AWG-6 is a Round Copper Wire grade Wire Copper Alloy. Other designations of AWG-6 copper alloy include ASTM B1, ASTM B3, and ASTM B258.
Copper is one of the most useful metals known to man, and it was one of the first to be utilized. Copper is a reddish-yellow material and is extremely ductile. Copper has a face-centered-cubic (fcc) crystal structure and has the second best electrical conductivity of the metals, second only to silver compared to which it has a conductivity of 97%. The thermal conductivity of copper is very high, falling in between silver and gold. There are almost 400 different copper alloys depending on the commercial product made; rods, plates, sheets, strips, tubes, pipes, extrusions, foils, forgings, wires, and castings from foundries.
The typical elastic modulus of copper alloys at room temperature (25°C) is about 117 GPa. The typical density of copper alloys ranges from 8.8 to 8.94 g/cm3. The typical tensile strength varies between 172 and 220 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wire Copper Alloys include AWG-1, AWG-1.0, AWG-10, AWG-11, AWG-12, AWG-13, AWG-14, AWG-15, AWG-16, AWG-17, AWG-18, AWG-19, AWG-2, AWG-2/0, AWG-20, AWG-21, AWG-22, AWG-23, AWG-24, AWG-25, AWG-26, AWG-27, AWG-28, AWG-29, AWG-3, AWG-3/0, AWG-30, AWG-31, AWG-32, AWG-33, AWG-34, AWG-35, AWG-36, AWG-37, AWG-38, AWG-39, AWG-4, AWG-4/0, AWG-40, AWG-41, AWG-42, AWG-43, AWG-44, AWG-5, AWG-7, AWG-8, and AWG-9.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C94800
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): Unreinforced, Toughened Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4145H Glossary: Materials: Polymers: Liquid Crystal Polymer: Unfilled: Medium Melting Point Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C74500 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C51100 Glossary: Materials: Polymers: Polyacetal: Copolymer: 25% Glass Coupled Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: 20% PAN Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 2618 Related Pages
eFunda: Theory of Hot-Wire Anemometers
Hot wire anemometers are used to measure the velocity of a fluid. The theory behind hot wire anemometers is discussed here.
eFunda: Chemicals Compatibile with O-Ring Material Butyl
ASTM Fuel B (1), ASTM Fuel C (1), ASTM Oil Four (1). ASTM Oil One (1), ASTM Oil Three (1), ASTM Oil Two (1). Automatic Transmission Fluid (1), Benzene (1) ...
eFunda: Properties of Alloy Steel AWG-12
Category, Copper Alloy. Class, Wire. Type, Round copper wire. Designations, United States: ASTM B1, ASTM B3, ASTM B258 ...
eFunda: General Information on Copper Alloys
General information for copper alloys, their classifications, and the UNS designations.
eFunda: Properties of Copper Alloy UNS C15000
eFunda: Properties of Copper Alloy UNS C15000. ... Category, Copper Alloy. Class
eFunda: Listing of Cast Copper Alloys
eFunda: Listing of Cast Copper Alloys. ... Copper Alloy. Name, Type, Common Name
eFunda: Properties of Copper Alloy UNS C14500
eFunda: Properties of Copper Alloy UNS C14500. ... Type, Phosphorus deoxidized, tellurium bearing copper alloy. Designations, United States: UNS C14500 ...
eFunda: Properties of Copper Alloy UNS C11000
eFunda: Properties of Copper Alloy UNS C11000. ... Type, Electrolytic tough pitch copper alloy. Designations, United States: UNS C11000 ...
eFunda: O-Ring Materials Compatibile with Chemical ASTM Fuel B
O-Ring Materials Compatible with ASTM Fuel B (select a material to show its compatible chemicals). Aflas (0), Buna-N (Nitrile) (2), Butyl (1) ...
eFunda: Chemicals Compatibile with O-Ring Material Polyacrylate
Aniline (1), Aniline Oil (1), Arachlor 1248 (1). Askarel Transformer Oil (1), ASTM Fuel B (1), ASTM Fuel C (1). ASTM Fuel D (1), Beer (1), Benzaldehyde (1) ...
|
||||||||