Copper Alloy: AWG-17
Home |
Directory |
Career |
News |
Industrial
|
|
![]() ![]()
|
|
Glossary » Materials » Alloys » Copper Alloy » Wire » AWG-17
AWG-17 is a Round Copper Wire grade Wire Copper Alloy. Other designations of AWG-17 copper alloy include ASTM B1, ASTM B3, and ASTM B258.
Copper is one of the most useful metals known to man, and it was one of the first to be utilized. Copper is a reddish-yellow material and is extremely ductile. Copper has a face-centered-cubic (fcc) crystal structure and has the second best electrical conductivity of the metals, second only to silver compared to which it has a conductivity of 97%. The thermal conductivity of copper is very high, falling in between silver and gold. There are almost 400 different copper alloys depending on the commercial product made; rods, plates, sheets, strips, tubes, pipes, extrusions, foils, forgings, wires, and castings from foundries.
The typical elastic modulus of copper alloys at room temperature (25°C) is about 117 GPa. The typical density of copper alloys ranges from 8.8 to 8.94 g/cm3. The typical tensile strength varies between 172 and 220 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wire Copper Alloys include AWG-1, AWG-1.0, AWG-10, AWG-11, AWG-12, AWG-13, AWG-14, AWG-15, AWG-16, AWG-18, AWG-19, AWG-2, AWG-2/0, AWG-20, AWG-21, AWG-22, AWG-23, AWG-24, AWG-25, AWG-26, AWG-27, AWG-28, AWG-29, AWG-3, AWG-3/0, AWG-30, AWG-31, AWG-32, AWG-33, AWG-34, AWG-35, AWG-36, AWG-37, AWG-38, AWG-39, AWG-4, AWG-4/0, AWG-40, AWG-41, AWG-42, AWG-43, AWG-44, AWG-5, AWG-6, AWG-7, AWG-8, and AWG-9.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-21
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5155H Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1065 Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 13% Glass Fiber Reinforced, Heat-Stablized Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade C Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A109 Temper 4 Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 40% Glass: Flame-Retardant Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 30% Long Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Tool Steel: AISI P4 Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 10% PTFE: Lubricated Related Pages
eFunda: Chemicals Compatibile with O-Ring Material Hypalon
Arachlor 1248 (1), Argon (1), Aromatic Fuel 50% (1). Askarel Transformer Oil (1)
eFunda: Properties of Alloy Steel AWG-17
eFunda: Properties of Alloy Steel AWG-17. ... Alloy Steel AWG-17 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Chemicals Compatibile with O-Ring Material Neoprene
Aromatic Fuel 50% (1), Askarel Transformer Oil (1), ASTM Fuel B (1). ASTM Fuel C (1), ASTM Fuel D (1), ASTM Oil Four (1) ...
efunda: wire gage Size Calculator
Calculator for looking up available wire gauge diameters.
eFunda: Properties of Copper Alloy UNS C11000
eFunda: Properties of Copper Alloy UNS C11000. ... Type, Electrolytic tough pitch copper alloy. Designations, United States: UNS C11000 ...
eFunda: Chemicals Compatibile with O-Ring Material Silicone
Amyl Chloronaphthalene (1), Aniline Oil (1), Aromatic Fuel 50% (1). Askarel Transformer Oil (1), ASTM Fuel A (1), ASTM Fuel B (1) ...
eFunda: Listing of Coppers, High-Copper Alloys
eFunda: Listing of Coppers, High-Copper Alloys. ... UNS C12500, Wrought, Fire-
eFunda: Chemicals Compatibile with O-Ring Material Polyacrylate
Aniline (1), Aniline Oil (1), Arachlor 1248 (1). Askarel Transformer Oil (1), ASTM Fuel B (1), ASTM Fuel C (1). ASTM Fuel D (1), Beer (1), Benzaldehyde (1) ...
eFunda: Introduction to Hot-Wire Anemometers
The Hot-Wire Anemometer is the most well known thermal anemometer, and measures a fluid velocity by noting the heat convected away by the fluid.
eFunda: Listing of Alloy Steels
AWG-16, Wire, Round copper wire. AWG-17, Wire, Round copper wire. AWG-18, Wire, Round copper wire. AWG-19, Wire, Round copper wire ...
|
|||||||||||||||||||||||||