Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 6463
AA 6463 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 98.9% Aluminum (Al), 0.40% Silicon (Si), and 0.70% Magnesium (Mg). It can be seen in forms of extruded rod bar and wire and extruded shapes.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C91700
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1522H Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A588 Grade H Glossary: Materials: Polymers: Polyacetal: Homopolymer: Extrusion Grade Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-32 Glossary: Materials: Polymers: Polyamide: Partially Aromatic: 40% Glass Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-2 Glossary: Materials: Alloys: Steel: Stainless Steel: CryogenicTenelon Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 945A Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316LN Related Pages
eFunda: Typical Properties of Aluminum Alloys
Typical physical properties of aluminum alloys such as melting point, elastic modulus, poisson ration, thermal expansion coefficient, etc.
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel Alloy ...
eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel Alloy Steel AA 6463. ... Alloy Steel Alloy Steel Alloy Steel Alloy Steel AA 6463 ...
eFunda: Properties of Aluminum Alloy AA 6463
eFunda: Properties of Aluminum Alloy AA 6463. ... Al Alloy List. Wrought: AA 1xxx · AA 2xxx · AA 3xxx · AA 4xxx · AA 5xxx · AA 6xxx · AA 7xxx. Cast: ...
eFunda: Listing of UNS C6xxxx Copper Alloys
Wrought Alloys. Cu Alloy List ... Name, Type, Common Name. UNS C60800, Wrought, Aluminum bronze, 5% ... UNS C65500, Wrought, High-silicon bronze, A ...
eFunda: Properties of Magnesium Alloy ASTM ZK40A-T5
Tensile Strength (Mpa), 276.0 · 25, T5 (extruded bars and shapes). Yield Strength (Mpa), 255.0 (140.0). Elongation (%), 4.0. Reduction in Area (%) ...
eFunda: Properties of Alloy Steel Alloy Steel AA 6463
eFunda: Properties of Alloy Steel Alloy Steel AA 6463.
eFunda: Properties of Magnesium Alloy ASTM AZ31B-F
Hardness (HB500), 49, 25, F (extruded bars and shapes). Shear Strength (MPa), 130 · 25, F (extruded bars and shapes) ...
eFunda: General Information on Aluminum Alloys
General information for aluminum alloys and their characteristics.
eFunda: Properties of Magnesium Alloy ASTM M1A-F
Hardness (HB500), 44, 25, (extruded bars and shapes). Shear Strength (MPa), 125 · 25, F (extruded bars and shapes). Thermal Properties ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy ...
Aluminum Alloy Aluminum Alloy Aluminum Alloy Aluminum Alloy AA 6463 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
|
||||||||