Aluminum Alloy: AA 6009
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 6009
AA 6009 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 97.7% Aluminum (Al), 0.80% Silicon (Si), 0.35% Copper (Cu), 0.5% Manganese (Mn), and 0.60% Magnesium (Mg). It can be seen in the form of sheet.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A572 Grade 60
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6463 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A284 Grade D Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4027 Glossary: Materials: Polymers: Cellulosic: Cellulose Acetate Butyrate: Molding and Extrusion Compound Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5147 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 9260 Glossary: Materials: Polymers: Polyacrylates: Alloy: Acrylic / PC: Molding and Extrusion Compounds Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 25% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Tool Steel: AISI H19 Related Pages
Stamping: Gage
The most commonly used sheet metal gage for brass, mild steel and stainless steel. ... Metal Gages are often used in the sheet metal industry. ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043.
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
eFunda: Listing of Wrought Aluminum Alloys
AA 5254, Wrought. AA 5356, Wrought. AA 5454, Wrought. AA 5456, Wrought. AA 5457, Wrought. AA 5652, Wrought. AA 5657, Wrought. AA 6005, Wrought. AA 6009 ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C18900, Wrought, High-copper alloy ... UNS C19100, Wrought, Copper-nickel-phosphorus-tellurium alloy ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy ...
Aluminum Alloy Aluminum Alloy Aluminum Alloy Aluminum Alloy AA 6009 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Listing of Bronzes Copper Alloys
Copper Alloy. Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass ... UNS C54400, Wrought, Free-cutting phosphor bronze ...
eFunda: Listing of AA 2xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx. AA 2xxx ...
Stamping: Machining of Sheet Metals
Drilling, tapping, counterboring, and countersinking are the usual operations done in sheet metal.
eFunda: Listing of Coppers, High-Copper Alloys
UNS C11100, Wrought, Electrolytic tough pitch, anneal resistant copper alloy ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
|
||||||||