Glossary » Materials » Polymers » Fluoroplastics » Poly(vinyl Fluoride) » Unfilled » Film
Unfilled Film PTFE is a subcategory of Fluoroplastics. The additative is added during the manufacturing process. Its elastic modulus ranges from 300 to 380 MPa. Its tensile strength ranges from 6000 to 16000 MPa at break. Its elongation at break ranges from 100 to 250 %. Its specific gravity ranges from 1.38 to 1.4.
Fluoroplastics, also known as PTFE, is a thermoplastic polymer. The most common trade name is Teflon. poly(vinyl fluoride) It has low mechanical strength and is expensive. It has very low coefficient of friction. PTFE is commonly used in applications needing excellent dielectric strength and chemical and temperature resistance.
Additional Information
Other common Fluoroplastics (PTFE) include PTFE, Granular PTFE, 25% Glass Fiber Reinforced PTFE, PTFE, Unfilled PTFE, 20% Milled Glass Fiber PTFE, Filled Film PTFE, Molding and Extrusion PTFE, Wire and Cable Jacketing PTFE, 30% PAN Carbon Fiber EMI Shilding (conductive) PTFE, Unfilled PTFE, 25% Glass Fiber Reinforced PTFE, PTFE, PTFE, PTFE, and PE-CTFE PTFE.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1140 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4042 Glossary: Materials: Polymers: Polystyrene: Rubber-Modified: Flame-Retardant, UL-V0 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1541H Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A553 Type I Glossary: Materials: Alloys: Steel: Tool Steel: AISI M34 Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): 40% Glass Fiber Filled Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82400 Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PC: Injection Molding and Extrusion Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda Polymers: Properties of Polybutylene {film grades}
eFunda Polymers: Properties of Polybutylene {film grades}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Acetal {copolymer, 2 - 20% PTFE filled}
eFunda Polymers: Properties of Acetal {copolymer, 2 - 20% PTFE filled}
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 10% PTFE ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 10% PTFE, lubricated}
eFunda Polymers: Properties of Fluoroplastics {PE-CTFE}
eFunda Polymers: Properties of Fluoroplastics {PE-CTFE}
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, 20 ...
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, 20% fiber reinforced, lubricated}
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 15% PTFE ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 15% PTFE, 30% glass fiber reinforced, lubricated}
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone ...
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone), unfilled} ... State: poly(ethersulfone). Additives: unfilled ...
eFunda: Chemicals Compatibile with O-Ring Material Teflon, Virgin
Chemicals Compatible with Teflon, Virgin (select a chemical to show its compatible O-ring materials). Acetaldehyde (4), Acetamide (4), Acetic Acid, ...
|
||||||||