AISI T8 is a Tungsten High Speed Steel grade Tool Steel. It is composed of (in weight percentage) 0.75-0.85% Carbon (C), 0.20-0.40% Manganese (Mn), 0.20-0.40% Silicon (Si), 3.75-4.50% Chromium (Cr), 0.3% Nickel (Ni), 0.40-1.00% Molybdenum (Mo), 13.25-14.75% Tungsten (W), 1.80-2.40% Vanadium (V), 4.25-5.75% Cobalt (Co), 0.25% Copper (Cu), 0.03% Phosphorus (P), 0.03% Sulfur (S), and the base metal Iron (Fe). Other designations of AISI T8 tool steel include UNS T12008 and AISI T8.
Steel is the common name for a large family of iron alloys. Steels can either be cast directly to shape, or into ingots which are reheated and hot worked into a wrought shape by forging, extrusion, rolling, or other processes. Wrought steels are the most common engineering material used, and come in a variety of forms with different finishes and properties. Tool steels typically have excess carbides (carbon alloys) which make them hard and wear-resistant. Most tool steels are used in a heat-treated state, generally hardened and tempered.
The typical elastic modulus of tool steels at room temperature (25°C) ranges from 190 to 210 GPa. The typical density of tool steels ranges from 7.72 to 8.0 g/cm3. The typical tensile strength varies between 640 and 2000 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Tool steels include AISI A10, AISI A2, AISI A3, AISI A4, AISI A6, AISI A7, AISI A8, AISI A9, AISI D2, AISI D3, AISI D4, AISI D5, AISI D7, AISI H10, AISI H11, AISI H12, AISI H13, AISI H14, AISI H19, AISI H21, AISI H22, AISI H23, AISI H24, AISI H25, AISI H26, AISI H42, AISI L2, AISI L6, AISI M1, AISI M10, AISI M2, AISI M30, AISI M33, AISI M34, AISI M36, AISI M3 Class 1, AISI M3 Class 2, AISI M4, AISI M41, AISI M42, AISI M43, AISI M44, AISI M46, AISI M47, AISI M6, AISI M7, AISI O1, AISI O2, AISI O6, AISI O7, AISI P2, AISI P20, AISI P21, AISI P3, AISI P4, AISI P5, AISI P6, AISI S1, AISI S2, AISI S5, AISI S6, AISI S7, AISI T1, AISI T15, AISI T2, AISI T4, AISI T5, AISI T6, AISI W1, AISI W2, and AISI W5.
Related Glossary Pages
Glossary: Materials: Polymers: Epoxy: Carbon Fiber Reinforced: Sheet Molding Compound (SMC)
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C99750 Glossary: Materials: Alloys: Titanium Alloy: Wrought: 99.2Ti-0.2Pd Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1541 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1525 Glossary: Design: Oring: Material: Virgin Teflon Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C71700 Glossary: Materials: Polymers: Polyurethane: Thermoset: Casting Resin, Liquid Glossary: Materials: Alloys: Steel: Stainless Steel: 29-4 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C91600 Related Pages
eFunda: Listing of AISI Type T Tool Steels
AISI T5, Tool steel, Tungsten high speed steel. AISI T6, Tool steel, Tungsten high speed steel. AISI T8, Tool steel, Tungsten high speed steel ...
eFunda: Listing of Austenitic Stainless Steels
eFunda: Listing of Austenitic Stainless Steels. ... AISI Type 216, Stainless steel, Austenitic nonstandard. Chromium-Manganese-Nickel steel ...
eFunda: Listing of Martensitic Stainless Steels
eFunda: Listing of Martensitic Stainless Steels. ... Chromium steel. AISI Type 410Cb, Stainless steel, Martensitic nonstandard. Chromium steel ...
Column Design: Structural Steel
Compute critical buckling load for structural steel columns.
eFunda: Properties of Tool Steel AISI T8
eFunda: Properties of Tool Steel AISI T8. ... Tool Steel AISI T8 About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an Expert ...
eFunda: Listing of AISI Type M Tool Steels
eFunda: Listing of AISI Type M Tool Steels. ... AISI M2, Tool steel, Molybdenum high speed steel. AISI M3 class 1, Tool steel, Molybdenum high speed steel ...
eFunda: Listing of AISI Type A Tool Steels
AISI A10, Tool steel, Air-hardening medium-alloy cold work steel. AISI A2, Tool steel, Air-hardening medium-alloy cold work steel ...
eFunda: Listing of Magnesium Alloys for Sheets and Plates
Keywords, AISI (US), UNS (US), SAE (US), ASTM (US), AMS (US), ASME (US), MIL (US
eFunda: Properties of Tool Steel AISI T8
eFunda: Properties of Tool Steel AISI T8. ... AISI Wx. Resources. Bibliography. FREE Publications. Auto Industries · Packaging World ...
eFunda: Properties of Aluminum Alloy Aluminum Alloy AA 2011
Keywords, AISI (US), UNS (US), SAE (US), ASTM (US), AMS (US), ASME (US), MIL (US
|
||||||||