UNS C95410 is an Aluminum Bronze grade Cast Copper Alloy. It is composed of (in weight percentage) 85% Copper (Cu), 4% Iron (Fe), 11% AIodine (I), and 2% Nickel (Ni). Another common designation of UNS C95410 copper alloy is UNS C95410.
Copper is one of the most useful metals known to man, and it was one of the first to be utilized. Copper is a reddish-yellow material and is extremely ductile. Copper has a face-centered-cubic (fcc) crystal structure and has the second best electrical conductivity of the metals, second only to silver compared to which it has a conductivity of 97%. The thermal conductivity of copper is very high, falling in between silver and gold. There are almost 400 different copper alloys depending on the commercial product made; rods, plates, sheets, strips, tubes, pipes, extrusions, foils, forgings, wires, and castings from foundries.
The typical elastic modulus of copper alloys at room temperature (25°C) is about 117 GPa. The typical density of copper alloys ranges from 8.8 to 8.94 g/cm3. The typical tensile strength varies between 172 and 220 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Cast Copper Alloys include UNS C80100, UNS C80300, UNS C80500, UNS C80700, UNS C80900, UNS C81100, UNS C81300, UNS C81400, UNS C81500, UNS C81700, UNS C81800, UNS C82000, UNS C82100, UNS C82200, UNS C82400, UNS C82500, UNS C82600, UNS C82700, UNS C82800, UNS C83300, UNS C83400, UNS C83600, UNS C83800, UNS C84200, UNS C84400, UNS C84500, UNS C84800, UNS C85200, UNS C85400, UNS C85500, UNS C85700, UNS C85800, UNS C86100, UNS C86200, UNS C86300, UNS C86400, UNS C86500, UNS C86700, UNS C86800, UNS C87200, UNS C87400, UNS C87500, UNS C87600, UNS C87800, UNS C87900, UNS C90200, UNS C90300, UNS C90500, UNS C90700, UNS C90800, UNS C90900, UNS C91000, UNS C91100, UNS C91300, UNS C91600, UNS C91700, UNS C92200, UNS C92300, UNS C92400, UNS C92500, UNS C92600, UNS C92700, UNS C92800, UNS C92900, UNS C93200, UNS C93400, UNS C93500, UNS C93700, UNS C93800, UNS C93900, UNS C94000, UNS C94100, UNS C94300, UNS C94400, UNS C94500, UNS C94700, UNS C94800, UNS C94900, UNS C95200, UNS C95300, UNS C95400, UNS C95500, UNS C95600, UNS C95700, UNS C95800, UNS C96200, UNS C96300, UNS C96400, UNS C96600, UNS C96700, UNS C97300, UNS C97400, UNS C97600, UNS C97800, UNS C98200, UNS C98400, UNS C98600, UNS C98800, UNS C99300, UNS C99400, UNS C99500, UNS C99600, UNS C99700, and UNS C99750.
Related Glossary Pages
Glossary: Materials: Polymers: Polyethylene: Low and Medium Density, Branched Homopolymer
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 309SCb Glossary: Materials: Alloys: Steel: Stainless Steel: Sea-Cure/Sc-1 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1137 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8645 Glossary: Materials: Alloys: Magnesium Alloy: ASTM ZK61A-T6 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8620 Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 945X Glossary: Materials: Polymers: Polyacrylates: Poly(methylmethacrylate), PMMA: Molding and Extrusion Compounds Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A620 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}
eFunda: Chemicals Compatibile with O-Ring Material Polyurethane, Cast
Chemicals Compatible with Polyurethane, Cast (select a chemical to show its compatible O-ring materials). Acetaldehyde (0), Acetamide (0), Acetic Acid, ...
eFunda: Listing of Aluminum Bronzes Copper Alloys
UNS C95200, Cast, Aluminum bronze. UNS C95300, Cast, Aluminum bronze. UNS C95400
Die Casting
On the other hand, pure Aluminum is rarely cast due to high shrinkage, and susceptibility to hot ... Aluminum is cast at a temperature of 650 ºC (1200 ºF). ...
eFunda: Listing of Cast Copper Alloys
eFunda: Listing of Cast Copper Alloys. ... Copper Alloy. Name, Type, Common Name
eFunda: Properties of Copper Alloy UNS C11000
eFunda: Properties of Copper Alloy UNS C11000. ... Type, Electrolytic tough pitch copper alloy. Designations, United States: UNS C11000 ...
eFunda: Listing of Cast Aluminum Alloys
eFunda: Listing of Cast Aluminum Alloys. ... Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Listing of Wrought Copper Alloys
UNS C11300, Wrought, Silver-bearing tough pitch copper alloy ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Properties of Copper Alloy UNS C95410
eFunda: Properties of Copper Alloy UNS C95410. ... Category, Copper Alloy. Class
|
||||||||