AWG-23 is a Round Copper Wire grade Wire Copper Alloy. Other designations of AWG-23 copper alloy include ASTM B1, ASTM B3, and ASTM B258.
Copper is one of the most useful metals known to man, and it was one of the first to be utilized. Copper is a reddish-yellow material and is extremely ductile. Copper has a face-centered-cubic (fcc) crystal structure and has the second best electrical conductivity of the metals, second only to silver compared to which it has a conductivity of 97%. The thermal conductivity of copper is very high, falling in between silver and gold. There are almost 400 different copper alloys depending on the commercial product made; rods, plates, sheets, strips, tubes, pipes, extrusions, foils, forgings, wires, and castings from foundries.
The typical elastic modulus of copper alloys at room temperature (25°C) is about 117 GPa. The typical density of copper alloys ranges from 8.8 to 8.94 g/cm3. The typical tensile strength varies between 172 and 220 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wire Copper Alloys include AWG-1, AWG-1.0, AWG-10, AWG-11, AWG-12, AWG-13, AWG-14, AWG-15, AWG-16, AWG-17, AWG-18, AWG-19, AWG-2, AWG-2/0, AWG-20, AWG-21, AWG-22, AWG-24, AWG-25, AWG-26, AWG-27, AWG-28, AWG-29, AWG-3, AWG-3/0, AWG-30, AWG-31, AWG-32, AWG-33, AWG-34, AWG-35, AWG-36, AWG-37, AWG-38, AWG-39, AWG-4, AWG-4/0, AWG-40, AWG-41, AWG-42, AWG-43, AWG-44, AWG-5, AWG-6, AWG-7, AWG-8, and AWG-9.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11500
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1548 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C18700 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11000 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2124 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type H Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1100 Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Injection Molding Grade, Platable Glossary: Materials: Polymers: Polyphenylene Sulfide: 65% Mineral and Glass Filled Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 20-25% Glass Fiber Reinforced: Flame-Retardant Grade Related Pages
eFunda: Properties of Copper Alloy UNS C10100
eFunda: Properties of Copper Alloy UNS C10100. ... Type, Oxygen-free electronic copper alloy. Designations, United States: UNS C10100 ...
eFunda: Properties of Alloy Steel AWG-10
ASTM Steels. Specific Alloy Steel. General Information. Resources. Bibliography ... Designations, United States: ASTM B1, ASTM B3, ASTM B258 ...
eFunda: Chemicals Compatibile with O-Ring Material Natural Rubber
Askarel Transformer Oil (1), ASTM Fuel A (1), ASTM Fuel B (1). ASTM Fuel C (1), ASTM Fuel D (0), ASTM Oil Four (1). ASTM Oil One (1), ASTM Oil Three (1) ...
eFunda: Chemicals Compatibile with O-Ring Material Butyl
ASTM Fuel B (1), ASTM Fuel C (1), ASTM Oil Four (1). ASTM Oil One (1), ASTM Oil Three (1), ASTM Oil Two (1). Automatic Transmission Fluid (1), Benzene (1) ...
eFunda: Introduction to Hot-Wire Anemometers
The Hot-Wire Anemometer is the most well known thermal anemometer, and measures a fluid velocity by noting the heat convected away by the fluid.
eFunda: Properties of Copper Alloy UNS C15710
eFunda: Properties of Copper Alloy UNS C15710. ... Category, Copper Alloy. Class
efunda: wire gage Size Calculator
Calculator for looking up available wire gauge diameters.
eFunda: Listing of Cast Copper Alloys
eFunda: Listing of Cast Copper Alloys. ... Copper Alloy. Name, Type, Common Name
eFunda: Properties of Copper Alloy UNS C14500
eFunda: Properties of Copper Alloy UNS C14500. ... Type, Phosphorus deoxidized, tellurium bearing copper alloy. Designations, United States: UNS C14500 ...
eFunda: General Information on Copper Alloys
General information for copper alloys, their classifications, and the UNS designations.
|
||||||||