AA 6010 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 97.3% Aluminum (Al), 1.0% Silicon (Si), 0.35% Copper (Cu), 0.5% Manganese (Mn), and 0.80% Magnesium (Mg). It can be seen in the form of sheet.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Tool Steel: AISI M3 Class 2
Glossary: Materials: Alloys: Steel: Stainless Steel: 26-1Ti Glossary: Materials: Polymers: Polyester: Poly(butylene-Terephthalate): Unfilled Glossary: Materials: Polymers: Liquid Crystal Polymer: 50% Mineral Filled Glossary: Materials: Polymers: Polyacetal: Copolymer: Mineral Filled Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-16 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A225 Grade B Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A715 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5160 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 420 Related Pages
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
Stamping: Gage
The most commonly used sheet metal gage for brass, mild steel and stainless steel. ... Metal Gages are often used in the sheet metal industry. ...
eFunda: Temper Designations of Aluminum Alloys
A list of temper designations and their definitions for aluminum alloys.
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda Polymers: Properties of Cellulosic {cellulose acetate, sheet}
eFunda: Listing of Brasses Copper Alloys
Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass. UNS C22600, Wrought, Copper-zinc brass. UNS C23000, Wrought, Copper-zinc brass ...
Polymers: Data Sheet terms (Plastics)
Descriptive polymer selection guidelines with emphasis on reading data sheets.
eFunda: Properties of Aluminum Alloy AA 6010
eFunda: Properties of Aluminum Alloy AA 6010. ... AA 1xxx. AA 2xxx. AA 3xxx. AA 4xxx. AA 5xxx. AA 6xxx. AA 7xxx. Cast: 2xx.0 or x2xx.0. 3xx.0 or x3xx.0 ...
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
|
||||||||