Ti-3Al-2.5V is an Alpha-Beta Alloy grade Wrought Titanium Alloy. It is composed of (in weight percentage) 3% Aluminum (Al), 2.5% Vanadium (V), and the base metal Titanium (Ti). Other designations of Ti-3Al-2.5V titanium alloy include AMS 4943, AMS 4944, and AMS 4954.
Titanium is a white metal, and has the best strength to weight ratio among the metals. Titanium is very reactive, and because of this it is often used for alloying and deoxidizing other metals. Titanium is a more powerful deoxidizer of steel than silicon or manganese. Titanium is 40% lighter than steel and 60% heavier than aluminum. This combination of high strength and low weight makes titanium a very useful structural metal. Titanium also features excellent corrosion resistance, which stems from a thin oxide surface film which protects it from atmospheric and ocean conditions as well as a wide variety of chemicals.
The typical elastic modulus of titanium alloys at room temperature (25°C) ranges from 100 to 120 GPa. The typical density of titanium alloys is about 4.5 g/cm3. The typical tensile strength varies between 152 and 379 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions. Additional Information
Other common Wrought Titanium Alloys include 99.5 Ti, Ti-8Al-1Mo-1V, Ti-2.25-Al-11Sn-5Zr-1Mo-0.2Si, Ti-6Al-2Sn-4Zr-2Mo, Ti-5Al-5Sn-2Zr-2Mo-0.25Si, Ti-6Al-2Nb-1Ta-1Mo, Ti-6Al-2Sn-L.5Zr-1Mo-0.35Bi-0.1Si, Ti-8Mn, Ti-6Al-4V, Ti-6Al-4V-ELI (low O2), 99.2 Ti, Ti-6Al-6V-2Sn-0.75Cu, Ti-7AI-4Mo, Ti-6Al-2Sn-4Zr-6Mo, Ti-6Al-2Sn-2Zr-2Mo-2Cr-0.25Si, Ti-10V-2Fe-3Al, Ti-13V-11Cr-3Al, Ti-8Mo-8V-2Fe-3Al, Ti-3Al-8V-6Cr-4Mo-4Zr, Ti-11.5Mo-6Zr-4.5Sn, Ti-5AI-2Sn-2Zr-4Mo-4Cr, 99.1 Ti, 99.0 Ti, 99.2Ti-0.2Pd, Ti-0.3Mo-0.8Ni, Ti-5Al-2.5Sn, and Ti-5Al-2.5Sn-ELI (low O2).
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type H
Glossary: Materials: Polymers: Polystyrene: Copolymer: 20% PAN Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Polymers: Polyamide: Nylon (PA 612): 30-35% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4815H Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4620 Glossary: Materials: Alloys: Steel: Stainless Steel: Nitronic33 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade J Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 409 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C65100 Glossary: Materials: Polymers: Liquid Crystal Polymer: Glass / Mineral Filled Related Pages
eFunda: Properties of Titanium Alloy Ti Alloy Ti Alloy Ti Alloy Ti ...
Ti Alloy Ti Alloy Ti Alloy Ti Alloy Ti Alloy Ti Alloy Ti Alloy Ti-3Al-2.5V About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an ...
eFunda: Listing of Bronzes Copper Alloys
Copper Alloy. Name, Type, Common Name. UNS C22000, Wrought, Copper-zinc brass ... UNS C54400, Wrought, Free-cutting phosphor bronze ...
eFunda: Properties of Titanium Alloy Ti-3Al-2.5V
eFunda: Properties of Titanium Alloy Ti-3Al-2.5V. ... Ti Alloy Ti-3Al-2.5V Home | Directory | Career | News | InfoStore | Industrial ...
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C12500, Wrought, Fire-refined tough pitch copper alloy with silver ...
eFunda: Properties of Titanium Alloy Ti-3Al-2.5V
eFunda: Properties of Titanium Alloy Ti-3Al-2.5V. ... Ti Alloy Ti-3Al-2.5V About Us | Directory | Career | News | Chat | InfoStore | Industrial | Ask an ...
Materials: Metal Alloys: Properties
Ti-3Al-2.5V. Category, Titanium Alloy. Class, Wrought. Type, Alpha-beta alloy. Designations, United States: AMS 4943, AMS 4944, AMS 4954. Composition ...
eFunda: Listing of Alpha-Beta Titanium Alloys
Ti-3Al-2.5V, Wrought, Alpha-beta alloy. Ti-5AI-2Sn-2Zr-4Mo-4Cr, Wrought, Alpha-
eFunda: Listing of Wrought Copper Alloys
eFunda: Listing of Wrought Copper Alloys. ... UNS C18900, Wrought, High-copper alloy ... UNS C19100, Wrought, Copper-nickel-phosphorus-tellurium alloy ...
eFunda: Listing of Wrought Aluminum Alloys
eFunda: Listing of Wrought Aluminum Alloys. ... Al Alloy Types. Cast Alloys. Wrought Alloys. Al Alloy List. Wrought: ...
eFunda: Listing of UNS C6xxxx Copper Alloys
Wrought Alloys. Cu Alloy List ... Name, Type, Common Name. UNS C60800, Wrought, Aluminum bronze, 5% ... UNS C65500, Wrought, High-silicon bronze, A ...
|
||||||||