Aluminum Alloy: AA 5254
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 5254
AA 5254 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 96.2% Aluminum (Al), 3.5% Magnesium (Mg), and 0.25% Chromium (Cr). It can be seen in forms of sheet and plate.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A440
Glossary: Materials: Polymers: Polyacetal: Copolymer: 2 - 20% PTFE Filled Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-42 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C81300 Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 50% Long Glass Fiber Reinforced Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5182 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A699 Glossary: Materials: Polymers: Polyester: Poly(butylene-Terephthalate): 35% Glass Fiber Reinforced: Flame-Retardant Grade Glossary: Materials: Polymers: Polypropylene: Homopolymer: 30% PAN Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8640H Related Pages
eFunda: Listing of Wrought Aluminum Alloys
Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Temper Designations of Aluminum Alloys
A list of temper designations and their definitions for aluminum alloys.
eFunda: Properties of Aluminum Alloy AA 3004
eFunda: Properties of Aluminum Alloy AA 3004. ... Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5254
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 5254.
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys.
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy ...
Aluminum Alloy Aluminum Alloy Aluminum Alloy AA 5254 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Properties of Aluminum Alloy AA 2218
Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Listing of Titanium Alloys
Ti-5Al-2.5Sn, Wrought, Alpha alloy. Ti-5Al-2.5Sn-ELI (low O2), Wrought, Alpha alloy. Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Wrought, Near alpha alloy ...
eFunda: Properties of Aluminum Alloy AA 5254
eFunda: Properties of Aluminum Alloy AA 5254. ... Aluminum Alloy AA 5254 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an ...
|
||||||||