Aluminum Alloy: AA 5182
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 5182
AA 5182 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 95.2% Aluminum (Al), 0.35% Manganese (Mn), and 4.5% Magnesium (Mg). It can be seen in the form of sheet.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PVC: Flame-Retardant Grades, Molding and Extrusion
Glossary: Materials: Polymers: Polyacrylates: Copolymer: MMA / Styrene: Molding and Extrusion Compounds Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type F Glossary: Materials: Polymers: Fluoroplastics: THV-200 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C69000 Glossary: Materials: Polymers: Polystyrene: Styrene / Maleic Anhydride (SMA) Copolymer: Impact Modified Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A678 Grade B Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4621H Glossary: Materials: Alloys: Steel: Tool Steel: AISI A2 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316N Related Pages
eFunda: Listing of Wrought Aluminum Alloys
AA 5052, Wrought. AA 5056, Wrought. AA 5083, Wrought. AA 5086, Wrought. AA 5154, Wrought. AA 5182, Wrought. AA 5252, Wrought ...
eFunda: Listing of Magnesium Alloys for Sheets and Plates
eFunda: Listing of Magnesium Alloys for Sheets and Plates.
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda: Listing of AA 2xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx. AA 2xxx ...
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5182
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5182.
eFunda: Listing of Titanium Alloys
Ti-5Al-2.5Sn, Wrought, Alpha alloy. Ti-5Al-2.5Sn-ELI (low O2), Wrought, Alpha alloy. Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Wrought, Near alpha alloy ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043.
|
||||||||