Stainless Steel: AISI Type 414L
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Steel » Stainless Steel » AISI Type 414L
AISI Type 414L is a Martensitic Nonstandard grade Stainless Steel. It is commonly called AISI Type 414L Chromium steel. It is composed of (in weight percentage) 0.06% Carbon (C), 0.50% Manganese (Mn), 0.15% Silicon (Si), 12.5-13.0% Chromium (Cr), 2.5-3.0% Nickel (Ni), 0.04% Phosphorus (P), 0.03% Sulfur (S), 0.5% Molybdenum (Mo), 0.03% Aluminum (Al), and the base metal Iron (Fe). Another common designation of AISI Type 414L stainless steel is AISI 414L.
Steel is the common name for a large family of iron alloys. Steels can either be cast directly to shape, or into ingots which are reheated and hot worked into a wrought shape by forging, extrusion, rolling, or other processes. Wrought steels are the most common engineering material used, and come in a variety of forms with different finishes and properties. Stainless steels are high-alloy steels that have superior corrosion resistance than other steels because they contain large amounts of chromium. Stainless steels contains at least 10% chromium, with or without other elements. Stainless steels can be divided into three basic groups based on their crystalline structure: austenitic, ferritic, and martensitic.
The typical elastic modulus of stainless steels at room temperature (25°C) ranges from 190 to 210 GPa. The typical density of stainless steels ranges from 7.75 to 8.1 g/cm3. The typical tensile strength varies between 515 and 827 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Stainless steels include 15-5PH, 17-10P, 17-4PH, 17-7PH, 18-18-2, 18-18PlusTM, 18-2FM, 18SR, 20Cb-3TM, 26-1Ti, 29-4, 29-4-2, 904L, AISI S30430, AISI Type 201, AISI Type 202, AISI Type 205, AISI Type 216, AISI Type 301, AISI Type 302, AISI Type 302B, AISI Type 302Cu, AISI Type 303, AISI Type 303PlusX, AISI Type 303Se, AISI Type 304, AISI Type 304H, AISI Type 304HN, AISI Type 304L, AISI Type 304LN, AISI Type 304N, AISI Type 305, AISI Type 308, AISI Type 308L, AISI Type 309, AISI Type 309Cb+Ta, AISI Type 309S, AISI Type 309SCb, AISI Type 310, AISI Type 310S, AISI Type 312, AISI Type 314, AISI Type 316, AISI Type 316F, AISI Type 316H, AISI Type 316L, AISI Type 316LN, AISI Type 316N, AISI Type 317, AISI Type 317L, AISI Type 317LM, AISI Type 321, AISI Type 321H, AISI Type 329, AISI Type 330, AISI Type 330HC, AISI Type 332, AISI Type 347, AISI Type 347H, AISI Type 348, AISI Type 348H, AISI Type 384, AISI Type 385, AISI Type 403, AISI Type 404, AISI Type 405, AISI Type 409, AISI Type 410, AISI Type 410Cb, AISI Type 410S, AISI Type 414, AISI Type 416, AISI Type 416PlusX, AISI Type 416Se, AISI Type 418, AISI Type 420, AISI Type 420F, AISI Type 422, AISI Type 429, AISI Type 430, AISI Type 430F, AISI Type 430FSe, AISI Type 430Ti, AISI Type 431, AISI Type 434, AISI Type 436, AISI Type 440A, AISI Type 440B, AISI Type 440C, AISI Type 442, AISI Type 444, AISI Type 446, AISI Type 501, AISI Type 501A, AISI Type 501B, AISI Type 502, AISI Type 503, AISI Type 504, AISI Type 632, AISI Type 633, AISI Type 634, AISI Type 635, AL-6X, AM-350, AM-355, AM-363, Crutemp25, CryogenicTenelon, Custom450TM, Custom455TM, E-Brite26-1, HNM, JS-700, JS-777, Monit, Nitronic32, Nitronic33, Nitronic40, Nitronic50, Nitronic60, PH 13-8Mo, Sea-Cure/Sc-1, and Tenelon.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A607 Grade 50
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): 15-20% Glass: Flame-Retardant Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4820 Glossary: Materials: Polymers: Polyvinylchloride: PVC and PVC-AMC: Filled: Sheets, Rods and Tubes; Flexible Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1100 Glossary: Materials: Alloys: Steel: Stainless Steel: Nitronic40 Glossary: Materials: Alloys: Steel: Tool Steel: AISI P2 Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-8Al-1Mo-1V Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-6Al-2Sn-L.5Zr-1Mo-0.35Bi-0.1Si Glossary: Materials: Polymers: Polyphenylene Sulfide: 40% PAN Carbon Fiber: EMI Shielding (conductive) Related Pages
American Standard Steel Channels
American Standard Steel Channels. ... Steel Channels. Steel Angles · Aluminum I-
eFunda: Listing of AISI Type 3xx Stainless Steels
AISI Type 302Cu, Stainless steel, Austenitic standard. Chromium-Nickel steel ... AISI Type 303PlusX, Stainless steel, Austenitic nonstandard ...
eFunda Polymers: Properties of ABS {6% stainless steel fiber, EMI ...
eFunda Polymers: Properties of ABS {6% stainless steel fiber, EMI shielding (
eFunda: Listing of AISI Type A Tool Steels
AISI A10, Tool steel, Air-hardening medium-alloy cold work steel. AISI A2, Tool steel, Air-hardening medium-alloy cold work steel ...
eFunda: Listing of Austenitic Stainless Steels
eFunda: Listing of Austenitic Stainless Steels. ... AISI Type 216, Stainless steel, Austenitic nonstandard. Chromium-Manganese-Nickel steel ...
eFunda: Listing of AISI Type M Tool Steels
eFunda: Listing of AISI Type M Tool Steels. ... AISI M2, Tool steel, Molybdenum high speed steel. AISI M3 class 1, Tool steel, Molybdenum high speed steel ...
eFunda: Listing of Precipitation-Hardening Stainless
AISI Type 632, Stainless steel, Precipitation-hardening nonstandard. Chromium steel. AISI Type 633, Stainless steel, Precipitation-hardening nonstandard ...
Column Design: Structural Steel
Compute critical buckling load for structural steel columns.
eFunda: Properties of Stainless Steel AISI Type 414L
eFunda: Properties of Stainless Steel AISI Type 414L.
eFunda: Listing of AISI Type 4xx Stainless Steels
AISI Type 414, Stainless steel, Martensitic standard. Chromium steel. AISI Type 414L, Stainless steel, Martensitic nonstandard. Chromium steel ...
|
||||||||