Aluminum Alloy: AA 7049
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Aluminum Alloy » Wrought » AA 7049
AA 7049 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 88.2% Aluminum (Al), 1.5% Copper (Cu), 2.5% Magnesium (Mg), 0.15% Chromium (Cr), and 7.6% Zinc (Zn). It can be seen in forms of plate, extruded rod bar and wire, extruded shapes, and forgings.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7050, AA 7072, AA 7075, AA 7175, AA 7178, and AA 7475.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A515 Grade 60
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4419 Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-3Al-2.5V Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 7075 Glossary: Materials: Polymers: Polysulfone: Poly(phenylene-Sulfone) Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A387 Grade 9 Glossary: Materials: Polymers: Polyamide: Nylon (PA 11): Molding and Extrusion Compound Glossary: Materials: Alloys: Steel: Tool Steel: AISI H42 Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): 30% Carbon Fiber Reinforced Glossary: Materials: Polymers: Polyphenylene Sulfide: 40% Long Glass Fiber Reinforced Related Pages
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2014.
eFunda: Properties of Aluminum Alloy AA 5154
eFunda: Properties of Aluminum Alloy AA 5154. ... Sponsored Links. AA 5154. Category, Aluminum Alloy. Class, Wrought. Composition. Element, Weight % ...
eFunda: Plate Calculator -- Free-Simply supported circular plate ...
This calculator computes the displacement of a simply-supported circular plate with free edge under a uniformly distributed load.
eFunda: Listing of Wrought Aluminum Alloys
Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Classical Plate Case Study
Plate calculators, rectangular and circular plates with various boundary and loading conditions.
eFunda: Listing of Wrought Aluminum Alloys
AA 6101, Wrought. AA 6151, Wrought. AA 6201, Wrought. AA 6205, Wrought. AA 6262, Wrought. AA 6351, Wrought. AA 6463, Wrought. AA 7005, Wrought. AA 7049 ...
Cold Forging
Cold Forging is a cold working process where the material is squeezed into a die and the finished parts assume the shape of the die.
eFunda: Listing of AA 2xxx Aluminum Alloys
Al Alloy Types. Cast Alloys · Wrought Alloys. Al Alloy List. Wrought: AA 1xxx. AA 2xxx ...
eFunda: Introduction to Extrusion Molding
... usually a custom steel die with shape of the cross section of the intended part, ... When designing an extruded part, it is advisable to keep the wall ...
eFunda: Listing of AA 7xxx Aluminum Alloys
AA 7049, Wrought. AA 7050, Wrought. AA 7072, Wrought. AA 7075, Wrought. AA 7175, Wrought. AA 7178, Wrought. AA 7475, Wrought ...
|
||||||||