AA 6351 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 97.8% Aluminum (Al), 1.0% Silicon (Si), 0.6% Manganese (Mn), and 0.6% Magnesium (Mg). It can be seen in forms of extruded rod bar and wire and extruded shapes.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 440B
Glossary: Materials: Alloys: Aluminum Alloy: Cast: 201.0 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 15B48H Glossary: Materials: Polymers: Thermoplastic Elastomers: Silicone / Polyolefin: Pseudo-Interpenetrating Networks Glossary: Materials: Polymers: Polyester: Poly(butylene-Terephthalate): 50% Glass Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C80700 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1145 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1015 Glossary: Materials: Polymers: Polyamide: Nylon (PA 612): 10% PTFE: Lubricated Related Pages
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
eFunda: Listing of AA 2xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx. AA 2xxx ...
eFunda: Properties of Magnesium Alloy ASTM M1A-F
Hardness (HB500), 44, 25, (extruded bars and shapes). Shear Strength (MPa), 125 · 25, F (extruded bars and shapes). Thermal Properties ...
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys
eFunda: Listing of Cast Alumnium Alloys 2xx.0 Aluminum Alloys.
eFunda: Listing of AA 5xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx. AA 5xxx. AA 6xxx · AA 7xxx. Cast: ...
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda: Listing of Wrought Aluminum Alloys
Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
Extrusion, hot extrusion, cold extrusion
The parts can be solid or hollow, and can be round, rectangular, T shape, tubes etc. ... Examples of parts that are cold extruded are collapsible tubes, ...
eFunda: Properties of Magnesium Alloy ASTM ZK21A-F
Tensile Strength (Mpa), 260.0 · 25, F (extruded bars and shapes). Yield Strength (Mpa), 195.0 (135.0). Elongation (%), 4.0. Reduction in Area (%) ...