Glossary » Materials » Alloys » Copper Alloy » Wire » AWG-36
AWG-36 is a Round Copper Wire grade Wire Copper Alloy. Other designations of AWG-36 copper alloy include ASTM B1, ASTM B3, and ASTM B258.
Copper is one of the most useful metals known to man, and it was one of the first to be utilized. Copper is a reddish-yellow material and is extremely ductile. Copper has a face-centered-cubic (fcc) crystal structure and has the second best electrical conductivity of the metals, second only to silver compared to which it has a conductivity of 97%. The thermal conductivity of copper is very high, falling in between silver and gold. There are almost 400 different copper alloys depending on the commercial product made; rods, plates, sheets, strips, tubes, pipes, extrusions, foils, forgings, wires, and castings from foundries.
The typical elastic modulus of copper alloys at room temperature (25°C) is about 117 GPa. The typical density of copper alloys ranges from 8.8 to 8.94 g/cm3. The typical tensile strength varies between 172 and 220 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wire Copper Alloys include AWG-1, AWG-1.0, AWG-10, AWG-11, AWG-12, AWG-13, AWG-14, AWG-15, AWG-16, AWG-17, AWG-18, AWG-19, AWG-2, AWG-2/0, AWG-20, AWG-21, AWG-22, AWG-23, AWG-24, AWG-25, AWG-26, AWG-27, AWG-28, AWG-29, AWG-3, AWG-3/0, AWG-30, AWG-31, AWG-32, AWG-33, AWG-34, AWG-35, AWG-37, AWG-38, AWG-39, AWG-4, AWG-4/0, AWG-40, AWG-41, AWG-42, AWG-43, AWG-44, AWG-5, AWG-6, AWG-7, AWG-8, and AWG-9.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C92500
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade A Glossary: Materials: Polymers: Polyaryletherketone: Poly(arylether-Ketone): 30% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A284 Grade C Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4042 Glossary: Materials: Alloys: Steel: Tool Steel: AISI S6 Glossary: Materials: Polymers: Polyacetal: 30% Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C97400 Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Phenol-Formaldehyde: PAN Carbon: Molding Compounds Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1527 Related Pages
eFunda: Properties of Alloy Steel AWG-10
ASTM Steels. Specific Alloy Steel. General Information. Resources. Bibliography ... Designations, United States: ASTM B1, ASTM B3, ASTM B258 ...
eFunda: Listing of Alloy Steels
AWG-35, Wire, Round copper wire. AWG-36, Wire, Round copper wire. AWG-37, Wire, Round copper wire. AWG-38, Wire, Round copper wire ...
eFunda: Chemicals Compatibile with O-Ring Material Hypalon
Arachlor 1248 (1), Argon (1), Aromatic Fuel 50% (1). Askarel Transformer Oil (1)
eFunda: Chemicals Compatibile with O-Ring Material Polyacrylate
Aniline (1), Aniline Oil (1), Arachlor 1248 (1). Askarel Transformer Oil (1), ASTM Fuel B (1), ASTM Fuel C (1). ASTM Fuel D (1), Beer (1), Benzaldehyde (1) ...
eFunda: Chemicals Compatibile with O-Ring Material Neoprene
Aromatic Fuel 50% (1), Askarel Transformer Oil (1), ASTM Fuel B (1). ASTM Fuel C (1), ASTM Fuel D (1), ASTM Oil Four (1) ...
eFunda: Chemicals Compatibile with O-Ring Material Butyl
ASTM Fuel B (1), ASTM Fuel C (1), ASTM Oil Four (1). ASTM Oil One (1), ASTM Oil Three (1), ASTM Oil Two (1). Automatic Transmission Fluid (1), Benzene (1) ...
eFunda: Theory of Hot-Wire Anemometers
Hot wire anemometers are used to measure the velocity of a fluid. The theory behind hot wire anemometers is discussed here.
eFunda: Properties of Copper Alloy UNS C15710
eFunda: Properties of Copper Alloy UNS C15710. ... Category, Copper Alloy. Class
eFunda: Chemicals Compatibile with O-Ring Material Silicone
Amyl Chloronaphthalene (1), Aniline Oil (1), Aromatic Fuel 50% (1). Askarel Transformer Oil (1), ASTM Fuel A (1), ASTM Fuel B (1) ...
eFunda: Properties of Copper Alloy UNS C11500
eFunda: Properties of Copper Alloy UNS C11500. ... Category, Copper Alloy. Class
|
||||||||