Glossary: Materials: Polymers: Polycarbonate: Unfilled: Molding and Extrusion Resins, Low Viscosity Glossary: Materials: Polymers: Polysulfone: Poly(phenylene-Sulfone) Glossary: Materials: Polymers: Polyphthalamide: 45% Glass Reinforced Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-8Al-1Mo-1V Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 410 Related Pages
Laminar Forced Convection Over an Isothermal Plate
The transition from laminar to turbulent for flow over a flat plate occurs in ... We are interested only in laminar flow, so it is assumed that the plate ...
efunda: Sheet metal gage Size Calculator
Calculator for the specification of sheet metal thickness.
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C18900, Wrought, High-copper alloy ... UNS C19100, Wrought, Copper-nickel-phosphorus-tellurium alloy ...
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the displacement of a clamped rectangular plate under a uniform load.
Welding
Plating of spot welded assemblies can cause problems when the sheet metal is overlapped. This can cause plating salts to be trapped-requiring special ...
eFunda: Properties of Aluminum Alloy AA 2218
Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Properties of Aluminum Alloy AA 5086
eFunda: Properties of Aluminum Alloy AA 5086. ... Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx · AA 5xxx · AA 6xxx · AA 7xxx. Cast: ...
eFunda: Properties of Magnesium Alloy ASTM ZK60A-T5
Hardness (HB500), 88, 25, T5 (extruded bars and shapes). Shear Strength (MPa), 180 · 25, T5 (extruded bars and shapes) ...
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
eFunda: Plate Calculator -- Free-Simply supported circular plate ...
This calculator computes the displacement of a simply-supported circular plate with free edge under a uniformly distributed load.
|
|||||||||||||||||||||||||