AA 7475 is categorized as Wrought Aluminum Alloy. It is composed of (in weight percentage) 90.3% Aluminum (Al), 1.50% Silicon (Si), 2.3% Magnesium (Mg), 0.22% Chromium (Cr), and 5.7% Zinc (Zn). It can be seen in forms of sheet, plate, and forgings.
Aluminum is a silverish white metal that has a strong resistance to corrosion and like gold, is rather malleable. It is a relatively light metal compared to metals such as steel, nickel, brass, and copper with a specific gravity of 2.7. Aluminum is easily machinable and can have a wide variety of surface finishes. It also has good electrical and thermal conductivities and is highly reflective to heat and light.
The typical elastic modulus of aluminum alloys at room temperature (25°C) ranges from 70 to 79 GPa. The typical density of aluminum alloys ranges from 2.6 to 2.8 g/cm3. The typical tensile strength varies between 230 and 570 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Aluminum Alloys include AA 1050, AA 1060, AA 1100, AA 1145, AA 1199, AA 1350, AA 2011, AA 2014, AA 2024, AA 2036, AA 2048, AA 2124, AA 2218, AA 2219, AA 2319, AA 2618, AA 3003, AA 3004, AA 3105, AA 4032, AA 4043, AA 5005, AA 5050, AA 5052, AA 5056, AA 5083, AA 5086, AA 5154, AA 5182, AA 5252, AA 5254, AA 5356, AA 5454, AA 5456, AA 5457, AA 5652, AA 5657, AA 6005, AA 6009, AA 6010, AA 6061, AA 6063, AA 6066, AA 6070, AA 6101, AA 6151, AA 6201, AA 6205, AA 6262, AA 6351, AA 6463, AA 7005, AA 7049, AA 7050, AA 7072, AA 7075, AA 7175, and AA 7178.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 5% Molydenum Disulfide and 30% PTFE: Lubricated
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A538 Grade B Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8642 Glossary: Materials: Polymers: Polyphthalamide: Extra Tough Glossary: Materials: Alloys: Aluminum Alloy: Cast: 712.0 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A588 Grade A Glossary: Materials: Polymers: Polyimide: Thermoset: Unfilled Glossary: Materials: Polymers: Fluoroplastics: PE-CTFE Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4130H Glossary: Materials: Polymers: Thermoplastic Elastomers: Elastomeric Alloy: Low and Medium Hardness Related Pages
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 4043.
eFunda: Properties of Aluminum Alloy AA 7475
eFunda: Properties of Aluminum Alloy AA 7475. ... Aluminum Alloy AA 7475 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an ...
eFunda: Properties of Aluminum Alloy AA 3004
eFunda: Properties of Aluminum Alloy AA 3004. ... Aluminum Alloys. General Information · Properties · Temper. Al Alloy Types. Cast Alloys · Wrought Alloys ...
eFunda: Classical Plate Case Study
Plate calculators, rectangular and circular plates with various boundary and loading conditions.
eFunda: Properties of Alloy Steel AA 7475
eFunda: Properties of Alloy Steel AA 7475. ... Alloy Steel AA 7475 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the displacement of a clamped rectangular plate under a uniform load.
efunda: Sheet metal gage Size Calculator
Calculator for the specification of sheet metal thickness.
eFunda: Plate Calculator -- Clamped rectangular plate with ...
This calculator computes the displacement of a clamped rectangular plate under a triangularly distributed load.
Cold Forging
Cold Forging is a cold working process where the material is squeezed into a die and the finished parts assume the shape of the die.
eFunda: Listing of UNS C6xxxx Copper Alloys
Wrought Alloys. Cu Alloy List ... Name, Type, Common Name. UNS C60800, Wrought, Aluminum bronze, 5% ... UNS C65500, Wrought, High-silicon bronze, A ...
|
||||||||