Extrusion Grade ABS is a subcategory of Acrylonitrile-Butadiene-Styrene. It is specially formulated to extrusion grade. Its elastic modulus ranges from 150 to 390 MPa. Its flexural modulus ranges from 130 to 440 MPa. Its tensile strength ranges from 2500 to 8000 MPa at break. Its flexural strength ranges from 4000 to 14000 MPa. Its compressive strength ranges from 5200 to 10000 MPa. Its Izod Impact strength ranges from 1.5 to 12 J/cm. Its elongation at break ranges from 2.9 to 100 %. Its hardness ranges from 75 to 115 Rockwell R. Its specific gravity ranges from 1.02 to 1.08. Its coefficient of thermal expansion ranges from 60 to 130 x 10-6/°C. Its melting temperature ranges from 88 to 120 °C.
Acrylonitrile-Butadiene-Styrene, also known as ABS, is a thermoplastic. Common trade names are Cycolac and Lustran. It is tough, hard and rigid. It has good chemical resistance, dimensional stability, and creep resistance. It is electroplatable and inexpensive. It has moderate mechanical strength but with a tendency to stress crack. Also, it will be degraded (dissolved) when exposed to acetone. ABS is commonly used in electronic housings, auto parts, consumer products, pipe fittings, waste pipes, computer housings (electroplated on the inside), and automotive interior and exterior trim. ABS is considered superior for its hardness, gloss, toughness, and electrical insulation properties. Although ABS plastics are used primarily for their mechanical properties, they also have good electrical properties that are fairly constant over a wide range of frequencies.
Additional Information
Other common Acrylonitrile-Butadiene-Styrene (ABS) include Flame-Retardant Grades, Molding and Extrusion ABS, ABS / PVC Flame-Retardant Grades, Molding and Extrusion ABS, ABS / PC Flame-Retardant Grades, Molding and Extrusion ABS, ABS / Nylon ABS, ABS / PC Injection Molding and Extrusion ABS, Injection Molding Grade, Heat Resistant ABS, Injection Molding Grade, Medium Impact ABS, Injection Molding Grade, High Impact ABS, Injection Molding Grade, Platable ABS, Injection Molding Grade ABS, 20% Glass Fiber Reinforced Injection Molding Grade ABS, 30% Glass Fiber Reinforced Injection Molding Grade ABS, 20% Long Glass Fiber Reinforced Injection Molding Grade ABS, 40% Long Glass Fiber Reinforced Injection Molding Grade ABS, 6% Stainless Steel Fiber EMI Shielding (conductive) ABS, 7% Stainless Steel Fiber EMI Shielding (conductive) ABS, 10% Stainless Steel Fiber EMI Shielding (conductive) ABS, 20% PAN Carbon Fiber EMI Shielding (conductive) ABS, 20% Graphite Fiber EMI Shielding (conductive) ABS, 40% Aluminum Flake EMI Shielding (conductive) ABS, and Rubber Modified Injection Molding and Extrusion Grades ABS.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 434
Glossary: Materials: Polymers: Polystyrene: Homopolymer: 20% Long and Short Glass Fiber Reinforced Glossary: Materials: Polymers: Polycarbonate: 10% Stainless Steel Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-12 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316LN Glossary: Materials: Alloys: Magnesium Alloy: ASTM ZK51A-T5 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1025 Glossary: Materials: Alloys: Titanium Alloy: Wrought Glossary: Materials: Polymers: Polyaryletherketone: Poly(etherether-Ketone): 30% Carbon Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11100 Related Pages
eFunda Polymers: Listing of Polysulfone (Ultrason)
Sulfone polymers, polysulfone, extrusion / injection molding grade. 4. Sulfone polymers, polysulfone, 20% glass fiber reinforced. ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced, injection molding grade}
eFunda Polymers: Properties of Acetal {homopolymer, extrusion grade}
eFunda Polymers: Properties of Acetal {homopolymer, extrusion grade}
eFunda Polymers: Listing of Polyacetal (Delrin, Ultraform)
Acetal, terpolymer, extrusion and blow molding grade. 7. Acetal, copolymer, 2% silicone, low wear. ... Acetal, homopolymer, extrusion grade. ...
eFunda Polymers: Properties of ABS {injection molding grade, platable}
eFunda Polymers: Properties of ABS {injection molding grade, platable}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Polymer (Plastic) Supplier Contact Information
eFunda: Polymer (Plastic) Supplier Contact Information.
eFunda Polymers: Properties of ABS {extrusion grade}
eFunda Polymers: Properties of ABS {extrusion grade}
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
|
||||||||