Aluminum Alloy: AA 6151
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 6151
AA 6151 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 98.2% Aluminum (Al), 0.90% Silicon (Si), 0.60% Magnesium (Mg), and 0.25% Chromium (Cr). It can be seen in the form of forgings.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4427
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ92A-T6 Glossary: Materials: Alloys: Magnesium Alloy: ASTM AM60A-F Glossary: Materials: Polymers: Melamine Formaldehyde: Cellulose Filled Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 81B45H Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6262 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 329 Glossary: Materials: Alloys: Aluminum Alloy: Cast: A356.0 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1050 Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Platable Related Pages
eFunda: Listing of Bronzes Copper Alloys
Copper Alloy. Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass ... UNS C54400, Wrought, Free-cutting phosphor bronze ...
eFunda: Listing of Brasses Copper Alloys
Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass. UNS C22600, Wrought, Copper-zinc brass. UNS C23000, Wrought, Copper-zinc brass ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys.
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: General Information on Titanium Alloys
Commercially produced titanium products are made in the following mill wrought forms; plate, tubing, sheet, wire, extrusions, and forgings. ...
eFunda: Properties of Alloy Steel AA 6151
eFunda: Properties of Alloy Steel AA 6151. ... Alloy Steel AA 6151 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda: Listing of Titanium Alloys
Ti-5Al-2.5Sn, Wrought, Alpha alloy. Ti-5Al-2.5Sn-ELI (low O2), Wrought, Alpha alloy. Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Wrought, Near alpha alloy ...
|
||||||||