Tool Steel: AISI H11
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Alloys » Steel » Tool Steel » AISI H11
AISI H11 is a Chromium Hot Work Steel grade Tool Steel. It is composed of (in weight percentage) 0.33-0.43% Carbon (C), 0.20-0.50% Manganese (Mn), 0.80-1.20% Silicon (Si), 4.75-5.50% Chromium (Cr), 0.3% Nickel (Ni), 1.10-1.60% Molybdenum (Mo), 0.30-0.60% Vanadium (V), 0.25% Copper (Cu), 0.03% Phosphorus (P), 0.03% Sulfur (S), and the base metal Iron (Fe). Other designations of AISI H11 tool steel include UNS T20811 and AISI H11.
Steel is the common name for a large family of iron alloys. Steels can either be cast directly to shape, or into ingots which are reheated and hot worked into a wrought shape by forging, extrusion, rolling, or other processes. Wrought steels are the most common engineering material used, and come in a variety of forms with different finishes and properties. Tool steels typically have excess carbides (carbon alloys) which make them hard and wear-resistant. Most tool steels are used in a heat-treated state, generally hardened and tempered.
The typical elastic modulus of tool steels at room temperature (25°C) ranges from 190 to 210 GPa. The typical density of tool steels ranges from 7.72 to 8.0 g/cm3. The typical tensile strength varies between 640 and 2000 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Tool steels include AISI A10, AISI A2, AISI A3, AISI A4, AISI A6, AISI A7, AISI A8, AISI A9, AISI D2, AISI D3, AISI D4, AISI D5, AISI D7, AISI H10, AISI H12, AISI H13, AISI H14, AISI H19, AISI H21, AISI H22, AISI H23, AISI H24, AISI H25, AISI H26, AISI H42, AISI L2, AISI L6, AISI M1, AISI M10, AISI M2, AISI M30, AISI M33, AISI M34, AISI M36, AISI M3 Class 1, AISI M3 Class 2, AISI M4, AISI M41, AISI M42, AISI M43, AISI M44, AISI M46, AISI M47, AISI M6, AISI M7, AISI O1, AISI O2, AISI O6, AISI O7, AISI P2, AISI P20, AISI P21, AISI P3, AISI P4, AISI P5, AISI P6, AISI S1, AISI S2, AISI S5, AISI S6, AISI S7, AISI T1, AISI T15, AISI T2, AISI T4, AISI T5, AISI T6, AISI T8, AISI W1, AISI W2, and AISI W5.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C95700
Glossary: Materials: Polymers: Polycarbonate: Unfilled: Molding and Extrusion Resins, Low Viscosity Glossary: Materials: Polymers: Polyacetal: Copolymer: 10% PAN Carbon Fiber, 10% PTFE Filled: EMI Shielding (conductive) Glossary: Materials: Polymers: Epoxy: Silica Filled: Casting Resins and Compounds Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8630H Glossary: Design: Oring: Material: Virgin Teflon Glossary: Materials: Polymers: Thermoplastic Elastomers: Polyurethane: Polyester Compound: Molding and Extrusion Compounds, Low and Medium Hardness Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8622 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1536 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1078 Related Pages
Column Design: Structural Steel
Compute critical buckling load for structural steel columns.
eFunda: Listing of AISI Type H Tool Steels
Steel. Name, Class, Alloy Type. AISI H21, Tool steel, Tungsten hot work steel. AISI H22, Tool steel, Tungsten hot work steel ...
eFunda: Listing of AISI Type P Tool Steels
eFunda: Listing of AISI Type P Tool Steels. ... Steel. Name, Class, Alloy Type. AISI P20, Tool steel, General mold steel ...
eFunda: Temper Designations of Magnesium Alloys
Keywords, AISI (US), UNS (US), SAE (US), ASTM (US), AMS (US), ASME (US), MIL (US
Steel S Section I-Beams
Steel S Section I-Beams. ... Steel S-Type I-beam. Steel W-Type I-beam · Steel Channels · Steel Angles · Aluminum I-Beams · Aluminum Channels ...
eFunda: General Information on Steels
General information for steels and their classifications.
eFunda: Properties of Tool Steel AISI H11
eFunda: Properties of Tool Steel AISI H11. ... AISI Wx. Specific Tool Steel. General Information. Resources. Bibliography. FREE Publications ...
eFunda: Listing of AISI Type T Tool Steels
Steel. Name, Class, Alloy Type. AISI T1, Tool steel, Tungsten high speed steel. AISI T15, Tool steel, Tungsten high speed steel ...
eFunda: Listing of AISI Type H Tool Steels
AISI H10, Tool steel, Chromium hot work steel. AISI H11, Tool steel, Chromium hot work steel. AISI H12, Tool steel, Chromium hot work steel ...
eFunda: Listing of Hot-Work Tool Steels
Steel. Name, Class, Alloy Type. AISI H10, Tool steel, Chromium hot work steel. AISI H11, Tool steel, Chromium hot work steel. AISI H12, Tool steel ...
|
||||||||